| 纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化 |
苏震奇1,2, 张丛江1,2, 袁笑坦1,2, 胡兴金1,2, 芦可可1,2, 任维丽1,2( ), 丁彪1,2( ), 郑天祥1,2, 沈喆1,2, 钟云波1,2, 王晖3, 王秋良3 |
1上海大学 材料科学与工程学院 上海 200444 2上海大学 省部共建高品质特殊钢冶金与制备国家重点实验室 上海 200444 3中国科学院电工研究所 北京 100190 |
|
| Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field |
SU Zhenqi1,2, ZHANG Congjiang1,2, YUAN Xiaotan1,2, HU Xingjin1,2, LU Keke1,2, REN Weili1,2( ), DING Biao1,2( ), ZHENG Tianxiang1,2, SHEN Zhe1,2, ZHONG Yunbo1,2, WANG Hui3, WANG Qiuliang3 |
1School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China 2State Key Laboratory of Advanced Special Steel, Shanghai University, Shanghai 200444, China 3Institute of Electrical Engineering, Chinese Academy of Sciences, Beijing 100190, China |
引用本文:
苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良. 纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化[J]. 金属学报, 2023, 59(12): 1568-1580.
Zhenqi SU,
Congjiang ZHANG,
Xiaotan YUAN,
Xingjin HU,
Keke LU,
Weili REN,
Biao DING,
Tianxiang ZHENG,
Zhe SHEN,
Yunbo ZHONG,
Hui WANG,
Qiuliang WANG.
Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. Acta Metall Sin, 2023, 59(12): 1568-1580.
| 1 |
Guo J T. The current situation of application and development of superalloys in the fields of energy industry[J]. Acta Metall. Sin., 2010, 46: 513
doi: 10.3724/SP.J.1037.2009.00860
|
| 1 |
郭建亭. 高温合金在能源工业领域中的应用现状与发展[J]. 金属学报, 2010, 46: 513
doi: 10.3724/SP.J.1037.2009.00860
|
| 2 |
Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades[J]. Acta Metall. Sin., 2015, 51: 1179
|
| 2 |
马德新. 高温合金叶片单晶凝固技术的新发展[J]. 金属学报, 2015, 51: 1179
|
| 3 |
Sun X F, Jin T, Zhou Y Z, et al. Research progress of nickel-base single crystal superalloys[J]. Mater. China, 2012, 31(12): 1
|
| 3 |
孙晓峰, 金 涛, 周亦胄 等. 镍基单晶高温合金研究进展[J]. 中国材料进展, 2012, 31(12): 1
|
| 4 |
Zhang J, Huang T W, Liu L, et al. Advances in solidification characteristics and typical casting defects in nickel-based single crystal superalloys[J]. Acta Metall. Sin., 2015, 51: 1163
doi: 10.11900/0412.1961.2015.00448
|
| 4 |
张 军, 黄太文, 刘 林 等. 单晶高温合金凝固特性与典型凝固缺陷研究[J]. 金属学报, 2015, 51: 1163
|
| 5 |
Ren N, Panwisawas C, Li J, et al. Solute enrichment induced dendritic fragmentation in directional solidification of nickel-based superalloys[J]. Acta Mater., 2021, 215: 117043
doi: 10.1016/j.actamat.2021.117043
|
| 6 |
Zhang J, Wang L, Wang D, et al. Recent progress in research and development of nickel-based single crystal superalloys[J]. Acta Metall. Sin., 2019, 55: 1077
|
| 6 |
张 健, 王 莉, 王 栋 等. 镍基单晶高温合金的研发进展[J]. 金属学报, 2019, 55: 1077
|
| 7 |
D'Souza N, Newell M, Devendra K, et al. Formation of low angle boundaries in Ni-based superalloys[J]. Mater. Sci. Eng., 2005, A413-414: 567
|
| 8 |
Zhou Y Z. Formation of stray grains during directional solidification of a nickel-based superalloy[J]. Scr. Mater., 2011, 65: 281
doi: 10.1016/j.scriptamat.2011.04.023
|
| 9 |
Yang X L, Dong H B, Wang W, et al. Microscale simulation of stray grain formation in investment cast turbine blades[J]. Mater. Sci. Eng., 2004, A386: 129
|
| 10 |
Meng X B, Lu Q, Li J G, et al. Modes of grain selection in spiral selector during directional solidification of nickel-base superalloys[J]. J. Mater. Sci. Technol., 2012, 28: 214
doi: 10.1016/S1005-0302(12)60044-9
|
| 11 |
Li Y F, Liu L, Huang T W, et al. The process analysis of seeding-grain selection and its effect on stray grain and orientation control[J]. J. Alloys Compd., 2016, 657: 341
doi: 10.1016/j.jallcom.2015.09.249
|
| 12 |
Hu S S, Yang W C, Li Z R, et al. Formation mechanisms and control method for stray grains at melt-back region of Ni-based single crystal seed[J]. Prog. Nat. Sci., 2021, 31: 624
doi: 10.1016/j.pnsc.2021.07.004
|
| 13 |
Hallensleben P, Schaar H, Thome P, et al. On the evolution of cast microstructures during processing of single crystal Ni-base superalloys using a Bridgman seed technique[J]. Mater. Des., 2017, 128: 98
doi: 10.1016/j.matdes.2017.05.001
|
| 14 |
Zhang T, Ren W L, Dong J W, et al. Effect of high magnetic field on the primary dendrite arm spacing and segregation of directionally solidified superalloy DZ417G[J]. J. Alloys Compd., 2009, 487: 612
doi: 10.1016/j.jallcom.2009.08.025
|
| 15 |
Dong J W, Ren Z M, Ren W L, et al. Effect of horizontal magnetic field on the microstructure of directionally solidified Ni-based superalloy[J]. Acta Metall. Sin., 2010, 46: 71
|
| 15 |
董建文, 任忠鸣, 任维丽 等. 横向磁场对镍基高温合金定向凝固组织的影响[J]. 金属学报, 2010, 46: 71
|
| 16 |
Ren W L, Lu L, Yuan G Z, et al. The effect of magnetic field on precipitation phases of single-crystal nickel-base superalloy during directional solidification[J]. Mater. Lett., 2013, 100: 223
doi: 10.1016/j.matlet.2013.03.023
|
| 17 |
Xuan W D, Song G, Duan F M, et al. Enhanced creep properties of nickel-base single crystal superalloy CMSX-4 by high magnetic field[J]. Mater. Sci. Eng., 2021, A803: 140729
|
| 18 |
Li Q D, Shen J, Qin L, et al. Effect of traveling magnetic field on freckle formation in directionally solidified CMSX-4 superalloy[J]. Mater. Process. Technol., 2019, 274: 116308
doi: 10.1016/j.jmatprotec.2019.116308
|
| 19 |
Xuan W D, Ren Z M, Li C J. Effect of a high magnetic field on microstructures of Ni-based superalloy during directional solidification[J]. J. Alloys Compd., 2015, 620: 10
doi: 10.1016/j.jallcom.2014.09.114
|
| 20 |
Zhang K L, Li Y J, Yang Y S. Influence of the low voltage pulsed magnetic field on the columnar-to-equiaxed transition during directional solidification of superalloy K4169[J]. J. Mater. Sci. Technol., 2020, 48: 9
doi: 10.1016/j.jmst.2020.02.009
|
| 21 |
Ren W L, Niu C L, Ding B, et al. Improvement in creep life of a nickel-based single-crystal superalloy via composition homogeneity on the multiscales by magnetic-field-assisted directional solidification[J]. Sci. Rep., 2018, 8: 1452
doi: 10.1038/s41598-018-19800-5
pmid: 29362394
|
| 22 |
Xuan W D, Liu H, Lan J, et al. Effect of a transverse magnetic field on stray grain formation of Ni-based single crystal superalloy during directional solidification[J]. Metall. Mater. Trans., 2016, 47B: 3231
|
| 23 |
Xuan W D, Liu H, Li C J, et al. Effect of a high magnetic field on microstructures of Ni-based single crystal superalloy during seed melt-back[J]. Metall. Mater. Trans., 2016, 47B: 828
|
| 24 |
Xuan W D, Lan J, Liu H, et al. Effects of a high magnetic field on the microstructure of Ni-based single-crystal superalloys during directional solidification[J]. Metall. Mater. Trans., 2017, 48A: 3804
|
| 25 |
Yuan X T, Zhou T, Ren W L, et al. Nondestructive effect of the cusp magnetic field on the dendritic microstructure during the directional solidification of nickel-based single crystal superalloy[J]. J. Mater. Sci. Technol., 2021, 62: 52
doi: 10.1016/j.jmst.2020.05.059
|
| 26 |
Liu C L, Su H J, Zhang J, et al. Effect of electromagnetic field on microstructure of Ni-based single crystal superalloys[J]. Acta Metall. Sin., 2018, 54: 1428
|
| 26 |
刘承林, 苏海军, 张 军 等. 电磁场对镍基单晶高温合金组织的影响[J]. 金属学报, 2018, 54: 1428
doi: 10.11900/0412.1961.2017.00539
|
| 27 |
Li Y J, Teng Y F, Feng X H, et al. Effects of pulsed magnetic field on microsegregation of solute elements in a Ni-based single crystal superalloy[J]. J. Mater. Sci. Technol., 2017, 33: 105
doi: 10.1016/j.jmst.2015.12.021
|
| 28 |
Niu C L, Ren W L, Ding B, et al. The change of mushy-zone length of a nickel-based single-crystal superalloy during the static-magnetic-field-assisted directional solidification[J]. Cryst. Res. Technol., 2018, 53: 1700187
doi: 10.1002/crat.v53.6
|
| 29 |
Liu Q. EBSD technique and its applications in materials science[J]. Chin. J. Stereol. Image Anal., 2005, 10: 205
|
| 29 |
刘 庆. 电子背散射衍射技术及其在材料科学中的应用[J]. 中国体视学与图像分析, 2005, 10: 205
|
| 30 |
Xu W L, Wang F, Ma D X, et al. Sliver defect formation in single crystal Ni-based superalloy castings[J]. Mater. Des., 2020, 196: 109138
doi: 10.1016/j.matdes.2020.109138
|
| 31 |
Ren Z M, Lei Z S, Li C J, et al. New study and development on electromagnetic field technology in metallurgical processes[J]. Acta Metall. Sin., 2020, 56: 583
doi: 10.11900/0412.1961.2019.00373
|
| 31 |
任忠鸣, 雷作胜, 李传军 等. 电磁冶金技术研究新进展[J]. 金属学报, 2020, 56: 583
doi: 10.11900/0412.1961.2019.00373
|
| 32 |
Wang J, Fautrelle Y, Ren Z M, et al. Thermoelectric magnetic force acting on the solid during directional solidification under a static magnetic field[J]. Appl. Phys. Lett., 2012, 101: 251904
doi: 10.1063/1.4772510
|
| 33 |
Dahle A K, Arnberg L. Development of strength in solidifying aluminium alloys[J]. Acta Mater., 1997, 45: 547
doi: 10.1016/S1359-6454(96)00203-0
|
| 34 |
Khine Y Y, Walker J S. Thermoelectric magnetohydrodynamic effects during Bridgman semiconductor crystal growth with a uniform axial magnetic field[J]. J. Cryst. Growth, 1998, 183: 150
doi: 10.1016/S0022-0248(97)00394-1
|
| 35 |
Ma D X. Freckle formation during directional solidification of complex castings of superalloys[J]. Acta Metall. Sin., 2016, 52: 426
|
| 35 |
马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成[J]. 金属学报, 2016, 52: 426
doi: 10.11900/0412.1961.2015.00379
|
| 36 |
Walton D, Chalmers B. The origin of the preferred orientation in the columnar zone of ingots[J]. Trans. Am. Inst. Min. Metall. Eng., 1959, 215: 447
|
| 37 |
Zhou Y Z, Volek A, Green N R. Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy[J]. Acta Mater., 2008, 56: 2631
doi: 10.1016/j.actamat.2008.02.022
|
| 38 |
Hu S S, Liu L, Cui Q W, et al. Converging competitive growth in bi-crystal of Ni-based superalloy during directional solidification[J]. Acta. Metall. Sin., 2016, 52: 897
|
| 38 |
胡松松, 刘 林, 崔强伟 等. 镍基高温合金定向凝固过程中的汇聚型双晶竞争生长[J]. 金属学报, 2016, 52: 897
doi: 10.11900/0412.1961.2015.00631
|
| 39 |
Guo C W, Takaki T, Sakane S, et al. Overgrowth behavior at converging grain boundaries during competitive grain growth: A two-dimensional phase-field study[J]. Int. J. Heat Mass Transfer, 2020, 160: 120196
doi: 10.1016/j.ijheatmasstransfer.2020.120196
|
| 40 |
Zhou Y Z, Jin T, Sun X F. Structure evolution in directionally solidified bicrystals of nickel base superalloys[J]. Acta Metall. Sin., 2010, 46: 1327
doi: 10.3724/SP.J.1037.2010.01327
|
| 40 |
周亦胄, 金 涛, 孙晓峰. 双晶镍基高温合金定向凝固过程的结构演化[J]. 金属学报, 2010, 46: 1327
doi: 10.3724/SP.J.1037.2010.00280
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|