Bi2O3涂覆Al18B4O33晶须增强铝基复合材料的阻尼性能 |
刘刚1, 孙雅丽2, 胡津1, 周科1 |
1. 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001
2. 烟台工程职业技术学院机制工艺系, 烟台 264006 |
|
DAMPING CAPACITY OF Bi2O3–COATED Al18B4O33 WHISKER REINFORCED Al MATRIX COMPOSITES |
LIU Gang 1, SUN Yali 2, HU Jin 1, ZHOU Ke 1 |
1. School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
2. Department of Mechanical Technology, Yantai Engineering & Technology College, Yantai 264006 |
引用本文:
刘刚 孙雅丽 胡津 周科. Bi2O3涂覆Al18B4O33晶须增强铝基复合材料的阻尼性能[J]. 金属学报, 2010, 46(8): 979-983.
,
,
,
.
DAMPING CAPACITY OF Bi2O3–COATED Al18B4O33 WHISKER REINFORCED Al MATRIX COMPOSITES[J]. Acta Metall Sin, 2010, 46(8): 979-983.
[1] Deo N and Vakil S, Scr. Mater, 1999; 40: 791
[2] Starink M J, Wang P, Sinclair I and Gregson P J, Acta Mater, 1999; 47: 3841
[3] Arsenault R J and Shi N, Mater. Sci. Eng, 1986; A 81: 175
[4] Gu J H, Zhang X N and Gu M Y, J. Alloy. Compd, 2004; 381: 182
[5] Parrina L and Schaller R, Acta Mater, 1996; 44: 4881
[6] Carreno-morelli E, Urreta S E and Schaller R, Acta Mater, 2000; 48: 4725
[7] Zhang X Q, Wang H W, Liao L H and Ma N H, Compos. Sci. Technol, 2007; 67: 720
[8] Gu J H, Zhang X N and Gu M Y, Mater. Lett, 2005; 59: 180
[9] Gu J H, Zhang X N, Qiu Y F and Gu M Y, Compos. Sci. Technol, 2005; 65: 1736
[10] Zhang X N, Wu R J,Li X C, Guo Z X, Science in China (Series E: Technological Sciences) 2002; 32: 14-19
(张小农,吴人洁,李小璀, Z X Guo, 中国科学(E 辑),2002; 32:14-19).
[11] Gu J H, Zhang X N, Gu M Y, Journal of Aeronautical Materials, 2004; 24(6): 29-33.
(顾金海,张小农,顾明元, 航空材料学报, 2004; 24(6): 29-33)
[12] Hu J, Wang X F, Comp Sci Tech, 2008; 68: 2297-2299.
[13]Liu G, Ren W C, Hu J, Mater Sci Eng A, 2010 under reviewer
[14] Hu J, Wang X F and Zheng Z Z, J Appl Phys, 2010 in press
[15] Zhang J M, Perez R J, Wong C R and Lavernia E J, Mater. Sci. Eng, 1994; R13: 325
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|