| 硼对快凝Ni_3Al组织结构及力学性能的影响 |
| 李辉;刘祥;郭建亭;胡壮麒 |
| 中国科学院金属研究所;东北工学院;中国科学院金属研究所;副研究员;沈阳文化路;中国科学院金属研究所 |
|
| INFLUENCE OF BORON ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF RAPIDLY SOLIDIFIED Ni_3Al |
| LI Hui;LIU Xiang;GUO Jianting;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang Northeast Institute of Technology; Shenyang Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
李辉;刘祥;郭建亭;胡壮麒. 硼对快凝Ni_3Al组织结构及力学性能的影响[J]. 金属学报, 1989, 25(1): 25-30.
,
,
,
.
INFLUENCE OF BORON ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF RAPIDLY SOLIDIFIED Ni_3Al[J]. Acta Metall Sin, 1989, 25(1): 25-30.
1 Pope D P. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys Ⅱ. Proc of MRS, Vol. 81, Mars, Pennsylvania: Choice Book, 1987: 93 2 Pope D P, Ezz S S. Int Metall Rev, 1984; 29 (3) : 137 3 Takaougi T, Izumi O, Masdhashi N, Acta Metall, 1985; 33: 1259 4 Talasugi T, Izumi O. Acta Metall, 1985; 33: 1247 5 Liu C T. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys Ⅱ, Proc of MRS, Vol. 81, Mars, Pennsylvania: Choice Book, 1987; 355 6 McLean M, Strang A. Met Tech, 1984; 11 (10) : 414 7 Sikka V K. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys Ⅱ, Proc of MRS, Vol. 81, Mars, Pennsylvania: Choice Book. 1987: 487 8 Liu C T. J Met, 1986; 38 (5) : 19 9 Inoue A, Tomioka H, Maoumoto T. Metall Trans, 1983: 14A: 1367 10 Cahn R W. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys, Ⅱ, Proc of MRS, Vol. 81, Mars, Pennsylvania: Choice Book, 1987: 27 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|