| 高炉低钛渣脱硫的动力学研究 |
| 鄢毓璋;兰洪 |
| 重庆大学;重庆大学 |
|
| KINETICS OF DESULPHURIZING REACTION OF BLAST FURNACE LOW TITANIA SLAG |
| YAN Yuzhang;LAN Hong Chongqing University |
引用本文:
鄢毓璋;兰洪. 高炉低钛渣脱硫的动力学研究[J]. 金属学报, 1991, 27(4): 80-83.
,
.
KINETICS OF DESULPHURIZING REACTION OF BLAST FURNACE LOW TITANIA SLAG[J]. Acta Metall Sin, 1991, 27(4): 80-83.