| 应力松驰与非晶态Fe_(79)B_(16)Si_5合金磁性优化 |
| 车晓舟 |
| 上海交通大学 |
|
| STRESS RELIEF AND MAGNETISM OPTIMIZATION OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY |
| CHE Hiaozhou(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1994-12-09; in revised forrn 1995-03-27) |
引用本文:
车晓舟. 应力松驰与非晶态Fe_(79)B_(16)Si_5合金磁性优化[J]. 金属学报, 1995, 31(21): 418-422.
.
STRESS RELIEF AND MAGNETISM OPTIMIZATION OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY[J]. Acta Metall Sin, 1995, 31(21): 418-422.
| 1林肇华,戴道生,物理学报,1982;31:8712FujimoriH.In:LubroskyFEed.,AmorphousMetallicAlloys,London:Butterworth&CoLtd,1983:3003FujimoriH.In:SteebS,WarlimontHeds.,RapidlyQuenchedMetals,Amsterdam:ElsevierSci-encePublishersBV,1985:11014LuborsiyFE.IEEETransMagnMAG-11,1975;6:16445SongJS,ParkJW,ImHB.ScriptaMetall,1991,25(1):736HuangDR,LiJCM.ScriptaMetall,1990;24:1137 |
|