| 热弹性马氏体的长大 |
| 邓永瑞;G.S.ANSELL |
| 北京科技大学材料系;ColoradoSchoolofMines |
|
| GROWTH OF THERMOELASTIC MARTENSITE |
| DENG Yongrui;G. S. ANSELL University of Science and Technology Beijing Colorado School of Mines; Golden; CO 80401; USA |
引用本文:
邓永瑞;G.S.ANSELL. 热弹性马氏体的长大[J]. 金属学报, 1990, 26(5): 70-72.
,
.
GROWTH OF THERMOELASTIC MARTENSITE[J]. Acta Metall Sin, 1990, 26(5): 70-72.
1 Kaufman L, Cohen M. Prog Met Phys, 1958; 7: 165 2 Olson G B, Cohen M. Scr Metall, 1975; 9: 1247 3 Olson G B, Cohen M. Scr Metall, 1977; 11: 345 4 Ling H C, Owen W S. Acta Metall, 1981; 29: 1721 5 Eshelby J D. Prog Solid Mech, 1961; 2: 87 6 Eshelby J D. Proc R Soc, London, Ser. A, 1959; 252: 561 7 Eshelby J D. Proc R Soc, London, Ser. A, 1957; 241: 376 8 Deng Y, Ansell G S. Acta Metall, 1990; 38: 69 9 Deng Y. Doctoral Thesis, Rensselaer Polytechnic Institute, USA, 1984 10 Wayman C M, Tong H C. Scr Metall, 1977; 11: 341> |
|