| 激光快速熔凝Ni-Sn共晶合金的组织演变 |
| 曹永青, 林鑫, 汪志太, 杨海欧, 黄卫东 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| MICROSTRUCTURE EVOLUTION OF Ni-Sn EUTECTIC ALLOY IN LASER RAPID SOLIDIFICATION |
| CAO Yongqing, LIN Xin, WANG Zhitai, YANG Haiou, HUANG Weidong |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
曹永青 林鑫 汪志太 杨海欧 黄卫东. 激光快速熔凝Ni-Sn共晶合金的组织演变[J]. 金属学报, 2011, 47(5): 540-547.
,
,
,
,
.
MICROSTRUCTURE EVOLUTION OF Ni-Sn EUTECTIC ALLOY IN LASER RAPID SOLIDIFICATION[J]. Acta Metall Sin, 2011, 47(5): 540-547.
| [1] Powell G L, Hogan L M. Inst Met, 1965; 93: 505[2] Kattamis T Z, Fleming M C. Metall Trans, 1970; 1: 1449[3] Jones B L. Metall Trans, 197l; 2: 2950[4] Wei B, Herlach D M, Feuerbacher B, Sommer F. Acta Metall Mater, 1993; 41: 1801[5] Wei B, Herlach D M, Sommer F, Kurz W. Mater Sci Eng, 1994; A181: 1150[6] Goetzinger R, Barth M, Herlach D M. Acta Mater, 1998; 46: 1647[7] Wei B, Yang G C, Zhou Y H. Acta Metall Mater, 1991; 39: 1249[8] Wei B, Herlach D M, Sommer F. Mater Sci Lett, 1993; 12: 1774[9] Xing L Q, Zhao D Q, Chen X C. Mater Sci, 1993; 28: 2733[10] Tewari S N. Metall Trans, 1987; 18A: 525[11] Chu M G, Shiohara Y. Metall Trans, 1984; 15A: 1303[12] Lu Y P, Liu F, Yang G C, Zhou Y H. Appl Phys Lett, 2006; 89: 241902[13] Li M J, Nagashio K, Ishikawa T, Yoda S, Kuribayashi K. Acta Mater, 2005; 53: 731[14] Li J F, JieWQ, Zhao S, Zhou Y H. Metall Mater Trans, 2007; 38A: 1806[15] Li J F, Li X L, Liu L, Lu S Y. Mater Res Soc, 2008; 23: 2139[16] Rappaz M, Gremaud M, Dekumbis R, Kurz W. In: Mordike B L ed., Laser Treatment of Materials, Oberursel: DGM Informations gesellschaft–Verlay, 1987: 43[17] GaumannM, Bezencqn C, Canalis P, Kurz W. Acta Mater, 2001; 49: 1051[18] Rappaz M, David S A, Vitek J M, Boatner L A. Metall Trans, 1989; 20A: 1125[19] Kurz W, Fisher D J. Fundamentals of Solidification, 3rd Ed. Switzerland: Trans Tech Publications, 1992: 83[20] Trivedi R, Kurz W. Acta Metal Mater, 1994; 42: 15[21] Hoadley A F A, Rappaz A. Metal Trans, 1992; 23B: 631[22] Lin X, Yue T M, Yang H O, Huang W D. Acta Mater, 2006; 54: 1901[23] Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34: 823[24] Aziz M J. Appl Phys, 1982, 53: 1158[25] Boettinger W J, Coriell S R, Trivedi R. Rapid Solidification Processing: Principles and Technologies IV. Baton Rouge, LA: Claitor’s Publishing Division, 1988: 13[26] Brandes E A. Smithells Metals Reference Book. Bodmin, Cornwall: Butterworth & Co. Ltd, 1983: 41[27] Trivedi R, Magnin P, Kurz W. Acta Metall, 1987; 35: 971 |
|