| 不锈钢材料的高效率焊接新工艺 |
| 陆善平, 董文超, 李殿中, 李依依 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| HIGH EFFICIENCY WELDING PROCESS FOR STAINLESS STEEL MATERIALS |
| LU Shanping, DONG Wenchao, LI Dianzhong, LI Yiyi |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
陆善平 董文超 李殿中 李依依. 不锈钢材料的高效率焊接新工艺[J]. 金属学报, 2010, 46(11): 1347-1364.
,
,
,
.
HIGH EFFICIENCY WELDING PROCESS FOR STAINLESS STEEL MATERIALS[J]. Acta Metall Sin, 2010, 46(11): 1347-1364.
| [1] Gurevich S M, Zamkov V N, Kushmienko N A. Avtom Svarka, 1965; 9: 1
[2] Gurevich S M, Zamkov V N. Avtom Svarka, 1966; 12: 13
[3] Ludwig H C. Weld J, 1968; 47: 234s
[4] Lucas W, Howse D S. Weld Met Fabr, 1996; 64: 11
[5] Howse D S, Lucas W. Sci Technol Weld Joi, 2000; 15: 189
[6] Tanaka M, Shimizu T, Terasaki H, Ushio M, Koshi–ishi F, Yang C L. Sci Technol Weld Join, 2000; 5: 397
[7] Anderson P C J, Wiktorowicz R. Weld Met Fabr, 1996; 64: 108
[8] Paskell T, Lundin C, Castner H. Weld J, 1997; 76: 57s
[9] Modenesi P J, Apolinario E R, Pereira I M. J Mater Proc Technol, 2000; 9: 260
[10] Kou M, Sun Z, Pan D. Sci Technol Weld Join, 2001; 6: 17
[11] Savitskii M M, Leskov G I. Avtom Svarka, 1980; 9: 17
[12] Lowke J J, Tanaka M, Ushio M. The 57th Annual Assembly of International Institute of Welding. Osaka, Japan, 2004, IIW Doc. 212–1053–04
[13] Heiple C R, Burgardt P. Weld J, 1985; 64: 159s
[14] Heiple C R, Roper J R. Weld J, 1982; 61: 97s
[15] Heiple C R, Roper J R, Stagner R T, Aden R J. Weld J, 1983; 62: 72s
[16] Heiple C R, Roper J R. Weld J, 1981; 60: 143s
[17] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2006; 11: 389
[18] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2007; 12: 120
[19] Lu S P, Fujii H, Sugiyama H, Nogi K. Metall Mater Trans, 2003; 34A: 1901
[20] Lu S P, Fujii H, Sugiyama H, Tanaka M, Nogi K. ISIJ Int, 2003; 43: 1590
[21] Lu S P, Fujii H, Nogi K. Scr Mater, 2004; 51: 271
[22] Lu S P, Fujii H, Nogi K. Sci Technol Weld Join, 2004; 9: 272
[23] Lu S P, Fujii H, Nogi K. Mater Sci Eng, 2004; A380: 290
[24] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2006; 22: 359
[25] Lu S P, Fujii H, Nogi K, Sato T. Sci Technol Weld Join, 2007; 12: 689
[26] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2010; 26: 170
[27] Wu C H, Hao D Q. Physical Chemistry. 1st Ed., Beijing: Machine Building Press, 1988: 138, 287
(吴长春, 郝德庆. 物理化学. 第一版, 北京: 机械工业出版社, 1988: 138, 287)
[28] Kraus H G. Weld J, 1989; 68: 269s
[29] Bad’yanov B N, Davdov V A, Ivanov V A. Avtom Svarka, 1974; 1: 11
[30] Bad’yanov B N. Avtom Svarka, 1975; 1: 74
[31] Palmer T A, DebRoy T. Weld J, 1996; 75: 197s
[32] Sato Y, Dong W, Kokawa H, Kuwana T. ISIJ Int Suppl, 2000; 40: S20
[33] Wada H, Pehlke R D. Metall Trans, 1977; 8B: 675
[34] Dong W, Kokawa H, Sato Y, Tsukamoto S. Metall Mater Trans, 2003; 34B: 75
[35] Katz J D, Kiong T B. Metall Trans, 1989; 20B: 175
[36] Palmer T A, DebRoy T. Sci Technol Weld Join, 1998; 3: 190
[37] Zhu P Y, Lowke J J, Morrow R. J Phys, 1992; 25D: 1221
[38] Lowke J J, Kovitya P, Schmidt H P. J Phys, 1992; 25D: 1601
[39] Zhu P Y, Lowke J J, Morrow R, Haidar J. J Phys, 1995; 28D: 1369
[40] Lowke J J, Morrow R, Haidar J. J Phys, 1997; 30D: 2033
[41] Scott D A, Kovitya P, Haddad G N. J Appl Phys, 1989; 66: 5232
[42] McKelliget J, Szekely J. Metall Trans, 1986; 17A: 1139
[43] Bini R, Monno M, Boulos M I. J Phys, 2006; 39D: 3253
[44] Ushio M, Szekely J, Chang C W. Iron Steel, 1981; 6: 279
[45] Wu C S, Ushio M, Tanaka M. Compt Mater Sci, 1997; 7: 308
[46] Lu S P, Dong W C, Li D Z, Li Y Y. Compt Mater Sci, 2009; 45: 327
[47] Sahoo P, DebRoy T, McNallan M J. Metall Mater Trans, 1988; 19B: 483
[48] DongWC, Lu S P, Li D Z, Li Y Y. Acta Metall Sin, 2008; 44: 249
(董文超, 陆善平, 李殿中, 李依依. 金属学报, 2008; 44: 249)
[49] Lu S P, Dong W C, Li D Z, Li Y Y. Sci Tech Weld Join, 2009; 14: 509
[50] Hsu K C, Etemadi K, Pfender E. J Appl Phys, 1983; 54: 1293
[51] Nestor O H. J Appl Phys, 1962; 33: 1638 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|