| Ti-Mo全铁素体基微合金高强钢纳米尺度析出相 |
| 段修刚, 蔡庆伍, 武会宾 |
| 北京科技大学冶金工程研究院, 北京 100083 |
|
| Ti-Mo FERRITE MATRIX MICRO-ALLOY STEEL WITH NANOMETER-SIZED PRECIPITATES |
| DUAN Xiugang, CAI Qingwu, WU Huibin |
| Research Institute of Metallurgical Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
段修刚 蔡庆伍 武会宾. Ti-Mo全铁素体基微合金高强钢纳米尺度析出相[J]. 金属学报, 2011, 47(2): 251-256.
,
,
.
Ti-Mo FERRITE MATRIX MICRO-ALLOY STEEL WITH NANOMETER-SIZED PRECIPITATES[J]. Acta Metall Sin, 2011, 47(2): 251-256.
| [1] Cao J C. PhD Thesis, Kunming University of Science and Technology, 2006(曹建春. 昆明理工大学博士学位论文, 2006)[2] Gladman T. Mater Sci Technol, 1999; 15: 30[3] Yong Q L. Secondary Phase in Steel. Beijing: Metallurgical Industry Press, 2006: 15(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 15)[4] Andrade H L, Akben M G, Jonas J J. Metall Trans, 1983; 14A: 1967[5] Lee W B, Hong S G, Park C G, et al. Metall Mater Trans, 2002; 33A: 1689[6] Lee W B, Hong S G, Park C G. Scr Mater, 2000; 43: 319[7] Yang S W, He X L, Chen M D. Mater Sci Technol, 1994; 12(2): 49(杨善武, 贺信莱, 陈梦滴. 材料科学与工程, 1994; 12(2): 49)[8] Wang Z D, Qu J B, Liu X H. Acta Metall Sin, 2000; 36: 618(王昭东, 曲锦波, 刘相华. 金属学报, 2000; 36: 618)[9] He X L, Shang C J, Yang S W. High Performance Low Carbon Bainite Steel/Ingredients, Process, Microstructure, Properties and Application. Beijing: Metallurgical Industry Press, 2008: 152(贺信来, 尚成嘉, 杨善武. 高性能低碳贝氏体钢--成分、工艺、组织、性能与应用. 北京, 冶金工业出版社, 2008: 152)[10] Craven A J, He K, Garvie L A J, Baker T N. Acta Mater, 2000; 48: 3857[11] Hong S G, Kang K B, Park C G. Scr Mater, 2002; 46: 163[12] Villars P, Calvert L D. Metals Park(USA OH): ASM, 1985: 52[13] Yu W. PhD Thesis, University of Science and Technology Beijing, 2008(余伟. 北京科技大学博士学位论文, 2008)[14] DeArdo A J. Mater Sci Forum, 1998; 284–286: 15[15] FunakawaY, Shiozaki T, Tomita K. ISIJ Int, 2004; 44, 1945[16] Cao J C, Yong Q L, Liu Q Y. Trans Mater Heat Treat, 2006; 27(5): 51(曹建春, 雍岐龙, 刘清友. 材料热处理学报, 2006; 27(5): 51)[17] Bacroix B, Akben M G, Jonas J J. Warrendale: A Publication of the Metallurgy Society of AIME, 1982: 293[18] Lee W B, Hong S G, Park C G, Kim K H, Park S H. Scr Mater, 2000; 43: 319[19] Akben M G, Baeroix B, Jonas J J. Acta Metall, 1983; 31: 161[20] Maruyama N, Uemori R, Suriyama M. Mater Sci Eng, 1998; A250: 2 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|