| Al2Sr和Mg2Sr相结构稳定性与弹性性能的第一原理计算 |
| 周惦武1,刘金水2,徐少华2,彭平2 |
1.湖南大学汽车车身先进设计制造国家重点实验室, 长沙 410082
2.湖南大学材料科学与工程学院, 长沙 410082 |
|
| FIRST–PRINCIPLE CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF Al2Sr AND Mg2Sr PHASES |
| ZHOU Dianwu1, LIU Jinshui2, XU Shaohua2, PENG Ping2 |
1.State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, Changsha 410082
2.School of Materials Science and Engineering, Hunan University, Changsha 410082 |
引用本文:
周惦武 刘金水 徐少华 彭平. Al2Sr和Mg2Sr相结构稳定性与弹性性能的第一原理计算[J]. 金属学报, 2011, 47(10): 1315-1320.
,
,
,
.
FIRST–PRINCIPLE CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF Al2Sr AND Mg2Sr PHASES[J]. Acta Metall Sin, 2011, 47(10): 1315-1320.
| [1] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37[2] Luo A, Pekguleryuz M O. J Mater Sci, 1994; 29: 5259[3] Parvez M A, Medraj M, Essadiqi E, Muntasar A, Denes G. J Alloys Compd, 2005; 402: 170[4] Chartrand P, Pelton A D. J Phase Equilib, 1994; 5: 591[5] Aljarrah M, Parvez M A, Li J, Essadiqi E, Medraj M. Sci Technol Adv Mater, 2007; 8: 237[6] Segall M D, Lindan P L D, Probert M J, Pickard C J, Hasnip P J, Clark S J, Payne M C. J Phys: Condens Matter, 2002; 14: 2717[7] Marlo M, Milman V. Phys Rev, 2000; 62B: 2899[8] Vanderbilt D. Phys Rev, 1990; 41B: 7892[9] Hammer B, Hansen L B, Norkov J K. Phys Rev, 1999; 59B: 7413[10] Franscis G P, Payne M C. J Phys: Condens Matter, 1990; 2: 4395[11] Monkhorst H J, Pack J D. Phys Rev, 1976; 13B: 5188[12] Duan Y H, Sun Y, Peng M J, Guo Z Z. Solid State Sci, 2011; 13: 455[13] Min X G, Du W W, Xue F, Sun Y S. Chin Sci Bull, 2002; 47: 109[14] Zhong Y, Sofo J O, Luo A A, Liu Z K. J Alloys Compd, 2006; 421: 172[15] Alcock C B, Itkin V P. Bull Alloy Phase Diagrams, 1989; 10: 624[16] Zhou DW, Liu J S, Lou Y Z, Zhang C H. Chin Nonferrous Met, 2008; 18: 118(周惦武, 刘金水, 卢远志, 张楚惠. 中国有色金属学报, 2008; 18: 118)[17] King R C, Kleppa O J. Acta Metall Mater, 1964; 12: 87[18] Aljarrah M, Medraj M. Comp Coup Phase Diagrams Thermochem, 2008; 32: 240[19] Zubov V I, Tretiakov N P, Teixeira Rabelo J N, Sanchez Ortiz J F. Phys Lett, 1995; 198A: 470[20] Ishii Y, Fujiwara T. Non–Cryst Solids, 2002; 312–314: 494[21] Wang N, Yu W Y, Tang B Y, Peng L M, Ding W J. J Phys, 2008; 41D: 195408[22] Hong S Y, Fu C L. Intermetallics, 1999; 7: 5[23] Mehl M J, Osburn J E, Papaconstantopoulos D A, Klein B M. Phys Rev, 1990; 41B: 10311[24] YuWY, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2009; 11: 1400[25] Mattesini M, Ahuja R, Johansson B. Phys Rev, 2003; 68B: 184108 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|