| β相水淬对Zr-4合金在LiOH水溶液中耐腐蚀性能的影响 |
| 沈月锋1), 姚美意1, 2), 张欣1), 李强1, 2), 周邦新1, 2), 赵文金3) |
1) 上海大学材料研究所, 上海 200072
2) 上海大学微结构重点实验室, 上海 200444
3) 中国核动力研究设计院核燃料及材料国家级重点实验室, 成都 610041 |
|
| EFFECT OF β-QUENCHING ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN LiOH AQUEOUS SOLUTION |
| SHEN Yuefeng1), YAO Meiy1, 2)i, ZHANG Xin1), LI Qiang1, 2), ZHOU Bangxin1, 2), ZHAO Wenjin3) |
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Laboratory for Microstructures, Shanghai University, Shanghai 200444
3) The Key Laboratory for Nuclear Fuel and Materials, Nuclear Power Institute of China, Chengdu 610041 |
引用本文:
沈月锋 姚美意 张欣 李强 周邦新 赵文金. β相水淬对Zr-4合金在LiOH水溶液中耐腐蚀性能的影响[J]. 金属学报, 2011, 47(7): 899-904.
,
,
,
,
,
.
EFFECT OF β-QUENCHING ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN LiOH AQUEOUS SOLUTION[J]. Acta Metall Sin, 2011, 47(7): 899-904.
| [1] Cox B, Wong Y M. In: Eucken C M, Garde A M, eds., Zirconium in the Nuclear Industry: 9th International Symposium, ASTM STP 1132, Baltimore: ASTM International, 1991: 643[2] Pecheur D, Godlewski J, Peybernes J, Fayette L, Noe M, Frichet A, Kerrec O. In: Sabol G P, Moan G D, eds., Zirconium in the Nuclear Industry: 12th International Symposium, ASTM STP 1354, Philadelphia: ASTM International, 2000: 793[3] Zhou B X, Li Q, Huang Q, Miao Z, Zhao W J, Li C. Nuc Power Eng, 2000; 21: 43(周邦新, 李强, 黄强, 苗志, 赵文金, 李 聪. 核动力工程, 2000; 21: 43)[4] Sabol G P, Comstock R J, Weiner R A, Larouere P, Stanutz R N. In: Garde A M, Bradley E R, eds., Zirconium in the Nuclear Industry: 10th International Symposium, ASTM STP 1245, Ann Arbor: ASTM International, 1994: 724[5] Nikulina A V, Markelvo V A, Peregud M M, Bibilashvili Y K, Kotrekhov V A, Lositsky A F, Kuzmenko N V, Shevnin YP, ShamardinVK, KobylyanskyGP, NovoselovAE. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 785[6] Zhao W J, Miao Z, Jiang H M, Yu X W, Li W J, Li C, Zhou B X. J Chin Soc Corros Prot, 2002; 22: 124(赵文金, 苗 志, 蒋宏曼, 于晓卫, 李卫军, 李聪, 周邦新. 中国腐蚀与防护学报, 2002; 22: 124)[7] Li Z K, Liu J Z, Li P Z, Zhou L, Song Q Z. Rare Met Mater Eng, 1999; 28: 101(李中奎, 刘建章, 李佩志, 周廉, 宋启忠. 稀有金属材料与工程, 1999; 28: 101)[8] Li Z K, Liu J Z, Zhu M S, Song Q Z. Rare Met Mater Eng, 1996; 25: 43(李中奎, 刘建章, 朱梅生, 宋启忠. 稀有金属材料与工程, 1996; 25: 43)[9] Yao M Y, Zhou B X, Li Q, Liu W Q, Geng X, Lu Y P. J Nucl Mater, 2008; 374: 197[10] Yao M Y, Zhou B X, Li Q, Liu W Q, Wang S A, Huang X S. Rare Met Mater Eng, 2007; 36: 1915(姚美意, 周邦新, 李 强, 刘文庆, 王树安, 黄新树. 稀有金属材料与工程, 2007; 36: 1915)[11] Zhou B X, Li Q, Miao Z. Nucl Power Eng, 2000; 21: 339(周邦新, 李强, 苗 志. 核动力工程, 2000; 21: 339)[12] Anada H, Herb B J, Nomoto K, Hagi S, Graham R A, Kuroda T. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 74[13] Foster P, Dougherty J, Burke M G, Bates J F, Worcester S. J Nucl Mater, 1990; 173: 164[14] Garzarolli G, Steinberg E, Weidinger H G. In: Van Swam L F P, Eucken C M, eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1989: 202[15] Zhou B X, Zhao W J, Miao Z, Pan S F, Li C, Jiang Y R. Chin J Nucl Sci Eng, 1995; 15: 242(周邦新, 赵文金, 苗志, 潘淑芳, 李 聪, 蒋有荣. 核科学与工程, 1995; 15: 242)[16] Choo K N, Kang Y H, Pyun S I, Vrbanic V F. J NuclMat, 1994; 209: 226[17] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1[18] Garzarolli F, Pohlmeyer I, Steinberg E, Trapp–pritsching S. Proc Technical Committee Meeting, Cadarache: the International Atomic Energy Agency, 1985: 66[19] Liu J Z. Structure Nuclear Materials. Beijing: Chemical Industry Press, 2007: 111(刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 111)[20] Yao M Y,Wang J H, Peng J C, Zhou B X, Li Q. J ASTM Intl, 2011; 8: 13[21] Liu W Q, Li Q, Zhou B X, Yao M Y. Rare Met Mater Eng, 2004, 33: 728(刘文庆, 李强, 周邦新, 姚美意. 稀有金属材料与工程, 2004, 33: 728)[22] Zhou B X, Li Q, Yao M Y, Liu WQ, Chu Y L. Nucl Power Eng, 2005; 26: 364(周邦新, 李强, 姚美意, 刘文庆, 褚于良. 核动力工程, 2005; 26: 364)[23] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)[24] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Intl, 2008; 5: 360 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|