| 热处理过程大型铸钢件变形的三维动态测量 |
| 康进武1), 聂刚1), 喻海良1, 2), 龙海敏1), 郝小坤1), 黄天佑1), 胡永沂1) |
1) 清华大学机械工程系教育部先进成形制造重点实验室, 北京 100084
2) 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110004 |
|
| THREE DIMENSIONAL DYNAMICAL MEASUREMENT OF DISTORTION OF HEAVY STEEL CASTINGS DURING HEAT TREATMENT PROCESS |
| KANG Jinwu1), NIE Gang1), YU Hailiang1, 2), LONG Haimin1), HAO Xiaokun1), HUANG Tianyou1), HU Yongyi1) |
1) Department of Mechanical Engineering, Key Laboratory for Advanced Materials Processing Technology, Tsinghua University, Beijing 100084
2) State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110004 |
引用本文:
康进武 聂刚 喻海良 龙海敏 郝小坤 黄天佑 胡永沂. 热处理过程大型铸钢件变形的三维动态测量[J]. 金属学报, 2011, 47(5): 535-539.
,
,
,
,
,
,
.
THREE DIMENSIONAL DYNAMICAL MEASUREMENT OF DISTORTION OF HEAVY STEEL CASTINGS DURING HEAT TREATMENT PROCESS[J]. Acta Metall Sin, 2011, 47(5): 535-539.
| [1] Yu H L, Kang J W, Huang T Y. Front Mater Sci, 2010; 4: 332[2] Huang T Y, Liu X G, Kang J W, Shen H F, Liu B C. Foundry, 2007; 56: 899(黄天佑, 刘小刚, 康进武, 沈厚发, 柳百成. 铸造, 2007; 56: 899)[3] Liu B C, Kang J W, Xiong S M. Sci Technol Adv Mater, 2001; 2: 157[4] Bruschi S, Ghiotti A. Int J Machine Tools Manuf, 2008; 48: 761[5] Yu H L, Kang J W, Huang S X, Huang T Y. Adv Mater Res, 2011; 148–149: 103[6] Wang P, Xiao N, Li D, Li Y. Mater Sci Forum, 2010; 654– 656: 1565[7] Wang Z K, Hu Z H. Dongfang Electric Rev, 2004; 18(3): 137(王贞凯, 胡章洪. 东方电气评论, 2004; 18(3): 137)[8] Wang Y X, Zhang P C, Li B C, Zeng W D. China Foundry Mach Technol, 2007; 1: 24(王云霞, 张鹏程, 李宝治, 曾卫东. 中国铸造装备与技术, 2007; 1: 24)[9] Yu H L, Kang J W, Huang T Y. Sci China, 2011; 54E: 81[10] Jiang R S, Zhang D H, Wang W H, Bu K, Cheng Y Y. Spec Cast Nonferrous Alloys, 2009; 29(1): 13(蒋睿嵩, 张定华, 汪文虎, 卜 昆, 程云勇. 特种铸造及有色合金, 2009; 29(1): 13)[11] Han W, Yu W S, Kong S G, Wu J T, Li J T, Ma Z L, Zhao M H. Foundry, 2009; 58: 1108(韩伟, 于望生, 孙胜国, 吴剑涛, 李俊涛, 马章林, 赵明汉. 铸造, 2009; 58: 1108)[12] Yu H L, Kang J W, Nie G, Long H M, Hao X K, Huang T Y. China Foundry, 2011; in press[13] Coret M, Combescure A. Int J Mech Sci, 2002; 44: 1947[14] Sun C Y, Fang G, Lei L P, Zeng P. Trans Mater Heat Treat, 2008; 29: 162(孙朝阳, 方刚, 雷丽萍, 曾 攀. 材料热处理学报, 2008; 29: 162) |
|