| Ll_0型TiAl金属间化合物的高温形变行为 |
| 郝士明;郑占青 |
| 东北工学院材料科学与工程系;教授;沈阳(110006);东北工学院 |
|
| HIGH TEMPERATURE DEFORMATION BEHAVIOUR OF TiAl INTERMETALLIC COMPOUND |
| HAO Shiming;ZHENG Zhanqing Northeast University of Technology; Shenyang professor; Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006 |
引用本文:
郝士明;郑占青. Ll_0型TiAl金属间化合物的高温形变行为[J]. 金属学报, 1990, 26(3): 131-135.
,
.
HIGH TEMPERATURE DEFORMATION BEHAVIOUR OF TiAl INTERMETALLIC COMPOUND[J]. Acta Metall Sin, 1990, 26(3): 131-135.