| 温度梯度对定向凝固TiAl基合金片层取向的影响 |
| 肖志霞,郑立静,杨莉莉,闫洁,张虎 |
| 北京航空航天大学材料科学与工程学院空天材料与服役教育部重点实验室, 北京 100191 |
|
| EFFECTS OF TEMPERATURE GRADIENT ON LAMEL-LAR ORIENTATIONS OF DIRECTIONAL SOLIDIFIED TiAl–BASED ALLOY |
| XIAO Zhixia, ZHENG Lijing, YANG Lili, YAN Jie, ZHANG Hu |
Key Laboratory of Aerospace Materials and Performance (Ministry of Education), School of Materials Science and
Engineering, Beihang University, Beijing, 100191 |
引用本文:
肖志霞 郑立静 杨莉莉 闫洁 张虎. 温度梯度对定向凝固TiAl基合金片层取向的影响[J]. 金属学报, 2010, 46(10): 1223-1229.
,
,
,
,
.
EFFECTS OF TEMPERATURE GRADIENT ON LAMEL-LAR ORIENTATIONS OF DIRECTIONAL SOLIDIFIED TiAl–BASED ALLOY[J]. Acta Metall Sin, 2010, 46(10): 1223-1229.
| [1] Yamaguchi M, Inui H, Ito K. Acta mater, 2000; 48(1): 307
[2] Dimiduk D M. Mater Sci Eng A, 1999; 263(2): 281
[3] Kim Y W. JOM, 1995, 47(7): 39
[4] Yamaguchi M, Johnson D R, Lee H N, Inui H. Intermetallics, 2000; 8: 511
[5] Kishida K, Johnson D R, Masuda Y, Umeda H, Inui H, Yamaguchi M. Intermetallics, 1998; 6: 679
[6] Johnson D R., Inui H, Muto S, Omiya Y, Yamanaka T. Acta Mater, 2006; 54(4): 1077
[7] Lee H N, Johnson D R, Inui H, Oh M H, Wee D M, Yamaguchi M. Mater Sci Eng A, 2002; 329-331: 19
[8] Takeyama M, Yamamoto Y, Morishima H, Koike K, Chang S Y, Matsuo T. Mater Sci Eng A, 2002; 329-331: 7
[9] Lee H N, Johnson D R, Inui H, Oh M H, Wee D M, Yamaguchi M. Acta Mater, 2000; 48(12): 3221
[10] Jung I S, Oh M H, Park N J, Kumar K S, Wee D M. Met Mater Int, 2007; 13(6): 455
[11] Jung I S, Jang H S, Oh M H, Lee J H, Wee D M. Acta Mater, 2002; 329-331: 13
[12] Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, Wee D M. Mater Sci Eng A, 1997; 239-240: 570
[13] Saari H, Beddoes J, Seo D Y, Zhao L. Intermetallics, 2005; 13(9): 937
[14] Sastry S M L, Lipsitt H A. Metall Trans A, 1977; 8(2): 299
[15] Pan J S, Tong J M, Tian M B. Fundamentals of Materials Science. 3rd ed. Beijing: Tsinghua University Press, 2002: 40
(潘金生, 仝健民, 田民波. 材料科学基础. 第3版. 北京: 清华大学出版社, 2002: 40)
[16] Singh A K, Muraleedharan K, Banerjee D. Scripta Mater, 2003; 48: 767
[17] Henry S, Jarry P, Rappaz M. Metall Trans A, 1998; 29: 2807
[18] Henry S, Jarry P, Rappza M. Metall Trans A, 1997; 28: 207
[19] Henry S, Minghetti T, Rappaz M. Acta Mater, 1998; 46(18): 6431
[20] Hu H Q. the Principle of Metal Solidification. 2nd ed. Beijing: China Machine Press, 2000: 119
(胡汉起. 金属凝固原理. 第2版. 北京: 机械工业出版社, 2000: 119)
[21] Jiang C B, Zhou S Z, Zhang M C, Wang R, Acta Metall Sin, 1998; 34(2):164
(蒋成保, 周寿增, 张茂才, 王润. 金属学报, 1998: 34(2): 164)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|