| 微观组织对7075铝合金的屈服强度和抗应力腐蚀性能的影响 |
| 华明建;李春志;王鸿渐 |
| 北京航空材料研究所;北京81号信箱;北京航空材料研究所;北京航空材料研究所 |
|
| EFFECT OF MICROSTRUCTURES ON THE YIELD STRENGTH AND SCR OF 7075 ALUMINIUM ALLOY |
| HUA Mingjian Institute of Aeronoutical Materials;Beijing;Post Box NO.81;LI Chunzhi;WANG Hongjian Institute of Aeronautical Materials; Beijing |
引用本文:
华明建;李春志;王鸿渐. 微观组织对7075铝合金的屈服强度和抗应力腐蚀性能的影响[J]. 金属学报, 1988, 24(1): 41-46.
,
,
.
EFFECT OF MICROSTRUCTURES ON THE YIELD STRENGTH AND SCR OF 7075 ALUMINIUM ALLOY[J]. Acta Metall Sin, 1988, 24(1): 41-46.
1 李春志.金属学报,1985;21:B233 2 Allen S M. Phil. Mag., 1981; 43: 325 3 Adler P, DeIasi R, Geschwind G. AD732321. Nov. 1971 4 Speidel M O. In: Scully J C ed. The Theory of SCC in Alloys, Erussel: NATC Sci, Affairs Division. 1971: 289 5 Hirsch P B, Humphreys F J. Physics of Strength and Plasticity. MIT Press, 1969: 189 6 Gerold V, Haberkorn V. Phys. Status Solidi, 1960; 16: 675 7 Park J K, Ardell A J. Metall Trans, 1983; 14A: 1957 8 Hua Mingjian, Li Chunzhi, Yan Minggao. In: the Secretariate of BCEIA ed. Froc. of Beijing Conf. and Exhibition on Instrumental Analysis, Beijing, Nov. 1985: Vol. 1, 102r |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|