| 一步法制备含扩散阻挡层的多层体系及其界面结合强度 |
| 李伟洲1; 2); 王启民1); 宫骏1); 孙超1); 姜辛3) |
1) 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016
2) 广西大学有色金属及材料加工新技术教育部重点实验室; 南宁 530004
3) Institute of Materials Engineering; University of Siegen; Siegen 57076; Germany |
|
| ONE-STEP DEPOSITION AND INTERFACIAL ADHESIVE STRENGTH OF THE MULTILAYER SYSTEM WITH A DIFFUSION BARRIER |
| LI Weizhou1; 2); WANG Qimin1); GONG Jun1); SUN Chao1); JIANG Xin3) |
1) State Key Laboratory for Corrosion and Protection; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
2) Key Laboratory of New Processing Technology for Nonferrous Metals and Materials; Ministry of Education; Guangxi University; Nanning 530004
3) Institute of Materials Engineering; University of Siegen; Siegen 57076; Germany |
引用本文:
李伟洲 王启民 宫骏 孙超 姜辛. 一步法制备含扩散阻挡层的多层体系及其界面结合强度[J]. 金属学报, 2010, 46(5): 561-568.
,
,
,
,
.
ONE-STEP DEPOSITION AND INTERFACIAL ADHESIVE STRENGTH OF THE MULTILAYER SYSTEM WITH A DIFFUSION BARRIER[J]. Acta Metall Sin, 2010, 46(5): 561-568.
| [1] Knotek O, Loffler F, Beele W. Surf Coat Technol, 1993; 61: 6
[2] Li S S, Song J X, Zhou C G, Gong S K, Han Y F. Intermetallics, 2005; 13: 309
[3] Sloof W G. Self Healing in Coating at High Temperatures: Self Healing Materials. Netherlands: Springer, 2007: 309
[4] Nicholls J R. MRS Bull, 2003; 28: 659
[5] Wang Q M,Wu Y N, Ji A L, Ke P L, Sun C, Huang R F, Wen L S. Acta Metall Sin, 2004; 40: 83
(王启民, 武颖娜, 纪爱玲, 柯培玲, 孙超, 黄荣芳, 闻立时. 金属学报, 2004; 40: 83)
[6] Li W Z, Yao Y, Wang Q M, Bao Z B, Gong J, Sun C, Jiang X. J Mater Res, 2008; 23: 341
[7] Li W Z, Yao Y, Li Y Q, Li J B, Gong J, Sun C, Jiang X. Mater Sci Eng, 2009; A512: 117
[8] Yao Y, Li W Z, Wang Q M, Gong J, Sun C, Li J B. Acta Metall Sin, 2008; 44: 876
(姚勇, 李伟洲, 王启民, 宫骏, 孙 超, 李家宝. 金属学报, 2008; 44: 876)
[9] Zhang K, Wang Q M, Sun C, Wang F H. Corros Sci, 2008; 50: 1707
[10] Sun C, Wang Q M, Tang Y J, Guan Q F, Gong J, Wen L S. Acta Metall Sin, 2005; 41: 1167
(孙超, 王启民, 唐永吉, 关庆丰, 宫 骏, 闻立时. 金属学报. 2005; 41: 1167)
[11] Ren X, Wang F H. Surf Coat Technol, 2006; 201: 30
[12] Yao Y. Master Dissertation. Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008
(姚勇. 中国科学院金属研究所硕士学位论文, 沈阳, 2008)
[13] Peng X, Wang F H, Clark D K. Acta Metall Sin, 2003; 39: 1055
(彭 晓, 王福会, Clarke D R. 金属学报. 2003; 39: 1055)
[14] Cremer R, Witthaut M, Reichert K, Schierling M, Neuschutz D. Surf Coat Technol, 1998; 108–109: 48
[15] Xie L, Sohn Y, Jordan E H, Gell M. Surf Coat Technol, 2003; 176: 57
[16] Evans A G, Mumm D R, Hutchinson J W, Meier G H, Pettit F S. Prog Mater Sci, 2001; 46: 505 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|