Please wait a minute...
金属学报  2010, Vol. 46 Issue (11): 1422-1427    DOI: 10.3724/SP.J.1037.2010.00462
  综述 本期目录 | 过刊浏览 |
纳米孪晶金属材料
卢磊, 卢柯
中国科学院金属研究所沈阳材料科学(联合)实验室, 沈阳 110016
METALLIC MATERIALS WITH NANO--SCALE TWINS
LU Lei, LU Ke
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

卢磊 卢柯. 纳米孪晶金属材料[J]. 金属学报, 2010, 46(11): 1422-1427.
, . METALLIC MATERIALS WITH NANO--SCALE TWINS[J]. Acta Metall Sin, 2010, 46(11): 1422-1427.

全文: PDF(784 KB)  
摘要: 材料的强化通常是在材料内部引入各种缺陷以阻碍位错运动来实现, 如固溶强化、弥散强化、细晶强化和应变强化等,但这些传统的强化途径无可避免地会影响材料的塑性形变能力, 导致塑性和韧性的降低. 利用纳米尺度孪晶界面实现材料强化可避免上述缺点. 本文对纳米孪晶强化原理和纳米孪晶金属研究进展进行了简要综述, 分别讨论了纳米孪晶变形机制、纳米孪晶金属的部分力学行为(如强度、塑性、应变速率敏感性和加工硬化等)和物理性能(如导电性), 以及纳米孪晶金属的制备技术等相关问题.
关键词 : 纳米孪晶,  力学性能,  物理性能,  变形机理,  制备技术    
Abstract:Strengthening materials is a central objective of materials research. Traditional approaches to strengthen materials, including solid solution strengthening, second phase strengthening, grain refinement strengthening, dispersion strengthening and work hardening strengthening etc., aim at creation of internal defects and boundaries so as to obstruct the motion of dislocations. Such strategies for strengthening invariably compromise the ductility and electrical conductivity of the material. By reviewing recent advances in our understanding of nanostructured metals and alloys, we propose a novel approach to optimize the strength, ductility and the electrical conductivity of materials by means of coherent twin boundaries at nano-meter scale. We assess current understanding of strengthening mechanism of twin boundaries (instead of incoherent boundaries as conventionally used). Additionally, some mechanical properties (such as strength, ductility, strain rate sensitivity, work hardening) and the physical properties (electrical conductivity and electrical migration) as well as the relative preparation techniques of the metallic materials with nano-scale twins will be reviewed in this paper.
Key words: nano-twin    mechanical property    physical property    deformation mechanism    syntheses technique
收稿日期: 2010-09-09     
基金资助:

国家自然科学基金项目50725103, 50890171和51071153以及国家重点基础研究发展计划项目2005CB623604资助

作者简介: 卢磊, 女, 1970年生, 研究员, 博士
[1] Lu K, Lu L, Suresh S. Science, 2009; 324: 349 [2] Hall E O. Proc Phys Soc London, 1951; 64B: 747 [3] Petch N J. J Iron Steel Inst, 1953; 174: 25 [4] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427 [5] Wei Q, Cheng S, Ramesh K T, Ma E. Mater Sci Eng, 2004; A381: 71 [6] Chen J, Lu L, Lu K. Scr Mater, 2006; 54: 1913 [7] Koch C C, Morris D G, Lu K, Inoue A. MRS Bull, 1999; 24: 54 [8] Koch C C. Scr Mater, 2003; 49: 657 [9] Ma E. Scr Mater, 2003; 49: 663 [10] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1 [11] Meyers M A, Chawla K K. Mechanical Behavior of Materials. Upper Saddle River, New Jersey: Pretice Hall, 1999: 1 [12] Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science, 2004; 304: 422 [13] Shen Y F, Lu L, Lu Q H, Jin Z H, Lu K. Scr Mater, 2005; 52: 989 [14] Jin Z H, Gumbsch P, Albe K, Ma E, Lu K, Gleiter H, Hahn H. Acta Mater, 2008; 56: 1126 [15] Jin Z H, Gumbsch P, Ma E, Albe K, Lu K, Hahn H, Gleiter H. Scr Mater, 2006; 54: 1163 [16] Lu L, Schwaiger R, Shan Z W, Dao M, Lu K, Suresh S. Acta Mater, 2005; 3: 2169 [17] Zhang X, Wang H, Chen X H, Lu L, Lu K, Hoagland R G, Misra A. Appl Phys Lett, 2006; 88: 173116 [18] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607 [19] Li X,Wei Y, Lu L, Lu K, Gao H. Nature, 2010; 464: 877 [20] Shen Y F, Lu L, Dao M, Suresh S. Scr Mater, 2006; 55: 319 [21] Lu L, Dao M, Zhu T, Li J. Scr Mater, 2009; 60: 1062 [22] Lu L, Zhu T, Shen Y F, Dao M, Lu K, Suresh S. Acta Mater, 2009; 57: 5165 [23] Zhao W S, Tao N R, Guo J Y, Lu Q H, Lu K. Scr Mater, 2005; 53: 745 [24] Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771 [25] Zhang Y, Tao N R, Lu K. Acta Mater, 2008; 56: 2429 [26] Li Y S, Tao N R, Lu K. Acta Mater, 2008; 56: 230 [27] Qin E W, Lu L, Tao N R, Lu K. Scr Mater, 2009; 60: 539 [28] Qin E W, Lu L, Tao N R, Tan J, Lu K. Acta Mater, 2009; 57: 6215 [29] Ustinov A I, Skorodzievski V S, Fesiun E V. Acta Mater, 2008; 56: 3770 [30] Dao M, Lu L, Shen Y F, Suresh S. Acta Mater, 2006; 54: 5421 [31] Chen K C, Wu W W, Liao C N, Chen L J, Tu K N. Science, 2008; 321: 1066 [32] Zhang X, Misra A,Wang H, Shen T D, Nastasi M, Mitchell T E, Hirth J P, Hoagland R G, Embury J D. Acta Mater, 2004; 52: 995 [33] Zhang X, Misra A, Wang H, Lima A L, Hundley M F, Hoagland R G. J Appl Phys, 2005; 97: 094302 [34] Zhang X, Anderoglu O, Misra A, Wang H. Appl Phys Lett, 2007; 90: 153101 [35] Li Y S, Zhang Y, Tao N R, Lu K. Acta Mater, 2009; 57: 761 [36] Hong C S, Tao N R, Huang X, Lu K. Acta Mater, 2010; 58: 3103 [37] Zhang Y, Tao N R, Lu K. Scr Mater, 2009; 60: 211 [38] Hong C S, Tao N R, Lu K, Huang X. Scr Mater, 2009; 61: 289
[1] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[7] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[9] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[10] 刘俊鹏, 陈浩, 张弛, 杨志刚, 张勇, 戴兰宏. 高熵合金的低温塑性变形机制及强韧化研究进展[J]. 金属学报, 2023, 59(6): 727-743.
[11] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[12] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[13] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[14] 万涛, 程钊, 卢磊. 组元占比对层状纳米孪晶Cu力学行为的影响[J]. 金属学报, 2023, 59(4): 567-576.
[15] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.