| 低温高应变量衬板控轧高固溶Al-Mg合金高强塑性与高热稳定性机制 |
田滕1, 查敏1,2,3( ), 殷皓亮1, 花珍铭1, 贾海龙1,3, 王慧远1,2,3( ) |
1 吉林大学 材料科学与工程学院 汽车材料教育部重点实验室 长春 130025 2 吉林大学 超硬材料国家重点实验室 长春 130012 3 吉林大学 未来科学国际合作联合实验室 长春 130012 |
|
| Enhanced Mechanical Properties and Thermal Stability Mechanism of a High Solid Solution Al-Mg Alloy Processed by Cryogenic High-Reduction Hard-Plate Rolling |
TIAN Teng1, ZHA Min1,2,3( ), YIN Haoliang1, HUA Zhenming1, JIA Hailong1,3, WANG Huiyuan1,2,3( ) |
1 Key Laboratory of Automobile Materials of Ministry of Education, School of Materials Science and Engineering, Jilin University, Changchun 130025, China 2 State Key Laboratory of Super Hard Materials, Jilin University, Changchun 130012, China 3 International Center of Future Science, Jilin University, Changchun 130012, China |
引用本文:
田滕, 查敏, 殷皓亮, 花珍铭, 贾海龙, 王慧远. 低温高应变量衬板控轧高固溶Al-Mg合金高强塑性与高热稳定性机制[J]. 金属学报, 2024, 60(4): 473-484.
Teng TIAN,
Min ZHA,
Haoliang YIN,
Zhenming HUA,
Hailong JIA,
Huiyuan WANG.
Enhanced Mechanical Properties and Thermal Stability Mechanism of a High Solid Solution Al-Mg Alloy Processed by Cryogenic High-Reduction Hard-Plate Rolling[J]. Acta Metall Sin, 2024, 60(4): 473-484.
| 1 |
Zha M, Zhang H M, Jia H L, et al. Prominent role of multi-scale microstructural heterogeneities on superplastic deformation of a high solid solution Al-7Mg alloy[J]. Int. J. Plast., 2021, 146: 103108
doi: 10.1016/j.ijplas.2021.103108
|
| 2 |
Tang Y P, Goto W, Hirosawa S, et al. Concurrent strengthening of ultrafine-grained age-hardenable Al-Mg alloy by means of high-pressure torsion and spinodal decomposition[J]. Acta Mater., 2017, 131: 57
doi: 10.1016/j.actamat.2017.04.002
|
| 3 |
Yuan T, Zhao X H, Jiang X Q, et al. Mechanism of grain refinement of pulse current assisted plasma arc welded Al-Mg alloy[J]. Acta Metall. Sin., 2024, 60: 323
doi: 10.11900/0412.1961.2022.00036
|
| 3 |
袁 涛, 赵晓虎, 蒋晓青 等. 脉冲电流辅助等离子弧焊Al-Mg合金晶粒细化机理[J]. 金属学报, 2024, 60: 323
|
| 4 |
Zha M, Zhang H M, Meng X T, et al. Stabilizing a severely deformed Al-7Mg alloy with a multimodal grain structure via Mg solute segregation[J]. J. Mater. Sci. Technol., 2021, 89: 141
doi: 10.1016/j.jmst.2021.01.086
|
| 5 |
Jang D H, Park Y B, Kim W J. Significant strengthening in superlight Al-Mg alloy with an exceptionally large amount of Mg (13 wt%) after cold rolling[J]. Mater. Sci. Eng., 2019, A744: 36
|
| 6 |
Morishige T, Hirata T, Uesugi T, et al. Effect of Mg content on the minimum grain size of Al-Mg alloys obtained by friction stir processing[J]. Scr. Mater., 2011, 64: 355
doi: 10.1016/j.scriptamat.2010.10.033
|
| 7 |
Sun J X, Yang K, Wang Q Y, et al. Microstructure and mechanical properties of 5356 aluminum alloy fabricated by TIG arc additive manufacturing[J]. Acta Metall. Sin., 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
|
| 7 |
孙佳孝, 杨 可, 王秋雨 等. 5356铝合金TIG电弧增材制造组织与力学性能[J]. 金属学报, 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
|
| 8 |
Zha M, Li Y J, Mathiesen R H, et al. Microstructure evolution and mechanical behavior of a binary Al-7Mg alloy processed by equal-channel angular pressing[J]. Acta Mater., 2015, 84: 42
doi: 10.1016/j.actamat.2014.10.025
|
| 9 |
Liu Y, Liu M P, Chen X F, et al. Effect of Mg on microstructure and mechanical properties of Al-Mg alloys produced by high pressure torsion[J]. Scr. Mater., 2019, 159: 137
|
| 10 |
Ruppert M, Schunk C, Hausmann D, et al. Global and local strain rate sensitivity of bimodal Al-laminates produced by accumulative roll bonding[J]. Acta Mater., 2016, 103: 643
doi: 10.1016/j.actamat.2015.11.009
|
| 11 |
Luo X, Feng Z Q, Yu T B, et al. Transitions in mechanical behavior and in deformation mechanisms enhance the strength and ductility of Mg-3Gd[J]. Acta Mater., 2020, 183: 398
doi: 10.1016/j.actamat.2019.11.034
|
| 12 |
Konkova T, Mironov S, Korznikov A, et al. Microstructural response of pure copper to cryogenic rolling[J]. Acta Mater., 2010, 58: 5262
doi: 10.1016/j.actamat.2010.05.056
|
| 13 |
Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal[J]. Nature, 2002, 419: 912
doi: 10.1038/nature01133
|
| 14 |
Zha M, Li Y J, Mathiesen R H, et al. High ductility bulk nanostructured Al-Mg binary alloy processed by equal channel angular pressing and inter-pass annealing[J]. Scr. Mater., 2015, 105: 22
doi: 10.1016/j.scriptamat.2015.04.018
|
| 15 |
Krymskiy S, Sitdikov O, Avtokratova E, et al. 2024 aluminum alloy ultrahigh-strength sheet due to two-level nanostructuring under cryorolling and heat treatment[J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 14
doi: 10.1016/S1003-6326(19)65176-9
|
| 16 |
Kumar V, Kumar D. Investigation of tensile behaviour of cryorolled and room temperature rolled 6082 Al alloy[J]. Mater. Sci. Eng., 2017, A691: 211
|
| 17 |
Zhang H M, Zha M, Jia H L, et al. Influences of the Al3Sc particle content on the evolution of bimodal grain structure and mechanical properties of Al-Mg-Sc alloys processed by hard-plate rolling[J]. Mater. Sci. Eng., 2021, A802: 140451
|
| 18 |
Zha M, Meng X T, Zhang H M, et al. High strength and ductile high solid solution Al-Mg alloy processed by a novel hard-plate rolling route[J]. J. Alloys Compd., 2017, 728: 872
doi: 10.1016/j.jallcom.2017.09.017
|
| 19 |
Zha M, Liang J W, Xing H, et al. Spheroiding and refining of coarse CaMgSn phase in Mg-Al-Sn-Ca alloys for simultaneously improved strength and ductility via sub-rapid solidification and controlled rolling[J]. Mater. Sci. Eng., 2022, A834: 142598
|
| 20 |
Li Y K, Zha M, Jia H L, et al. Tailoring bimodal grain structure of Mg-9Al-1Zn alloy for strength-ductility synergy: Co-regulating effect from coarse Al2Y and submicron Mg17Al12 particles[J]. J. Magnes. Alloy., 2021, 9: 1556
doi: 10.1016/j.jma.2021.01.008
|
| 21 |
Li Y K, Zha M, Rong J, et al. Effect of large thickness-reduction on microstructure evolution and tensile properties of Mg-9Al-1Zn alloy processed by hard-plate rolling[J]. J. Mater. Sci. Technol., 2021, 88: 215
doi: 10.1016/j.jmst.2021.01.050
|
| 22 |
Jin Z Z, Zha M, Jia H L, et al. Balancing the strength and ductility of Mg-6Zn-0.2Ca alloy via sub-rapid solidification combined with hard-plate rolling[J]. J. Mater. Sci. Technol., 2021, 81: 219
doi: 10.1016/j.jmst.2020.11.069
|
| 23 |
Zhang H, Zha M, Tian T, et al. Prominent role of high-volume fraction Mg17Al12 dynamic precipitations on multimodal microstructure formation and strength-ductility synergy of Mg-Al-Zn alloys processed by hard-plate rolling (HPR)[J]. Mater. Sci. Eng., 2021, A808: 140920
|
| 24 |
Zhou F, Liao X Z, Zhu Y T, et al. Microstructural evolution during recovery and recrystallization of a nanocrystalline Al-Mg alloy prepared by cryogenic ball milling[J]. Acta Mater., 2003, 51: 2777
doi: 10.1016/S1359-6454(03)00083-1
|
| 25 |
Alyani A, Kazeminezhad M. Annealing behavior of aluminum after low-temperature severe plastic deformation[J]. Mater. Sci. Eng., 2021, A824: 141810
|
| 26 |
Dhal A, Panigrahi S K, Shunmugam M S. Insight into the microstructural evolution during cryo-severe plastic deformation and post-deformation annealing of aluminum and its alloys[J]. J. Alloys Compd., 2017, 726: 1205
doi: 10.1016/j.jallcom.2017.08.062
|
| 27 |
Gao Y H, Liu G, Sun J. Recent progress in high-temperature resistant aluminum-based alloys: Microstructural design and precipitation strategy[J]. Acta Metall. Sin., 2021, 57: 129
doi: 10.11900/0412.1961.2020.00347
|
| 27 |
高一涵, 刘 刚, 孙 军. 耐热铝基合金研究进展: 微观组织设计与析出策略[J]. 金属学报, 2021, 57: 129
doi: 10.11900/0412.1961.2020.00347
|
| 28 |
Hasegawa H, Komura S, Utsunomiya A, et al. Thermal stability of ultrafine-grained aluminum in the presence of Mg and Zr additions[J]. Mater. Sci. Eng., 1999, A265: 188
|
| 29 |
Hayes J S, Keyte R, Prangnell P B. Effect of grain size on tensile behaviour of a submicron grained Al-3wt%-Mg alloy produced by severe deformation[J]. Mater. Sci. Technol., 2000, 16: 1259
doi: 10.1179/026708300101507479
|
| 30 |
Zha M, Meng X T, Yu Z Y, et al. Enhancing thermal stability of binary Al-Mg alloys by tailoring grain orientations using a high solute Mg content[J]. Metall. Mater. Trans., 2019, 50A: 5264
|
| 31 |
Jin S B, Tao N R, Marthinsen K, et al. Deformation of an Al-7Mg alloy with extensive structural micro-segregations during dynamic plastic deformation[J]. Mater. Sci. Eng., 2015, A628: 160
|
| 32 |
Han B S, Wei L J, Xu Y J, et al. Effect of pre-deformation on microstructure and mechanical properties of ultra-high strength Al-Zn-Mg-Cu alloy after ageing treatment[J]. Acta Metall. Sin., 2020, 56: 1007
doi: 10.11900/0412.1961.2019.00402
|
| 32 |
韩宝帅, 魏立军, 徐严谨 等. 预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响[J]. 金属学报, 2020, 56: 1007
doi: 10.11900/0412.1961.2019.00402
|
| 33 |
Kreyca J, Kozeschnik E. State parameter-based constitutive modelling of stress strain curves in Al-Mg solid solutions[J]. Int. J. Plast., 2018, 103: 67
doi: 10.1016/j.ijplas.2018.01.001
|
| 34 |
Fu S H, Cheng T, Zhang Q C, et al. Two mechanisms for the normal and inverse behaviors of the critical strain for the Portevin-Le Chatelier effect[J]. Acta Mater., 2012, 60: 6650
doi: 10.1016/j.actamat.2012.08.035
|
| 35 |
Jobba M, Mishra R K, Niewczas M. Flow stress and work-hardening behaviour of Al-Mg binary alloys[J]. Int. J. Plast., 2015, 65: 43
doi: 10.1016/j.ijplas.2014.08.006
|
| 36 |
Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy[J]. Acta Mater., 2014, 62: 141
doi: 10.1016/j.actamat.2013.09.042
|
| 37 |
Pan H C, Kang R, Li J R, et al. Mechanistic investigation of a low-alloy Mg-Ca-based extrusion alloy with high strength-ductility synergy[J]. Acta Mater., 2020, 186: 278
doi: 10.1016/j.actamat.2020.01.017
|
| 38 |
Hansen N. Hall-Petch relation and boundary strengthening[J]. Scr. Mater., 2004, 51: 801
doi: 10.1016/j.scriptamat.2004.06.002
|
| 39 |
Valiev R Z, Enikeev N A, Murashkin M Y, et al. On the origin of the extremely high strength of ultrafine-grained Al alloys produced by severe plastic deformation[J]. Scr. Mater., 2010, 63: 949
doi: 10.1016/j.scriptamat.2010.07.014
|
| 40 |
Liu G, Zhang P, Yang C, et al. Aluminum alloys: Solute atom clusters and their strengthening[J]. Acta Metall. Sin., 2021, 57: 1484
doi: 10.11900/0412.1961.2021.00301
|
| 40 |
刘 刚, 张 鹏, 杨 冲 等. 铝合金中的溶质原子团簇及其强韧化[J]. 金属学报, 2021, 57: 1484
|
| 41 |
Chen Y J, Roven H J, Gireesh S S, et al. Quantitative study of grain refinement in Al-Mg alloy processed by equal channel angular pressing at cryogenic temperature[J]. Mater. Lett., 2011, 65: 3472
doi: 10.1016/j.matlet.2011.07.067
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|