| Cu/Nb纳米金属多层膜延性及断裂行为的尺寸效应 |
| 张欣 张金钰 刘刚 张国君 孙军 |
| 西安交通大学金属材料强度国家重点实验室, 西安 710049 |
|
| LENGTH SCALE DEPENDENT DUCTILITY AND FRACTURE BEHAVIOR OF Cu/Nb NANOSTRUCTURED METALLIC MULTILAYERS |
| ZHANG Xin, ZHANG Jinyu, LIU Gang, ZHANG Guojun, SUN Jun |
| State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049 |
引用本文:
张欣 张金钰 刘刚 张国君 孙军. Cu/Nb纳米金属多层膜延性及断裂行为的尺寸效应[J]. 金属学报, 2011, 47(2): 246-250.
,
,
,
,
.
LENGTH SCALE DEPENDENT DUCTILITY AND FRACTURE BEHAVIOR OF Cu/Nb NANOSTRUCTURED METALLIC MULTILAYERS[J]. Acta Metall Sin, 2011, 47(2): 246-250.
| [1] Spearing S M. Acta Mater, 2000; 48: 179[2] Suo Z G, Vlassak J, Wagner S. China Particuology, 2005; 3: 321[3] Bakonyi I, P´eter L. Prog Mater Sci, 2010; 55(3): 107[4] Was G S, Foecke T. Thin Solid Films, 1996; 286: 1[5] Misra A, Krug H. Adv Eng Mater, 2001; 3(4): 217[6] Misra A, Hirth J P, Hoagland R G. Acta Mater, 2005; 53: 4817[7] Phillips M A, Clemens B M, Nix W D. Acta Mater, 2003; 51: 3171[8] Huang H B, Spaepen F. Acta Mater, 2000; 48: 3261[9] Mara N A, Bhattacharyya D, Hoagland R G, Misra A. Scr Mater, 2008; 58: 874[10] Niu R M, Liu G, Wang C, Zhang G, Ding X D. Appl Phys Lett, 2007; 90: 161907[11] Li Y P, Tan J, Zhang G P. Scr Mater, 2008; 59: 1226[12] Li Y P, Zhang G P. Acta Mater, 2010; 58: 3877[13] Zhu X F, Li Y P, Zhang G P, Tan J, Liu Y. Appl Phys Lett, 2008; 92: 161905[14] Yu D Y W, Spaepen F. J Appl Phys, 2004; 95: 2991[15] Zhang J Y, Zhang X, Liu G, Zhang G J, Sun J. Scr Mater, 2010; 63: 101[16] Hertzberg R W. Deformation and Fracture Mechanics of Engineering Materials. New York: John Wiley, 1989: 15[17] Dundurs J, Bogy D B. J Appl Mech, 1969; 36: 650[18] Jr Beuth J L. Int J Solids Struct, 1992; 29: 1657 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|