Please wait a minute...
金属学报  2011, Vol. 47 Issue (10): 1307-1314    DOI: 10.3724/SP.J.1037.2011.00151
  论文 本期目录 | 过刊浏览 |
梯度硬质合金梯度层形成的计算机模拟及验证
张伟彬1,沙春生1,杜勇1,温光华2,谢文2,王社权2
1.中南大学粉末冶金国家重点实验室, 长沙 410083
2.株洲钻石切削刀具股份有限公司, 株洲 412007
COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES
ZHANG Weibin1, SHA Chunsheng1, DU Yong1, WEN Guanghua2, XIE Wen2, WANG Shequan2
1.State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083
2.Zhuzhou Cemented Carbide Cutting Tools Limited Company, Zhuzhou 412007
引用本文:

张伟彬 沙春生 杜勇 温光华 谢文 王社权. 梯度硬质合金梯度层形成的计算机模拟及验证[J]. 金属学报, 2011, 47(10): 1307-1314.
, , , , , . COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. Acta Metall Sin, 2011, 47(10): 1307-1314.

全文: PDF(1248 KB)  
摘要: 建立了多组元梯度硬质合金W-C-Co-Ti-Ta-Nb-N体系的热力学和扩散动力学数据库, 采用Thermo-Calc相图热力学计算软件描述了梯度烧结过程中出现的各相及其成分,并采用DICTRA扩散动力学软件对WC-Ti(C, N)-Co, WC-Ti(C, N)-TaC-Co和WC-Ti(C, N)-NbC-Co合金梯度层的各相体积分数及各组元成分随距离的分布进行了计算机模拟, 模拟结果与实验结果吻合良好. 在热力学和扩散动力学数据库基础上制备了WC-(Ti, W)C-Ti(C, N)-(Ta, Nb)C-Co合金, 采用SEM观察梯度层的显微结构, 利用EDS分析合金组元分布, 并对合金梯度层的形成进行了计算模拟, 模拟结果与实验结果吻合良好.
关键词 : 梯度硬质合金,  热力学,  动力学,  相图计算,  模拟    
Abstract:The thermodynamic and kinetic databases for multi–component W–C–Co–Ti–Ta–Nb–N cemented carbides were established. The Thermo–Calc software was used to describe the phase composition of alloys during gradient sintering. Based on the established thermodynamic and kinetic databases, the volume fractions of different phases and elemental concentration profiles in the WC– Ti(C, N)–Co, WC–Ti(C, N)–TaC–Co and WC–Ti(C, N)–NbC–Co alloys were simulated by means of DICTRA software. The simulated results are in good agreement with the experimental data. In order to verify the reliability of the thermodynamic and kinetic databases, a gradiently sintered WC–Ti(C, N)–TaC–NbC–Co cemented carbide has been prepared. SEM and EDS were employed to examinate the microstructure and composition in the gradient zone. The gradient zone formation of the WC– Ti(C, N)–TaC–NbC–Co cemented carbides was then simulated by DICTRA, and the simulation results show a good agreement with the experimental results.
Key words: cemented carbide    thermodynamis    kinetics    phase diagram calculation    simulation
收稿日期: 2011-03-23     
基金资助:

国家自然科学基金项目51028101, 国家重点基础研究发展计划项目2011CB610401和国家自然科学基金创新群体项目51021063资助

作者简介: 张伟彬, 男, 1985年生, 硕士生
[1] Zhang W Z, Liu Y, He Y H, Wang H B. Rare Met Cem Carbides, 2005; 33(2): 28

(张武装, 刘 咏, 贺跃辉, 王海兵. 稀有金属及硬质合金, 2005; 33(2): 28)

[2] Konyashin I Y. Mater Sci Eng, 1997; A230: 213

[3] Konyashin I Y. Surf Coat Technol, 1995; 71: 277

[4] Knotek O, Loffler F, Kramer G. Int J Ref Hard Mater, 1996; 14: 195

[5] Narasimhan K, Boppana S P, Bhat D G. Wear, 1995; 188: 123

[6] Frykholm R, Ekroth M, Jansson B, Andrén H O, Ågren J. Acta Mater, 2003; 51: 1115

[7] Schwarzkopf M, Exner H E, Fischmeister H F. Mater Sci Eng, 1998; A105–106: 225

[8] Chen L M, Lengauer W, Ettmayer P, Dreyer K, Daub H W, Kassel D. Int J Ref Hard Mater, 2000; 18: 307

[9] Frykholm R, Andrén H O. Mater Chem Phys, 2001; 67: 203

[10] Andr´en H O. Mater Chem Phy, 2001; 67: 209

[11] Rosso M, Kassel D. Int J Ref Hard Mater, 1999; 17: 187

[12] Dreyer K, Kassel D. Int Plansee Seminar, 2001; 2: 768

[13] Suzuki H, Koji H, Yasuro T. Trans Jpn Inst Met, 1981; 22: 758

[14] Gustafson P, Östlund Å. Int J Ref Hard Mater, 1993–1994; 12: 129

[15] Ekroth M, Frykholm R, Lindholm M, Andrén H O, Ågren J. Acta Mater, 2000; 48: 2177

[16] Frykholm R, Ekroth M, Jansson B, Andrén H O, Ågren J. Int J Ref Hard Mater, 2001; 19: 527

[17] Ekroth M, Frisk K, Jansson B, Dumitrescu F S. Metall Mater Trans, 2000; 31B: 615

[18] Frisk K, Dumitrescu F S, Ekroth M, Jansson B, Kruse O, Sundman B. J Phase Equilib, 2001; 22: 645

[19] Gustafson P. Mater Sci Technol, 1986; 2: 635

[20] Andrén J O, Helander T, H¨oglund L H, Shi P F, Sundman B. Calphad, 2002; 26: 273

[21] Andrén H O. Mater Chem Phys, 2001; 67: 209
[1] 陈佳, 郭敏, 杨敏, 刘林, 张军. 新型钴基高温合金中W元素对蠕变组织和性能的影响[J]. 金属学报, 2023, 59(9): 1209-1220.
[2] 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继. 高温合金锻件残余应力量化表征及控制技术研究进展[J]. 金属学报, 2023, 59(9): 1144-1158.
[3] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[4] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[5] 张海峰, 闫海乐, 方烽, 贾楠. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟[J]. 金属学报, 2023, 59(8): 1051-1064.
[6] 张禄, 余志伟, 张磊成, 江荣, 宋迎东. GH4169高温合金热机械疲劳循环损伤机理及数值模拟[J]. 金属学报, 2023, 59(7): 871-883.
[7] 王寒玉, 李彩, 赵璨, 曾涛, 王祖敏, 黄远. 基于纳米活性结构的不互溶W-Cu体系直接合金化及其热力学机制[J]. 金属学报, 2023, 59(5): 679-692.
[8] 王长胜, 付华栋, 张洪涛, 谢建新. 冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响[J]. 金属学报, 2023, 59(5): 585-598.
[9] 张开元, 董文超, 赵栋, 李世键, 陆善平. 固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响[J]. 金属学报, 2023, 59(12): 1633-1643.
[10] 张月鑫, 王举金, 杨文, 张立峰. 冷却速率对管线钢中非金属夹杂物成分演变的影响[J]. 金属学报, 2023, 59(12): 1603-1612.
[11] 王重阳, 韩世伟, 谢峰, 胡龙, 邓德安. 固态相变和软化效应对超高强钢焊接残余应力的影响[J]. 金属学报, 2023, 59(12): 1613-1623.
[12] 陈凯旋, 李宗烜, 王自东, Demange Gilles, 陈晓华, 张佳伟, 吴雪华, Zapolsky Helena. Cu-2.0Fe合金等温处理过程中富Fe析出相的形态演变[J]. 金属学报, 2023, 59(12): 1665-1674.
[13] 周小宾, 赵占山, 汪万行, 徐建国, 岳强. 渣-金界面气泡夹带行为数值物理模拟[J]. 金属学报, 2023, 59(11): 1523-1532.
[14] 戚晓勇, 柳文波, 何宗倍, 王一帆, 恽迪. UN核燃料烧结致密化过程的相场模拟[J]. 金属学报, 2023, 59(11): 1513-1522.
[15] 杜宗罡, 徐涛, 李宁, 李文生, 邢钢, 巨璐, 赵利华, 吴华, 田育成. Ni-Ir/Al2O3 负载型催化剂的制备及其用于水合肼分解制氢性能[J]. 金属学报, 2023, 59(10): 1335-1345.