| MB15镁合金的相组成及其微观形态 |
| 张少卿 |
| 北京航空材料研究所;高级工程师;北京(100095) |
|
| PHASE CONSTITUTION AND MORPHOLOGIES OF Mg-Zn-Zr ALLOY (MB15) |
| ZHANG Shaoqing Institute of Aeronautical Materials; Beijing ZHANG Shaoqing; Institute of Aeronautical Materlols. P. O. Box No.81; 100095 Beijing |
引用本文:
张少卿. MB15镁合金的相组成及其微观形态[J]. 金属学报, 1989, 25(5): 36-41.
.
PHASE CONSTITUTION AND MORPHOLOGIES OF Mg-Zn-Zr ALLOY (MB15)[J]. Acta Metall Sin, 1989, 25(5): 36-41.
1 Emley E F. Principles of Magnesium Technology, London: Pergamon, 1966: 979 2 Bhambri AK, Kattamis T Z. AD 734770, 1971 3 #12 4 #12 5 Sturkey L. TMS AIME, 1960: 218: 466 6 Koster W, Muller F. Z Metallk, 1948; 39: 352 7 Clark J B. Acta Metall, 1965; 13: 1281 8 高桥恒夫,小岛阳,鹰西清.轻金属,1973;23:376 |
|