| 非晶态及部分晶化态Al-Ni-Y合金的磁性 |
| 龚静1,杨红旺1,杨柏俊2,王瑞春1,李荣德1,王建强3 |
1. 沈阳工业大学材料科学与工程学院, 沈阳 110870
2. 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| MAGNETISM OF MONOLITHIC AND PARTIALLY CRYSTALLIZED AMORPHOUS Al–Ni–Y ALLOYS |
| GONG Jing 1, YANG Hongwang 1, YANG Baijun 2, WANG Ruichun 1, LI Rongde 1,WANG Jianqiang 2 |
1. School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
2. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
龚静 杨红旺 杨柏俊 王瑞春 李荣德 王建强. 非晶态及部分晶化态Al-Ni-Y合金的磁性[J]. 金属学报, 2011, 47(3): 333-336.
,
,
,
,
,
.
MAGNETISM OF MONOLITHIC AND PARTIALLY CRYSTALLIZED AMORPHOUS Al–Ni–Y ALLOYS[J]. Acta Metall Sin, 2011, 47(3): 333-336.
| [1] Yoshizawa Y, Oguma S, Yamauchi K. J Appl Phys, 1988; 64: 6044[2] Fujii Y, Fujita H, Seki A. J Appl Phys, 1991; 70: 6241[3] Suzuki K, Makino A, Inoue A, Masumoto T. J Appl Phys, 1993; 74: 3316[4] Liu T, Gao Y F, Xu Z X, Zhao Z T, Ma R Z. J Appl Phys, 1996; 80: 3972[5] Guo S F, Wu Z Y, Liu L. J Alloy Compd, 2009; 468: 54[6] Duhaj P, Svec P, Janickovic D, Matko I, Hlasnik M. Mater Sci Eng, 1992; B14: 357[7] Hu Y, Liu L, Chan K C, Pan M X, Wang W H. Mater Lett, 2006; 60: 1080[8] Inoue A, Ohtera K, Tsai A P, Masumoto T. Jpn J Appl Phys, Part 2, 1988; 27: L280[9] He Y, Poon S J, Shiflet G J. Science, 1988; 241: 1640[10] Kim Y H, Inoue A, Masumoto T. Mater Trans JIM, 1990; 31: 747[11] Kim Y H, Inoue A, Masumoto T. Mater Trans JIM, 1991; 32: 331[12] Cochrane R F, Schumacher P, Greer A L. Mater Sci Eng, 1991; 133: 367[13] Benameur T, Inoue A. Mater Sci Froum, 1995; 179–181: 813[14] Gogebakan M, Warren P J, Cantor B. Mater Sci Eng, 1997; A226–228: 168[15] Foley J C, Allen D R, Perepezko J H. Scr Mater, 1996; 35: 655[16] Inoue A, Matsumoto N, Masumoto T. Mater Trans JIM, 1990; 31: 493[17] Guo F Q, Poon S J, Shiflet G J. Mater Sci Forum, 2000; 331–337: 31[18] Yang B J, Yao J H, Zhang J, Yang H W, Wang J Q, Ma E. Scr Mater, 2009; 61: 423[19] Zhuo L C, Pang S J, Wang H, Zhang T. Chin Phys Lett, 2009; 26: 066402[20] Wan D F, Luo S H. Physics of Magnetism. Beijing: Electronic Industry Press, 1987: 232(宛德福, 罗世华. 磁性物理. 北京: 电子工业出版社, 1987: 232)[21] Hono K, Zhang Y, Tsai A P, Inoue A, Sakurai T. Scr Metall Mater, 1995; 32: 191 |
|