| Cr12MoV钢激光熔凝层的显微组织 |
| 李晓东;尹钟大 |
| 哈尔滨工业大学金属材料及工艺系;讲师哈尔滨150006;哈尔滨工业大学 |
|
| MICROSTRUCTURE OF LASER MELTED LAYER ON Cr12MoV STEEL |
| LI Xiaodong;YIN Zhongda Harbin Institute of Technology |
引用本文:
李晓东;尹钟大. Cr12MoV钢激光熔凝层的显微组织[J]. 金属学报, 1991, 27(1): 72-74.
,
.
MICROSTRUCTURE OF LASER MELTED LAYER ON Cr12MoV STEEL[J]. Acta Metall Sin, 1991, 27(1): 72-74.