Please wait a minute...
金属学报  2026, Vol. 62 Issue (5): 721-732    DOI: 10.11900/0412.1961.2025.00367
  综述 本期目录 | 过刊浏览 |
TiAl合金疲劳小裂纹行为
相恒高1,2,3, 宋伟东1,2,3, 加陆毅1,2,3, 祁志祥1,2,3, 陈旸1,2,3(), 周冰1,2,3, 郑功1,2,3, 应盼1,2,3, 陈光1,2,3
1 南京理工大学 高温轻合金及应用技术全国重点实验室南京研究基地 南京 210094
2 南京理工大学 高端装备铸造技术全国重点实验室 南京 210094
3 南京百炼实验室 南京 210094
Fatigue Small Crack Behavior of TiAl Alloys
XIANG Henggao1,2,3, Song Weidong1,2,3, JIA Luyi1,2,3, QI Zhixiang1,2,3, CHEN Yang1,2,3(), ZHOU Bing1,2,3, ZHENG Gong1,2,3, YING Pan1,2,3, CHEN Guang1,2,3
1 State Key Laboratory of Light Superalloys, Nanjing Research Base, Nanjing University of Science and Technology, Nanjing 210094, China
2 National Key Laboratory of Advanced Casting Technologies, Nanjing University of Science and Technology, Nanjing 210094, China
3 Nanjing Belight Laboratory, Nanjing 210094, China
引用本文:

相恒高, 宋伟东, 加陆毅, 祁志祥, 陈旸, 周冰, 郑功, 应盼, 陈光. TiAl合金疲劳小裂纹行为[J]. 金属学报, 2026, 62(5): 721-732.
Henggao XIANG, Weidong Song, Luyi JIA, Zhixiang QI, Yang CHEN, Bing ZHOU, Gong ZHENG, Pan YING, Guang CHEN. Fatigue Small Crack Behavior of TiAl Alloys[J]. Acta Metall Sin, 2026, 62(5): 721-732.

全文: PDF(2273 KB)   HTML
摘要: 

TiAl合金具有密度低、抗蠕变和耐腐蚀性能优异等特点,是空天动力领域轻量化发展的重要材料。疲劳是航空发动机叶片第一失效形式,叶片一旦出现长裂纹便会发生瞬时断裂,疲劳小裂纹的萌生和扩展直接决定叶片的使用寿命。本文围绕TiAl合金疲劳小裂纹问题,系统介绍了疲劳小裂纹的定义及特点,归纳总结了TiAl合金疲劳小裂纹的萌生和扩展机理、疲劳小裂纹扩展模型及其适用范围。最后,对TiAl合金疲劳小裂纹萌生、扩展机理表征和统一寿命预测模型进行了展望。

关键词 : TiAl合金,  疲劳小裂纹,  萌生机理,  扩展机理,  预测模型    
Abstract:

TiAl alloys are important lightweight materials for aerospace propulsion systems owing to their low density, creep resistance, corrosion resistance, and other properties. Fatigue is the primary failure mode of aeroengine blades. Once a long crack forms in a blade, rapid fracture can occur. The initiation and propagation of small fatigue cracks therefore directly determine the service life of blades. Focusing on the issue of small fatigue cracks in TiAl alloys, this paper systematically reviews the definition and characteristics of small fatigue cracks and summarizes the mechanisms of crack initiation and propagation in TiAl alloys. In addition, the propagation models of small fatigue cracks, together with their applicability and limitations, are discussed. Finally, future perspectives are presented regarding the characterization of fatigue small-crack initiation and propagation behavior and the development of unified life prediction methods for TiAl alloys.

Key words: TiAl alloy    fatigue small crack    initiation mechanism    propagation mechanism    prediction model
收稿日期: 2025-11-12     
ZTFLH:  TG146.2+3  
基金资助:国家自然科学基金项目(12202201);国家自然科学基金项目(52571145);国家自然科学基金项目(92463301);国家自然科学基金项目(52433016);国家自然科学基金项目(92163215);国家自然科学基金项目(52305379);国家自然科学基金项目(52174364);国家自然科学基金项目(52595663);江苏省自然科学基金项目(BK20243066);江苏省自然科学基金项目(BE2023024);高温轻合金及应用技术全国重点实验室开放基金项目(Sysjj2025203);高温轻合金及应用技术全国重点实验室开放基金项目(Sysjj2025101)
通讯作者: 陈 旸,男, yang.chen@njust.edu.cn,主要从事空天动力材料与应用技术研究
Corresponding author: CHEN Yang, professor, Tel: (025)84315159, E-mail: yang.chen@njust.edu.cn
作者简介: 相恒高,男,1991年生,教授,博士
第一联系人:宋伟东(共同第一作者),男,1997年生,博士加陆毅(共同第一作者),男,2003年生,博士
图1  小裂纹和长裂纹的疲劳裂纹扩展速率[10]
图2  全片层Ti-47Al-2Nb-2Cr-0.2B合金中表面萌生的疲劳小裂纹[33]
图3  Ti-46Al-4Nb-1.8Cr-0.2Ta合金中疲劳小裂纹在片层团界处萌生及扩展的示意图[37]
图4  TiAl合金小裂纹萌生位置示意图
图5  Ti-45Al-5Nb-0.2C-0.2B合金中不同片层取向下小裂纹萌生位置的数量[34]
图6  Ti-46.5Al-2.5V-1.0Cr合金中小裂纹的扩展速率[34]
图7  晶界的倾斜角和扭转角对小裂纹扩展行为的影响[50]
图8  全片层TiAl合金中不同应力比下长裂纹和小裂纹的疲劳裂纹扩展速率[21]
图9  TiAl合金中界面阻碍小裂纹扩展的示意图
图10  基于Newman模型的铝合金中表面小裂纹和长裂纹的裂纹扩展速率[66]
图11  7075-T6合金裂纹扩展速率预测[70]
[1] Chen G, Peng Y B, Zheng G, et al. Polysynthetic twinned TiAl single crystals for high-temperature applications [J]. Nat. Mater., 2016, 15: 876
doi: 10.1038/nmat4677 pmid: 27322822
[2] Kear B H, Thompson E R. Aircraft gas turbine materials and processes [J]. Science, 1980, 208: 847
pmid: 17772808
[3] Lasalmonie A. Intermetallics: Why is it so difficult to introduce them in gas turbine engines? [J]. Intermetallics, 2006, 14: 1123
doi: 10.1016/j.intermet.2006.01.064
[4] Chen Y Y, Shi G H, Du Z M, et al. Research progress on additive manufacturing TiAl alloy [J]. Acta Metall. Sin., 2024, 60: 1
doi: 10.11900/0412.1961.2022.00582
[4] 陈玉勇, 时国浩, 杜之明 等. 增材制造TiAl合金的研究进展 [J]. 金属学报, 2024, 60: 1
doi: 10.11900/0412.1961.2022.00582
[5] Chen G, Chen F R, Zhu D M, et al. Polysynthetic twinned high-performance TiAl alloy with ordered structures of functional units [J]. Acta Metall. Sin., 2026, 62: 541
doi: 10.11900/0412.1961.2026.00048
[5] 陈 光, 陈奉锐, 朱德民 等. 聚片孪生功能基元序构的高性能TiAl合金 [J]. 金属学报, 2026, 62: 541
[6] Bewlay B P, Nag S, Suzuki A, et al. TiAl alloys in commercial aircraft engines [J]. Mater. High Temp., 2016, 33: 549
doi: 10.1080/09603409.2016.1183068
[7] Ma N N, Tao C H, He Y H, et al. Research progress of multiaxial fatigue test methods on blades of aviation engine [J]. J. Aeronaut. Mater., 2012, 32(6): 44
[7] 马楠楠, 陶春虎, 何玉怀 等. 航空发动机叶片多轴疲劳试验研究进展 [J]. 航空材料学报, 2012, 32(6): 44
doi: 10.3969/j.issn.1005-5053.2012.6.006
[8] Miller K J. The behaviour of short fatigue cracks and their initiation part II—A general summary [J]. Fatigue Fract. Eng. Mater. Struct., 1987, 10: 93
doi: 10.1111/ffe.1987.10.issue-2
[9] Xu L, Huang S J, Hui L, et al. Small fatigue crack growth behavior of TB6 titanium alloy [J]. J. Mater. Eng., 2019, 47(11): 171
doi: 10.11868/j.issn.1001-4381.2016.000866
[9] 许 良, 黄双君, 回 丽 等. TB6钛合金疲劳小裂纹扩展行为 [J]. 材料工程, 2019, 47(11): 171
[10] Meyers M A, Chawla K K, translated by Zhang Z F, Lu L. Mechanical Behavior of Materials [M]. 2nd Ed., Beijing: Higher Education Press, 2017: 787
[10] Meyers M A, Chawla K K著, 张哲峰, 卢 磊 译. 材料的力学行为 [M]. 第2版. 北京: 高等教育出版社, 2017: 787
[11] Kruzic J J, Campbell J P, Ritchie R O. On the fatigue behavior of γ-based titanium aluminides: Role of small cracks [J]. Acta Mater., 1999, 47: 801
doi: 10.1016/S1359-6454(98)00409-1
[12] Pearson S. Initiation of fatigue cracks in commercial aluminium alloys and the subsequent propagation of very short cracks [J]. Eng. Fract. Mech., 1975, 7: 235
doi: 10.1016/0013-7944(75)90004-1
[13] Wu X R, Newman J C, Zhao W, et al. Small‐crack growth and fatigue life predictions for high‐strength aluminium alloys. Part II: Crack closure and fatigue analyses [J]. Fatigue Fract. Eng. Mater. Struct., 2000, 23: 59
doi: 10.1046/j.1460-2695.2000.00242.x
[14] Findley K O, Evans J L, Saxena A. A critical assessment of fatigue crack nucleation and growth models for Ni- and Ni,Fe-based superalloys [J]. Int. Mater. Rev., 2011, 56: 49
doi: 10.1179/095066010X12777205875796
[15] Hironobu N, Masahiro G, Norio K. A small-crack growth law and its related phenomena [J]. Eng. Fract. Mech., 1992, 41(4): 499
doi: 10.1016/0013-7944(92)90297-R
[16] Hanlon T, Tabachnikova E D, Suresh S. Fatigue behavior of nanocrystalline metals and alloys [J]. Int. J. Fatigue, 2005, 27: 1147
doi: 10.1016/j.ijfatigue.2005.06.035
[17] Yang Q Z, Yang X G, Huang W Q, et al. Propagation behaviors of small cracks in powder metallurgy nickel-based superalloy FGH4096 [J]. Acta Metall. Sin., 2022, 58: 683
doi: 10.11900/0412.1961.2021.00221
[17] 杨秦政, 杨晓光, 黄渭清 等. 粉末高温合金FGH4096的疲劳小裂纹扩展行为 [J]. 金属学报, 2022, 58: 683
doi: 10.11900/0412.1961.2021.00221
[18] Tokaji K, Ogawa T, Harada Y. The growth of small fatigue cracks in a low carbon steel; the effect of microstructure and limitations of linear elastic fracture mechanics [J]. Fatigue Fract. Eng. Mater. Struct., 1986, 9: 205
doi: 10.1111/ffe.1986.9.issue-3
[19] Shibanuma K, Ueda K, Ito H, et al. Model for predicting fatigue life and limit of steels based on micromechanics of small crack growth [J]. Mater. Des., 2018, 139: 269
doi: 10.1016/j.matdes.2017.10.069
[20] Jiao Z H, Yu H C, Dong C L, et al. Propagation behavior of small and long fatigue cracks in TiAl alloy at elevated temperature [J]. Rare Met. Mater. Eng., 2019, 48: 538
[20] 焦泽辉, 于慧臣, 董成利 等. TiAl合金高温疲劳小裂纹与长裂纹扩展行为 [J]. 稀有金属材料与工程, 2019, 48: 538
[21] Zhu S J, Peng L M, Moriya T, et al. Effect of stress ratio on fatigue crack growth in TiAl intermetallics at room and elevated temperatures [J]. Mater. Sci. Eng., 2000, A290: 198
[22] Wang C H, Miller K J. Short fatigue crack growth under mean stress, uniaxial loading [J]. Fatigue Fract. Eng. Mater. Struct., 1993, 16: 181
doi: 10.1111/ffe.1993.16.issue-2
[23] Suresh S, Ritchie R O. Propagation of short fatigue cracks [J]. Int. Met. Rev., 1984, 29: 445
doi: 10.1179/imr.1984.29.1.445
[24] Zhao G L, Qi H Y, Li S L, et al. Effects of tensile load hold time on the fatigue and corrosion-fatigue behavior of turbine blade materials [J]. Int. J. Fatigue, 2021, 152: 106448
doi: 10.1016/j.ijfatigue.2021.106448
[25] Pippan R, Hageneder P, Knabl W, et al. Fatigue threshold and crack propagation in γ-TiAl sheets [J]. Intermetallics, 2001, 9: 89
doi: 10.1016/S0966-9795(00)00111-4
[26] Zhao G L, Qi H Y, Li S L, et al. Review of fatigue small cracks in key components of gas turbine engines [J]. Adv. Mech., 2023, 53: 819
[26] 赵高乐, 齐红宇, 李少林 等. 燃气涡轮发动机关键部件疲劳小裂纹研究进展 [J]. 力学进展, 2023, 53: 819
[27] Hong Y S, Fang B. Microscopic process and description for the initiation and propagation of short fatigue cracks [J]. Adv. Mech., 1993, 23: 468
[27] 洪友士, 方 飚. 疲劳短裂纹萌生及发展的细观过程和理论 [J]. 力学进展, 1993, 23: 468
[28] Ritchie R O, Lankford J. Small fatigue cracks: A statement of the problem and potential solutions [J]. Mater. Sci. Eng., 1986, 84: 11
doi: 10.1016/0025-5416(86)90217-X
[29] ASTM International. ASTM E1823-24a Standard terminology relating to fatigue and fracture testing [S]. West Conshohocken: ASTM International, 2024
[30] Mutoh Y, Moriya T, Zhu S J, et al. Initiation and growth of small fatigue crack in TiAl intermetallics at elevated and room temperatures [J]. J. Soc. Mater. Sci., Jpn., 1998, 47: 19
[31] Li T R, Xu Y Q, Wu W P, et al. Effects of V and B on the microstructure evolution and deformation mechanisms of Ti-44Al-5Nb-1Mo alloys [J]. Acta Metall. Sin., 2024, 60: 650
[31] 李天瑞, 许瑜倩, 吴文平 等. V和B元素对Ti-44Al-5Nb-1Mo合金显微组织及热变形机制的影响 [J]. 金属学报, 2024, 60: 650
doi: 10.11900/0412.1961.2022.00557
[32] Zuo Z B, Hu R, Luo X, et al. Solidification behavior and microstructures characteristics of Ti-48Al-3Nb-1.5Ta powder produced by supreme-speed plasma rotating electrode process [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 1221
doi: 10.1007/s40195-023-01539-2
[33] Chan K S, Shih D S. Fundamental aspects of fatigue and fracture in a TiAl sheet alloy [J]. Metall. Mater. Trans., 1998, 29A: 73
[34] Wessel W, Zeismann F, Brueckner-Foit A. Short fatigue cracks in intermetallic γ-TiAl-alloys [J]. Fatigue Fract. Eng. Mater. Struct., 2015, 38: 1507
doi: 10.1111/ffe.v38.12
[35] Edwards T E J. Recent progress in the high-cycle fatigue behaviour of γ-TiAl alloys [J]. Mater. Sci. Eng., 2018, 34: 1919
[36] Zhang M, Song X P, Yu L, et al. Fatigue small crack growth threshold determination of a high-Nb TiAl alloy at different temperatures by in-situ observation [J]. Int. J. Miner., Metall., Mater., 2013, 20: 1192
[37] Wang L, Huang X Y, Zhao P T, et al. Investigation of fatigue small crack propagation of TiAl alloy at 750 oC [J]. Failure Anal. Prev., 2018, 13: 159
[37] 王 亮, 黄新跃, 赵澎涛. TiAl合金750 ℃下疲劳小裂纹行为研究 [J]. 失效分析与预防, 2018, 13: 159
[38] Cottrell A H. Theory of brittle fracture in steel and similar metals [J]. Trans. Metall. Soc. AIME, 1958, 212: 192
[39] Huang Z W, Bowen P. Persistent microslip bands in the lamellar TiAl structure subjected to room temperature fatigue [J]. Scr. Mater., 2001, 45: 931
doi: 10.1016/S1359-6462(01)01114-9
[40] Ding R G, Li H Y, Hu D W, et al. Features of fracture surface in a fully lamellar TiAl-base alloy [J]. Intermetallics, 2015, 58: 36
doi: 10.1016/j.intermet.2014.10.020
[41] Yang J, Li H, Hu D, et al. Microstructural characterisation of fatigue crack growth fracture surfaces of lamellar Ti45Al2Mn2Nb1B [J]. Intermetallics, 2014, 45: 89
doi: 10.1016/j.intermet.2013.10.011
[42] Bode B, Wessel W, Brueckner-Foit A, et al. Local deformation at micro‐notches and crack initiation in an intermetallic γ‐TiAl‐alloy [J]. Fatigue Fract. Eng. Mater. Struct., 2016, 39: 227
doi: 10.1111/ffe.v39.2
[43] Tanaka K, Mura T. A dislocation model for fatigue crack initiation [J]. J. Appl. Mech., 1981, 48: 97
doi: 10.1115/1.3157599
[44] Motoyashiki Y, Brückner-Foit A, Sugeta A. Investigation of small crack behaviour under cyclic loading in a dual phase steel with an FIB tomography technique [J]. Fatigue Fract. Eng. Mater. Struct., 2007, 30: 556
doi: 10.1111/ffe.2007.30.issue-6
[45] Santus C, Taylor D. Physically short crack propagation in metals during high cycle fatigue [J]. Int. J. Fatigue, 2009, 31: 1356
doi: 10.1016/j.ijfatigue.2009.03.002
[46] Pippan R, Hohenwarter A. Fatigue crack closure: A review of the physical phenomena [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 471
doi: 10.1111/ffe.v40.4
[47] Li W, Sun C W, Li C, et al. In-situ experimental investigation on fatigue crack growth behavior and crack tip plastic zone evolution of laser powder bed fused TiC/Ti6Al4V composites [J]. Mater. Today Commun., 2025, 49: 113731
[48] Chan K S, Shih D S. Fatigue and fracture behavior of a fine-grained lamellar TiAl alloy [J]. Metall. Mater. Trans., 1997, 28A: 79
[49] Panwar S, Adams J F, Allison J E, et al. A grain boundary interaction model for microstructurally short fatigue cracks [J]. Int. J. Fatigue, 2018, 113: 401
doi: 10.1016/j.ijfatigue.2018.04.029
[50] Wen W, Zhai T G. Quantification of resistance of grain boundaries to short-fatigue crack growth in three dimensions in high-strength Al alloys [J]. Metall. Mater. Trans., 2012, 43A: 2743
[51] Zhai T, Jiang X P, Li J X, et al. The grain boundary geometry for optimum resistance to growth of short fatigue cracks in high strength Al-alloys [J]. Int. J. Fatigue, 2005, 27: 1202
doi: 10.1016/j.ijfatigue.2005.06.021
[52] Zhang X X, Dunne F P E. 3D CP-XFEM modelling of short crack propagation interacting with twist/tilt nickel grain boundaries [J]. J. Mech. Phys. Solids, 2022, 168: 105028
doi: 10.1016/j.jmps.2022.105028
[53] Schmiedel A, Burkhardt C, Rudolph S M, et al. Very high cycle fatigue properties at 973 K of additively manufactured and conventionally processed intermetallic TiAl 48-2-2 alloy [J]. Mater. Sci. Eng., 2023, A862: 144507
[54] Wang S C, Yang B, Liao Z, et al. Research on short fatigue crack initiation and propagation of metallic materials: A review [J]. J. Mech. Eng., 2023, 59(16): 32
[54] 王栓程, 杨 冰, 廖 贞 等. 金属材料疲劳短裂纹萌生与扩展研究综述 [J]. 机械工程学报, 2023, 59(16): 32
doi: 10.3901/JME.2023.16.032
[55] Antunes F V, Branco R, Prates P A, et al. Fatigue crack growth modelling based on CTOD for the 7050-T6 alloy [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 1309
doi: 10.1111/ffe.v40.8
[56] Zheng X L, Hirt M A. Fatigue crack propagation in steels [J]. Eng. Fract. Mech., 1983, 18: 965
doi: 10.1016/0013-7944(83)90070-X
[57] Chan K S, Lankford J. A crack-tip strain model for the growth of small fatigue cracks [J]. Scr. Metall., 1983, 17: 529
doi: 10.1016/0036-9748(83)90346-0
[58] Shyam A, Allison J E, Jones J W. A small fatigue crack growth relationship and its application to cast aluminum [J]. Acta Mater., 2005, 53: 1499
doi: 10.1016/j.actamat.2004.12.004
[59] Wang X Y, Zhao Y, Wang L B, et al. In-situ SEM investigation and modeling of small crack growth behavior of additively manufactured titanium alloy [J]. Int. J. Fatigue, 2021, 149: 106303
doi: 10.1016/j.ijfatigue.2021.106303
[60] Chai L D, Han L, Ren L P, et al. A unified threshold model for physically small and long crack based on CTOD [J]. Theor. Appl. Fract. Mech., 2025, 139: 105002
doi: 10.1016/j.tafmec.2025.105002
[61] Dowling N E, Begley J A. Fatigue crack growth during gross plasticity and the J-integral [R]. Philadelphia, PA: American Society for Testing and Materials, 1976: 82
[62] Polák J, Zezulka P. Short crack growth and fatigue life in austenitic-ferritic duplex stainless steel [J]. Fatigue Fract. Eng. Mater. Struct., 2005, 28: 923
doi: 10.1111/ffe.2005.28.issue-10
[63] Döring R, Hoffmeyer J, Seeger T, et al. Short fatigue crack growth under nonproportional multiaxial elastic-plastic strains [J]. Int. J. Fatigue, 2006, 28: 972
doi: 10.1016/j.ijfatigue.2005.08.012
[64] Chapetti M D. Fatigue propagation threshold of short cracks under constant amplitude loading [J]. Int. J. Fatigue, 2003, 25: 1319
doi: 10.1016/S0142-1123(03)00065-3
[65] Newman Jr J C. A crack-closure model for predicting fatigue-crack growth under aircraft spectrum loading [R]. Hampton, VA: NASA Langley Research Center, 1981
[66] Newman Jr J C, Phillips E P, Swain M H. Fatigue-life prediction methodology using small-crack theory [J]. Int. J. Fatigue, 1999, 21: 109
doi: 10.1016/S0142-1123(98)00058-9
[67] Newman Jr J C, Annigeri B S. Fatigue-life prediction method based on small-crack theory in an engine material [J]. J. Eng. Gas Turbines Power, 2012, 124: 032501
[68] Chan K S, Lankford J, Davidson D L. A comparison of crack-tip field parameters for large and small fatigue cracks [J]. J. Eng. Mater. Technol., 1986, 108: 206
doi: 10.1115/1.3225868
[69] Tada H, Paris P C, Irwin G R. The Stress Analysis of Cracks Handbook [M]. Hellertown: Del Research Corporation, 1973: 602
[70] Ye S, Zhang X C, Gong J G, et al. Multi‐scale fatigue crack propagation in 304 stainless steel: Experiments and modelling [J]. Fatigue Fract. Eng. Mater. Struct., 2017, 40: 1928
doi: 10.1111/ffe.v40.11
[71] Shamir M, Zhang X, Syed A K. Characterising and representing small crack growth in an additive manufactured titanium alloy [J]. Eng. Fract. Mech., 2021, 253: 107876
doi: 10.1016/j.engfracmech.2021.107876
[72] Jones R, Michopoulos J G, Iliopoulos A P, et al. Representing crack growth in additively manufactured Ti-6Al-4V [J]. Int. J. Fatigue, 2018, 116: 610
doi: 10.1016/j.ijfatigue.2018.07.019
[73] Iliopoulos A, Jones R, Michopoulos J, et al. Crack growth in a range of additively manufactured aerospace structural materials [J]. Aerospace, 2018, 5: 118
doi: 10.3390/aerospace5040118
[74] Jones R, Rans C, Iliopoulos A P, et al. Modelling the variability and the anisotropic behaviour of crack growth in SLM Ti-6Al-4V [J]. Materials, 2021, 14: 1400
doi: 10.3390/ma14061400
[75] Hartman A, Schijve J. The effects of environment and load frequency on the crack propagation law for macro fatigue crack growth in aluminium alloys [J]. Eng. Fract. Mech., 1970, 1: 615
doi: 10.1016/0013-7944(70)90003-2
[76] Markham M J, Fatemi A, Phan N. Mixed-mode small fatigue crack growth rates and modeling in additively manufactured metals [J]. Int. J. Fatigue, 2024, 183: 108258
doi: 10.1016/j.ijfatigue.2024.108258
[1] 吴欣强, 谭季波, 张兹瑜, 薛宝权, 柯伟. 金属材料在高温高压水、液态Pb-Bi和海洋环境中的腐蚀疲劳行为研究进展[J]. 金属学报, 2026, 62(5): 822-834.
[2] 陈光, 陈奉锐, 朱德民, 李贵忠, 李罗, 宋伟东, 王子特, 相恒高, 陈旸, 祁志祥. 聚片孪生功能基元序构的高性能TiAl合金[J]. 金属学报, 2026, 62(4): 541-549.
[3] 周志春, 刘仁慈, 张建达, 杨超, 崔玉友, 杨锐. γ-TiAl合金在700 ℃空气中的长时高温氧化行为和组织演变[J]. 金属学报, 2025, 61(8): 1217-1228.
[4] 王强, 李小兵, 郝俊杰, 陈波, 张滨, 张二林, 刘奎. 一种新型Ti-Al-Mn-Nb合金的固态相变行为[J]. 金属学报, 2025, 61(7): 1060-1070.
[5] 李天瑞, 许瑜倩, 吴文平, 甘文萱, 杨永, 刘国怀, 王昭东. V和B元素对Ti-44Al-5Nb-1Mo合金显微组织及热变形机制的影响[J]. 金属学报, 2024, 60(5): 650-660.
[6] 陈玉勇, 时国浩, 杜之明, 张宇, 常帅. 增材制造TiAl合金的研究进展[J]. 金属学报, 2024, 60(1): 1-15.
[7] 王秀琦, 李天瑞, 刘国怀, 郭瑞琪, 王昭东. 交叉包套轧制Ti-44Al-5Nb-1Mo-2V-0.2B合金的微观组织演化及力学性能[J]. 金属学报, 2024, 60(1): 95-106.
[8] 李小兵, 潜坤, 舒磊, 张孟殊, 张金虎, 陈波, 刘奎. W含量对Ti-42Al-5Mn-xW合金相转变行为的影响[J]. 金属学报, 2023, 59(10): 1401-1410.
[9] 陈玉勇, 叶园, 孙剑飞. TiAl合金板材轧制研究现状[J]. 金属学报, 2022, 58(8): 965-978.
[10] 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐. 700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响[J]. 金属学报, 2022, 58(8): 1003-1012.
[11] 杨秦政, 杨晓光, 黄渭清, 石多奇. 粉末高温合金FGH4096的疲劳小裂纹扩展行为[J]. 金属学报, 2022, 58(5): 683-694.
[12] 李玉星, 刘兴豪, 王财林, 胡其会, 王婧涵, 马宏涛, 张楠. 含杂质气态CO2输送管道腐蚀研究进展[J]. 金属学报, 2021, 57(3): 283-294.
[13] 李天瑞, 刘国怀, 于少霞, 王文娟, 张风奕, 彭全义, 王昭东. 直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制[J]. 金属学报, 2020, 56(8): 1091-1102.
[14] 刘先锋, 刘冬, 刘仁慈, 崔玉友, 杨锐. Ti-43.5Al-4Nb-1Mo-0.1B合金的包套热挤压组织与拉伸性能[J]. 金属学报, 2020, 56(7): 979-987.
[15] 王希,刘仁慈,曹如心,贾清,崔玉友,杨锐. 冷却速率对β凝固γ-TiAl合金硼化物和室温拉伸性能的影响[J]. 金属学报, 2020, 56(2): 203-211.