| 高炉型含钛炉渣中MnO对TiO_2还原的影响 |
| 杜鹤桂;邹安华 |
| 东北工学院;东北工学院 |
|
| INFLUENCE OF MnO ON REDUCTION OF TiO_2 IN Ti-CONTAINING SLAG OF BLAST FURNACE TYPE |
| DU Hegui;ZOU Anhua Northeast University of Technology; Shenyang |
引用本文:
杜鹤桂;邹安华. 高炉型含钛炉渣中MnO对TiO_2还原的影响[J]. 金属学报, 1991, 27(4): 73-79.
,
.
INFLUENCE OF MnO ON REDUCTION OF TiO_2 IN Ti-CONTAINING SLAG OF BLAST FURNACE TYPE[J]. Acta Metall Sin, 1991, 27(4): 73-79.
1 田村庸,中村成子.铁钢,1985;71(12) :S934 2 Bell H B.Iron and Steel.1963;36:643 3 彭瑞伍,邹元爔.全国第一届冶金过程物理化学学术报告论文集,上海:上海科学技术出版社,1965:410-411 4 莫培根,陈钧珊.全国第一届冶金过程物理化学学术报告论文集,上海;上海科学技术出版社,1965:339 5 黄希祜.钢铁冶金原理.北京:冶金工业出版社,1981:159 6 Sommerville I D, Grieveson P, Taylor J. Ironmaking and Steelmaking, 1980; 7: 25 7 万谷志郎.熔渣热力学.东北工学院内部资料,1984 |
|