| 铬钢的高温冲蚀腐蚀行为 |
| 满永发;A.V.LEVY |
| 中国科学院金属研究所;副研究员;沈阳文化路;加利福尼亚大学 |
|
| HIGH TEMPERATURE CORROSION-EROSION BEHAVIOR OF Cr-BEARING STEELS |
| A. V. LEVY Institute of Metal Research; Academia Sinica. Shenyang; Lawrence Berkely Lab.; University of California; USAMAN Yongfa Associate Professor;Istitute of Metal research;Academia Sintea;shenyang |
引用本文:
满永发;A.V.LEVY. 铬钢的高温冲蚀腐蚀行为[J]. 金属学报, 1988, 24(1): 34-40.
,
.
HIGH TEMPERATURE CORROSION-EROSION BEHAVIOR OF Cr-BEARING STEELS[J]. Acta Metall Sin, 1988, 24(1): 34-40.
1 Maasberg J A, Levy A V. Wear, 1981; 73: 355 2 Nagarajan Y, Wright I G. In: Rapp R A ed., High Temperature Corrosion, NACE, 1983: 398--405 3 Hill V L, Verely E J Jr. In: Proceedings of Corrosion Erosion Behavior of Materials, St Lours USA 1978: 695 4 Tabakoff W, Vittal B V R. Wear, 1983; 86: 89 5 Wright I G, Nagarajan V. In: Proceedings of Corrosion Erosion Behavior of Materjals. St Lours USA, 1978: 269 6 Ives L K, Ruff A W. In: Adler W F ed., Erosion: Frevention and Useful Application, ASTM STP 664, ASTM, 1979: 5 7 Hutchings I. In: Adler W F ed., Frosion: Prevention and Useful Application, ASTM STP--664, ASTM, 1979: 59 8 Khanna A S, Jha B B, Kaj B. Oxid Met, 1985 23: 159 9 Kuroda K, Labun P A. Welsch G, Mitchell T E. Oxid Met, 1983: 19: 117 10 Levy A V, Man Y F. Wear, 1986; 111: 135 11 Levy A V, Man Y F. NACE Corrosion 85, paper №338, Boston MA 1985 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|