| 激光熔化处理对灰铸铁显微组织的影响 |
| 沈莲;李成劳;王秀苓;马丽华;朱道珍 |
| 西安交通大学材料系;副教授;西安交通大学;西安交通大学;西安交通大学;西安交通大学 |
|
| EFFECT OF LASER MELTING PROCESSING ON MICROSTRUCTURE OF GRAY CAST IRON |
| SHEN Lian;LI Chenglao;WANG Xiuling;MA Lihua;ZHU Daozhen Xi'an Jiaotong University |
引用本文:
沈莲;李成劳;王秀苓;马丽华;朱道珍. 激光熔化处理对灰铸铁显微组织的影响[J]. 金属学报, 1989, 25(1): 75-77.
,
,
,
,
.
EFFECT OF LASER MELTING PROCESSING ON MICROSTRUCTURE OF GRAY CAST IRON[J]. Acta Metall Sin, 1989, 25(1): 75-77.