| TiAl-V金属间化合物的高温变形行为 |
| 蒲忠杰;蔡其巩;朱静 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| DEFORMATION BEHAVIOUR OF TiAl-V INTERMETALLIC COMPOUND AT ELEVATED TEMPERATURE |
| PU Zhongjie;CAI Qigong;ZHU Jing Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing PU Zhongjie; Laboratory of Physics; Central Iron and Steel Research Institute;Ministry of Metallurgical Industry; 100081 Beijing |
引用本文:
蒲忠杰;蔡其巩;朱静. TiAl-V金属间化合物的高温变形行为[J]. 金属学报, 1989, 25(5): 149-151.
,
,
.
DEFORMATION BEHAVIOUR OF TiAl-V INTERMETALLIC COMPOUND AT ELEVATED TEMPERATURE[J]. Acta Metall Sin, 1989, 25(5): 149-151.
1 Lipsitt H A, Shechtman D, Schafrik R E. Metall Trans, 1975; 6A: 1991 2 Blackburn M J, Smith M P. US Pat, 1981: №. 4294615 3 Martin P L, Mendiratta M G, Lipsitt H A. Metall Trans, 1983; 14A: 2170 4 Sauthoff G. Z Metallk, 1986; 77: 65 |
|