|
|
|
| Ti及钛合金表面改性在生物医用领域的研究进展 |
崔振铎, 朱家民, 姜辉, 吴水林, 朱胜利( ) |
| 天津大学 材料科学与工程学院 天津 300350 |
|
| Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application |
CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli( ) |
| School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China |
引用本文:
崔振铎, 朱家民, 姜辉, 吴水林, 朱胜利. Ti及钛合金表面改性在生物医用领域的研究进展[J]. 金属学报, 2022, 58(7): 837-856.
Zhenduo CUI,
Jiamin ZHU,
Hui JIANG,
Shuilin WU,
Shengli ZHU.
Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application[J]. Acta Metall Sin, 2022, 58(7): 837-856.
| 1 |
Geetha M, Singh A K, Asokamani R, et al. Ti based biomaterials, the ultimate choice for orthopaedic implants—A review [J]. Prog. Mater. Sci., 2009, 54: 397
doi: 10.1016/j.pmatsci.2008.06.004
|
| 2 |
Long M, Rack H J. Titanium alloys in total joint replacement—A materials science perspective [J]. Biomaterials, 1998, 19: 1621
pmid: 9839998
|
| 3 |
Elias C N, Lima J H C, Valiev R, et al. Biomedical applications of titanium and its alloys [J]. JOM, 2008, 60(3): 46
|
| 4 |
Fonseca-García A, Pérez-Alvarez J, Barrera C C, et al. The effect of simulated inflammatory conditions on the surface properties of titanium and stainless steel and their importance as biomaterials [J]. Mater. Sci. Eng., 2016, C66: 119
|
| 5 |
Barceloux D G. Chromium [J]. J. Toxicol.: Clin. Toxicol., 1999, 37: 173
doi: 10.1081/CLT-100102418
|
| 6 |
Nickens K P, Patierno S R, Ceryak S. Chromium genotoxicity: A double-edged sword [J]. Chem. Biol. Interact., 2010, 188: 276
doi: 10.1016/j.cbi.2010.04.018
|
| 7 |
Paustenbach D J, Tvermoes B E, Unice K M, et al. A review of the health hazards posed by cobalt [J]. Crit. Rev. Toxicol., 2013, 43: 316
doi: 10.3109/10408444.2013.779633
pmid: 23656559
|
| 8 |
Pavesi T, Moreira J C. Mechanisms and individuality in chromium toxicity in humans [J]. J. Appl. Toxicol., 2020, 40: 1183
doi: 10.1002/jat.3965
|
| 9 |
Kaur M, Singh K. Review on titanium and titanium based alloys as biomaterials for orthopaedic applications [J]. Mater. Sci. Eng., 2019, C102: 844
|
| 10 |
Chen L Y, Cui Y W, Zhang L C. Recent development in beta titanium alloys for biomedical applications [J]. Metals, 2020, 10: 1139
doi: 10.3390/met10091139
|
| 11 |
Niinomi M, Liu Y, Nakai M, et al. Biomedical titanium alloys with Young's moduli close to that of cortical bone [J]. Regen. Biomater., 2016, 3: 173
doi: 10.1093/rb/rbw016
pmid: 27252887
|
| 12 |
Wang L Q, Lu W J, Qin J N, et al. Effect of precipitation phase on microstructure and superelasticity of cold-rolled beta titanium alloy during heat treatment [J]. Mater. Des., 2009, 30: 3873
doi: 10.1016/j.matdes.2009.03.042
|
| 13 |
Wang L Q, Xie L C, Lv Y T, et al. Microstructure evolution and superelastic behavior in Ti-35Nb-2Ta-3Zr alloy processed by friction stir processing [J]. Acta Mater., 2017, 131: 499
doi: 10.1016/j.actamat.2017.03.079
|
| 14 |
Gode C, Attarilar S, Eghbali B, et al. Electrochemical behavior of equal channel angular pressed titanium for biomedical application [C]. AIP Conf. Proc., 2015, 1653: 020041
|
| 15 |
Apaza-Bedoya K, Tarce M, Benfatti C A M, et al. Synergistic interactions between corrosion and wear at titanium-based dental implant connections: A scoping review [J]. J. Periodontal Res., 2017, 52: 946
doi: 10.1111/jre.12469
pmid: 28612506
|
| 16 |
Goldberg J R, Gilbert J L, Jacobs J J, et al. A multicenter retrieval study of the taper interfaces of modular hip prostheses [J]. Clin. Orthop. Relat. Res., 2002, 401: 149
doi: 10.1097/00003086-200208000-00018
|
| 17 |
Takai S, Yoshino N, Kusaka Y, et al. Dissemination of metals from a failed patellar component made of titanium-base alloy [J]. J. Arthroplasty, 2003, 18: 931
doi: 10.1016/S0883-5403(03)00277-8
|
| 18 |
Moretti B, Pesce V, Maccagnano G, et al. Peripheral neuropathy after hip replacement failure: Is vanadium the culprit? [J]. Lancet, 2012, 379: 1676
doi: 10.1016/S0140-6736(12)60273-6
pmid: 22541583
|
| 19 |
Gilbert J L, Mali S, Urban R M, et al. In vivo oxide-induced stress corrosion cracking of Ti-6Al-4V in a neck-stem modular taper: Emergent behavior in a new mechanism of in vivo corrosion [J]. J. Biomed. Mater. Res., 2012, 100B: 584
doi: 10.1002/jbm.b.31943
|
| 20 |
Tsaryk R, Peters K, Barth S, et al. The role of oxidative stress in pro-inflammatory activation of human endothelial cells on Ti6Al4V alloy [J]. Biomaterials, 2013, 34: 8075
doi: 10.1016/j.biomaterials.2013.07.030
pmid: 23891083
|
| 21 |
Mouthuy P A, Snelling S J B, Dakin S G, et al. Biocompatibility of implantable materials: An oxidative stress viewpoint [J]. Biomaterials, 2016, 109: 55
doi: 10.1016/j.biomaterials.2016.09.010
|
| 22 |
Kasai Y, Iida R, Uchida A. Metal concentrations in the serum and hair of patients with titanium alloy spinal implants [J]. Spine, 2003, 28: 1320
|
| 23 |
Verstraeten S V, Aimo L, Oteiza P I. Aluminium and lead: Molecular mechanisms of brain toxicity [J]. Arch. Toxicol., 2008, 82: 789
doi: 10.1007/s00204-008-0345-3
pmid: 18668223
|
| 24 |
Jafari M S, Coyle C, Mortazavi J S M, et al. Revision hip arthroplasty: Infection is the most common cause of failure [J]. Clin. Orthop. Relat. Res., 2010, 468: 2046
doi: 10.1007/s11999-010-1251-6
|
| 25 |
Le D H, Goodman S B, Maloney W J, et al. Current modes of failure in TKA: Infection, instability, and stiffness predominate [J]. Clin. Orthop. Relat. Res., 2014, 472: 2197
doi: 10.1007/s11999-014-3540-y
|
| 26 |
Chouirfa H, Bouloussa H, Migonney V, et al. Review of titanium surface modification techniques and coatings for antibacterial applications [J]. Acta Biomater., 2019, 83: 37
doi: S1742-7061(18)30635-4
pmid: 30541702
|
| 27 |
Maher S, Mazinani A, Barati M R, et al. Engineered titanium implants for localized drug delivery: Recent advances and perspectives of titania nanotubes arrays [J]. Expert Opin. Drug Deliv., 2018, 15: 1021
doi: 10.1080/17425247.2018.1517743
|
| 28 |
Correa D R N, Kuroda P A B, Lourenço M L, et al. Development of Ti-15Zr-Mo alloys for applying as implantable biomedical devices [J]. J. Alloys Compd., 2018, 749: 163
doi: 10.1016/j.jallcom.2018.03.308
|
| 29 |
Bai Y J, Deng Y, Zheng Y F, et al. Characterization, corrosion behavior, cellular response and in vivo bone tissue compatibility of titanium-niobium alloy with low Young's modulus [J]. Mater. Sci. Eng., 2016, C59: 565
|
| 30 |
Ou K L, Weng C C, Lin Y H, et al. A promising of alloying modified beta-type titanium-niobium implant for biomedical applications: Microstructural characteristics, in vitro biocompatibility and antibacterial performance [J]. J. Alloys Compd., 2017, 697: 231
doi: 10.1016/j.jallcom.2016.12.120
|
| 31 |
Zhou Y, Li Y X, Yang X J, et al. Influence of Zr content on phase transformation, microstructure and mechanical properties of Ti75 - x Nb25Zr x (x = 0-6) alloys [J]. J. Alloys Compd., 2009, 486: 628
doi: 10.1016/j.jallcom.2009.07.006
|
| 32 |
Qiu K J, Liu Y, Zhou F Y, et al. Microstructure, mechanical properties, castability and in vitro biocompatibility of Ti-Bi alloys developed for dental applications [J]. Acta Biomater., 2015, 15: 254
doi: 10.1016/j.actbio.2015.01.009
pmid: 25595472
|
| 33 |
Ahn H, Lee D, Lee K M, et al. Oxidation behavior and corrosion resistance of Ti-10Ta-10Nb alloy [J]. Surf. Coat. Technol., 2008, 202: 5784
doi: 10.1016/j.surfcoat.2008.06.074
|
| 34 |
Nune K C, Misra R D K, Li S J, et al. Osteoblast cellular activity on low elastic modulus Ti-24Nb-4Zr-8Sn alloy [J]. Dent. Mater., 2017, 33: 152
doi: S0109-5641(16)30629-7
pmid: 27889088
|
| 35 |
Zheng Y F, Zhang B B, Wang B L, et al. Introduction of antibacterial function into biomedical TiNi shape memory alloy by the addition of element Ag [J]. Acta Biomater., 2011, 7: 2758
doi: 10.1016/j.actbio.2011.02.010
pmid: 21316493
|
| 36 |
Li H B, Cui Z D, Li Z Y, et al. Effect of gas nitriding treatment on cavitation erosion behavior of commercially pure Ti and Ti-6Al-4V alloy [J]. Surf. Coat. Technol., 2013, 221: 29
doi: 10.1016/j.surfcoat.2013.01.023
|
| 37 |
Li H B, Cui Z D, Li Z Y, et al. Microstructure and cavitation erosion properties of ceramic coatings fabricated on Ti-6Al-4V alloy by pack carburizing [J]. J. Mater. Eng. Perform., 2014, 23: 2772
doi: 10.1007/s11665-014-1030-8
|
| 38 |
Zhu Y H, Wang W, Jia X Y, et al. Deposition of TiC film on titanium for abrasion resistant implant material by ion-enhanced triode plasma CVD [J]. Appl. Surf. Sci., 2012, 262: 156
doi: 10.1016/j.apsusc.2012.03.152
|
| 39 |
Li Q, Niinomi M, Nakai M, et al. Improvements in the superelasticity and change in deformation mode of β-type TiNb24Zr2 alloys caused by aging treatments [J]. Metall. Mater. Trans., 2011, 42A: 2843
|
| 40 |
Liu Y, Li K Y, Luo T, et al. Powder metallurgical low-modulus Ti-Mg alloys for biomedical applications [J]. Mater. Sci. Eng., 2015, C56: 241
|
| 41 |
Karre R, Kodli B K, Rajendran A, et al. Comparative study on Ti-Nb binary alloys fabricated through spark plasma sintering and conventional P/M routes for biomedical application [J]. Mater. Sci. Eng., 2019, C94: 619
|
| 42 |
Attar H, Calin M, Zhang L C, et al. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium [J]. Mater. Sci. Eng., 2014, A593: 170
|
| 43 |
Li X P, Van Humbeeck J, Kruth J P. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: A study from laser power perspective [J]. Mater. Des., 2017, 116: 352
doi: 10.1016/j.matdes.2016.12.019
|
| 44 |
García I, De Damborenea J J. Corrosion properties of tin prepared by laser gas alloying of Ti and Ti6Al4V [J]. Corros. Sci., 1998, 40: 1411
doi: 10.1016/S0010-938X(98)00046-8
|
| 45 |
Jiang P, He X L, Li X X, et al. Wear resistance of a laser surface alloyed Ti-6Al-4V alloy [J]. Surf. Coat. Technol., 2000, 130: 24
doi: 10.1016/S0257-8972(00)00680-0
|
| 46 |
Yue T M, Yu J K, Mei Z, et al. Excimer laser surface treatment of Ti-6Al-4V alloy for corrosion resistance enhancement [J]. Mater. Lett., 2002, 52: 206
doi: 10.1016/S0167-577X(01)00395-0
|
| 47 |
Hays S J. Therapeutic approaches to the treatment of neuroinflammatory diseases [J]. Curr. Pharm. Des., 1998, 4: 335
|
| 48 |
Wang D, He G, Tian Y, et al. Dual effects of acid etching on cell responses and mechanical properties of porous titanium with controllable open-porous structure [J]. J. Biomed. Mater. Res., 2020, 108B: 2386
|
| 49 |
Szmukler-Moncler S, Perrin D, Ahossi V, et al. Biological properties of acid etched titanium implants: Effect of sandblasting on bone anchorage [J]. J. Biomed. Mater. Res., 2004, 68B: 149
doi: 10.1002/jbm.b.20003
|
| 50 |
Baleani M, Viceconti M, Toni A. The effect of sandblasting treatment on endurance properties of titanium alloy hip prostheses [J]. Artif. Organs, 2000, 24: 296
pmid: 10816203
|
| 51 |
Szmukler-Moncler S, Testori T, Bernard J P. Etched implants: A comparative surface analysis of four implant systems [J]. J. Biomed. Mater. Res., 2004, 69B: 46
doi: 10.1002/jbm.b.20021
|
| 52 |
Wennerberg A, Albrektsson T. Effects of titanium surface topography on bone integration: A systematic review [J]. Clin. Oral Implants Res., 2009, 20: 172
doi: 10.1111/j.1600-0501.2009.01775.x
|
| 53 |
Klokkevold P R, Johnson P, Dadgostari S, et al. Early endosseous integration enhanced by dual acid etching of titanium: A torque removal study in the rabbit [J]. Clin. Oral Implants Res., 2001, 12: 350
doi: 10.1034/j.1600-0501.2001.012004350.x
|
| 54 |
Ferraris S, Venturello A, Miola M, et al. Antibacterial and bioactive nanostructured titanium surfaces for bone integration [J]. Appl. Surf. Sci., 2014, 311: 279
doi: 10.1016/j.apsusc.2014.05.056
|
| 55 |
Li J, Zhou P, Attarilar S, et al. Innovative surface modification procedures to achieve micro/nano-graded Ti-based biomedical alloys and implants [J]. Coatings, 2021, 11: 647
doi: 10.3390/coatings11060647
|
| 56 |
Chiang H J, Hsu H J, Peng P W, et al. Early bone response to machined, sandblasting acid etching (SLA) and novel surface-functionalization (SLAffinity) titanium implants: Characterization, biomechanical analysis and histological evaluation in pigs [J]. J. Biomed. Mater. Res., 2016, 104A: 397
|
| 57 |
Gupta N, Santhiya D, Murugavel S, et al. Effects of transition metal ion dopants (Ag, Cu and Fe) on the structural, mechanical and antibacterial properties of bioactive glass [J]. Colloids Surf., 2018, 538A: 393
|
| 58 |
Attarilar S, Ebrahimi M, Djavanroodi F, et al. 3D printing technologies in metallic implants: A thematic review on the techniques and procedures [J]. Int. J. Bioprint., 2021, 7: 306
|
| 59 |
Kurella A, Dahotre N B. Review paper: Surface modification for bioimplants: The role of laser surface engineering [J]. J. Biomater. Appl., 2005, 20: 5
pmid: 15972362
|
| 60 |
Tiainen L, Abreu P, Buciumeanu M, et al. Novel laser surface texturing for improved primary stability of titanium implants [J]. J. Mech. Behav. Biomed. Mater., 2019, 98: 26
doi: S1751-6161(18)31498-X
pmid: 31176991
|
| 61 |
Cunha A, Elie A M, Plawinski L, et al. Femtosecond laser surface texturing of titanium as a method to reduce the adhesion of Staphylococcus aureus and biofilm formation [J]. Appl. Surf. Sci., 2016, 360: 485
doi: 10.1016/j.apsusc.2015.10.102
|
| 62 |
Lee B H, Kim J K, Kim Y D, et al. In vivo behavior and mechanical stability of surface-modified titanium implants by plasma spray coating and chemical treatments [J]. J. Biomed. Mater. Res., 2004, 69A: 279
doi: 10.1002/jbm.a.20126
|
| 63 |
Sargin F, Erdogan G, Kanbur K, et al. Investigation of in vitro behavior of plasma sprayed Ti, TiO2 and HA coatings on peek [J]. Surf. Coat. Technol., 2021, 411: 126965
doi: 10.1016/j.surfcoat.2021.126965
|
| 64 |
Khor K A, Gu Y W, Quek C H, et al. Plasma spraying of functionally graded hydroxyapatite/Ti-6Al-4V coatings [J]. Surf. Coat. Technol., 2003, 168: 195
doi: 10.1016/S0257-8972(03)00238-X
|
| 65 |
Hameed P, Gopal V, Bjorklund S, et al. Axial suspension plasma spraying: An ultimate technique to tailor Ti6Al4V surface with hap for orthopaedic applications [J]. Colloids Surf., 2019, 173B: 806
|
| 66 |
Singh H, Prakash C, Singh S. Plasma spray deposition of HA-TiO2 on β-phase Ti-35Nb-7Ta-5Zr alloy for hip stem: Characterization of bio-mechanical properties, wettability, and wear resistance [J]. J. Bionic Eng., 2020, 17: 1029
doi: 10.1007/s42235-020-0081-9
|
| 67 |
Duta L. In vivo assessment of synthetic and biological-derived calcium phosphate-based coatings fabricated by pulsed laser deposition: A review [J]. Coatings, 2021, 11: 99
doi: 10.3390/coatings11010099
|
| 68 |
Galindo-Valdés J S, Cortés-Hernández D A, Ortiz-Cuellar J C, et al. Laser deposition of bioactive coatings by in situ synthesis of pseudowollastonite on Ti6Al4V alloy [J]. Opt. Laser Technol., 2021, 134: 106586
doi: 10.1016/j.optlastec.2020.106586
|
| 69 |
Cao J X, Lian R Z, Jiang X H. Magnesium and fluoride doped hydroxyapatite coatings grown by pulsed laser deposition for promoting titanium implant cytocompatibility [J]. Appl. Surf. Sci., 2020, 515: 146069
doi: 10.1016/j.apsusc.2020.146069
|
| 70 |
Zaveri N, Mahapatra M, Deceuster A, et al. Corrosion resistance of pulsed laser-treated Ti-6Al-4V implant in simulated biofluids [J]. Electrochim. Acta, 2008, 53: 5022
doi: 10.1016/j.electacta.2008.01.086
|
| 71 |
Chen L Y, Komasa S, Hashimoto Y, et al. In vitro and in vivo osteogenic activity of titanium implants coated by pulsed laser deposition with a thin film of fluoridated hydroxyapatite [J]. Int. J. Mol. Sci., 2018, 19: 1127
doi: 10.3390/ijms19041127
|
| 72 |
Pelletier H, Nelea V, Mille P, et al. Mechanical properties of pulsed laser-deposited hydroxyapatite thin film implanted at high energy with N+ and Ar+ ions. Part I: nanoindentation with spherical tipped indenter [J]. Nucl. Instrum. Methods Phys. Res., 2004, 216B: 269
|
| 73 |
D'Alessio L, Ferro D, Marotta V, et al. Laser ablation and deposition of bioglass® 45S5 thin films [J]. Appl. Surf. Sci., 2001, 183: 10
doi: 10.1016/S0169-4332(01)00466-4
|
| 74 |
Gnanavel S, Ponnusamy S, Mohan L, et al. Electrochemical behavior of biomedical titanium alloys coated with diamond carbon in Hanks' solution [J]. J. Mater. Eng. Perform., 2018, 27: 1635
doi: 10.1007/s11665-018-3250-9
|
| 75 |
Kaliaraj G S, Bavanilathamuthiah M, Kirubaharan K, et al. Bio-inspired YSZ coated titanium by EB-PVD for biomedical applications [J]. Surf. Coat. Technol., 2016, 307: 227
doi: 10.1016/j.surfcoat.2016.08.039
|
| 76 |
Paital S R, Dahotre N B. Calcium phosphate coatings for bio-implant applications: Materials, performance factors, and methodologies [J]. Mater. Sci. Eng., 2009, R66: 1
|
| 77 |
Oyane A, Wang X P, Sogo Y, et al. Calcium phosphate composite layers for surface-mediated gene transfer [J]. Acta Biomater., 2012, 8: 2034
doi: 10.1016/j.actbio.2012.02.003
|
| 78 |
Surmenev R A, Surmeneva M A, Ivanova A A. Significance of calcium phosphate coatings for the enhancement of new bone osteogenesis—A review [J]. Acta Biomater., 2014, 10: 557
doi: 10.1016/j.actbio.2013.10.036
pmid: 24211734
|
| 79 |
Liu B, Shi X M, Xiao G Y, et al. In-situ preparation of scholzite conversion coatings on titanium and Ti-6Al-4V for biomedical applications [J]. Colloids Surf., 2017, 153B: 291
|
| 80 |
Yu W Z, Zhang Y Z, Liu X M, et al. Synergistic antibacterial activity of multi components in lysozyme/chitosan/silver/hydroxyapatite hybrid coating [J]. Mater. Des., 2018, 139: 351
doi: 10.1016/j.matdes.2017.11.018
|
| 81 |
Liu X H, Wu L, Ai H J, et al. Cytocompatibility and early osseointegration of nano TiO2-modified Ti-24Nb-4Zr-7.9Sn surfaces [J]. Mater. Sci. Eng., 2015, C48: 256
|
| 82 |
Zhang X M, Li Z Y, Yuan X B, et al. Fabrication of dopamine-modified hyaluronic acid/chitosan multilayers on titanium alloy by layer-by-layer self-assembly for promoting osteoblast growth [J]. Appl. Surf. Sci., 2013, 284: 732
doi: 10.1016/j.apsusc.2013.08.002
|
| 83 |
İzmir M, Ercan B. Anodization of titanium alloys for orthopedic applications [J]. Front. Chem. Sci. Eng., 2019, 13: 28
doi: 10.1007/s11705-018-1759-y
|
| 84 |
Minagar S, Berndt C C, Wang J, et al. A review of the application of anodization for the fabrication of nanotubes on metal implant surfaces [J]. Acta Biomater., 2012, 8: 2875
doi: 10.1016/j.actbio.2012.04.005
|
| 85 |
Schwartz Z, Olivares-Navarrete R, Wieland M, et al. Mechanisms regulating increased production of osteoprotegerin by osteoblasts cultured on microstructured titanium surfaces [J]. Biomaterials, 2009, 30: 3390
doi: 10.1016/j.biomaterials.2009.03.047
pmid: 19395022
|
| 86 |
Kim M J, Kim C W, Lim Y J, et al. Microrough titanium surface affects biologic response in MG63 osteoblast-like cells [J]. J. Biomed. Mater. Res., 2006, 79A: 1023
doi: 10.1002/jbm.a.31040
|
| 87 |
Yu W Q, Jiang X Q, Zhang F Q, et al. The effect of anatase TiO2 nanotube layers on MC3T3-E1 preosteoblast adhesion, proliferation, and differentiation [J]. J. Biomed. Mater. Res., 2010, 94A: 1012
|
| 88 |
Zhao L Z, Mei S L, Chu P K, et al. The influence of hierarchical hybrid micro/nano-textured titanium surface with titania nanotubes on osteoblast functions [J]. Biomaterials, 2010, 31: 5072
doi: 10.1016/j.biomaterials.2010.03.014
|
| 89 |
Huang X B, Liu Y P, Yu H W, et al. One-step fabrication of cytocompatible micro/nano-textured surface with TiO2 mesoporous arrays on titanium by high current anodization [J]. Electrochim. Acta, 2016, 199: 116
doi: 10.1016/j.electacta.2016.03.119
|
| 90 |
Hu N, Wu Y Z, Xie L X, et al. Enhanced interfacial adhesion and osseointegration of anodic TiO2 nanotube arrays on ultra-fine-grained titanium and underlying mechanisms [J]. Acta Biomater., 2020, 106: 360
doi: 10.1016/j.actbio.2020.02.009
|
| 91 |
Lee J K, Choi D S, Jang I, et al. Improved osseointegration of dental titanium implants by TiO2 nanotube arrays with recombinant human bone morphogenetic protein-2: A pilot in vivo study [J]. Int. J. Nanomedicine, 2015, 10: 1145
|
| 92 |
Su E P, Justin D E, Pratt C R, et al. Effects of titanium nanotubes on the osseointegration, cell differentiation, mineralisation and antibacterial properties of orthopaedic implant surfaces [J]. Bone Joint J., 2018, 100-B: 9
|
| 93 |
Kim S Y, Kim Y K, Park I S, et al. Effect of alkali and heat treatments for bioactivity of TiO2 nanotubes [J]. Appl. Surf. Sci., 2014, 321: 412
doi: 10.1016/j.apsusc.2014.09.177
|
| 94 |
Kang M K, Moon S K, Kim K M, et al. Antibacterial effect and cytocompatibility of nano-structured TiO2 film containing Cl [J]. Dent. Mater. J., 2011, 30: 790
doi: 10.4012/dmj.2011-021
|
| 95 |
Liang Y Q, Yang X J, Cui Z D, et al. Self-organized nanotubular layer on Ti-4Zr-22Nb-2Sn alloys formed in organic electrolytes [J]. J. Mater. Res., 2009, 24: 3647
doi: 10.1557/jmr.2009.0427
|
| 96 |
Shin K R, Kim Y S, Kim G W, et al. Effects of concentration of Ag nanoparticles on surface structure and in vitro biological responses of oxide layer on pure titanium via plasma electrolytic oxidation [J]. Appl. Surf. Sci., 2015, 347: 574
doi: 10.1016/j.apsusc.2015.04.161
|
| 97 |
Kaluđerović M R, Schreckenbach J P, Graf H L. First titanium dental implants with white surfaces: Preparation and in vitro tests [J]. Dent. Mater., 2014, 30: 759
doi: 10.1016/j.dental.2014.04.005
pmid: 24853435
|
| 98 |
Wang H Y, Zhu R F, Lu Y P, et al. Preparation and properties of plasma electrolytic oxidation coating on sandblasted pure titanium by a combination treatment [J]. Mater. Sci. Eng., 2014, C42: 657
|
| 99 |
Hong M H, Lee D H, Kim K M, et al. Study on bioactivity and bonding strength between Ti alloy substrate and TiO2 film by micro-arc oxidation [J]. Thin Solid Films, 2011, 519: 7065
doi: 10.1016/j.tsf.2011.01.223
|
| 100 |
Wang R Y, He X J, Gao Y E, et al. Antimicrobial property, cytocompatibility and corrosion resistance of Zn-doped ZrO2/TiO2 coatings on Ti6Al4V implants [J]. Mater. Sci. Eng., 2017, C75: 7
|
| 101 |
Matos A O, Ricomini-Filho A P, Beline T, et al. Three-species biofilm model onto plasma-treated titanium implant surface [J]. Colloids Surf., 2017, 152B: 354
|
| 102 |
Zhang J, Tu Q S, Bonewald L F, et al. Effects of miR-335-5p in modulating osteogenic differentiation by specifically downregulating Wnt antagonist DKK1 [J]. J. Bone Miner. Res., 2011, 26: 1953
doi: 10.1002/jbmr.377
pmid: 21351149
|
| 103 |
Li Y, Fan L K, Liu S Y, et al. The promotion of bone regeneration through positive regulation of angiogenic-osteogenic coupling using microRNA-26a [J]. Biomaterials, 2013, 34: 5048
doi: 10.1016/j.biomaterials.2013.03.052
|
| 104 |
Suh J S, Lee J Y, Choi Y S, et al. Erratum to ‘Peptide-mediated intracellular delivery of miRNA-29b for osteogenic stem cell differentiation' [Biomaterials 34 (2013) 4347-4359] [J]. Biomaterials, 2014, 35: 5039
doi: 10.1016/j.biomaterials.2014.03.010
|
| 105 |
Meng Y B, Li X, Li Z Y, et al. Surface functionalization of titanium alloy with miR-29b nanocapsules to enhance bone regeneration [J]. ACS Appl. Mater. Interfaces, 2016, 8: 5783
doi: 10.1021/acsami.5b10650
|
| 106 |
Geng Z, Wang X G, Zhao J, et al. The synergistic effect of strontium-substituted hydroxyapatite and microRNA-21 on improving bone remodeling and osseointegration [J]. Biomater. Sci., 2018, 6: 2694
doi: 10.1039/C8BM00716K
|
| 107 |
Geng Z, Yu Y M, Li Z Y, et al. Mir-21 promotes osseointegration and mineralization through enhancing both osteogenic and osteoclastic expression [J]. Mater. Sci. Eng., 2020, C111: 110785
|
| 108 |
Zhang X M, Zhu S L, Li Z Y, et al. Multilayer modification on titanium surface for in situ delivery of MicroRNAs [J]. Mater. Lett., 2014, 133: 243
doi: 10.1016/j.matlet.2014.07.024
|
| 109 |
Shahriyari F, Razaghian A, Taghiabadi R, et al. Effect of friction hardening pre-treatment on increasing cytocompatibility of alkali heat-treated Ti-6Al-4V alloy [J]. Surf. Coat. Technol., 2018, 353: 148
doi: 10.1016/j.surfcoat.2018.08.051
|
| 110 |
Sun Y S, Chang J H, Huang H H. Enhancing the biological response of titanium surface through the immobilization of bone morphogenetic protein-2 using the natural cross-linker genipin [J]. Surf. Coat. Technol., 2016, 303: 289
doi: 10.1016/j.surfcoat.2016.02.051
|
| 111 |
Hu H, Cui Z D, Zhu S L, et al. Preparation of hydroxyapatite layer on Ti-based bulk metallic glasses by acid and alkali pre-treatment [J]. Rare Met., 2015, 34: 22
doi: 10.1007/s12598-014-0402-4
|
| 112 |
Chen M F, Liu D B, You C, et al. Interfacial characteristic of graded hydroxyapatite and titanium thin film by magnetron sputtering [J]. Surf. Coat. Technol., 2007, 201: 5688
doi: 10.1016/j.surfcoat.2006.07.057
|
| 113 |
Li M, Li L Q, Su K, et al. Highly effective and noninvasive near-infrared eradication of a Staphylococcus aureus biofilm on implants by a photoresponsive coating within 20 min [J]. Adv. Sci., 2019, 6: 1900599
doi: 10.1002/advs.201900599
|
| 114 |
Tan L, Li J, Liu X M, et al. Rapid biofilm eradication on bone implants using red phosphorus and near-infrared light [J]. Adv. Mater., 2018, 30: 1801808
doi: 10.1002/adma.201801808
|
| 115 |
Hosseinabadi H N, Sajjady S A, Amini S. Creating micro textured surfaces for the improvement of surface wettability through ultrasonic vibration assisted turning [J]. Int. J. Adv. Manuf. Technol., 2018, 96: 2825
doi: 10.1007/s00170-018-1580-2
|
| 116 |
Gao X J, Tong W J, Ouyang X P, et al. Facile fabrication of a superhydrophobic titanium surface with mechanical durability by chemical etching [J]. RSC Adv., 2015, 5: 84666
doi: 10.1039/C5RA15293C
|
| 117 |
Hou X M, Wang X B, Zhu Q S, et al. Preparation of polypropylene superhydrophobic surface and its blood compatibility [J]. Colloids Surf., 2010, 80B: 247
|
| 118 |
Tang P F, Zhang W, Wang Y, et al. Effect of superhydrophobic surface of titanium on Staphylococcus aureus adhesion [J]. J. Nanomater., 2011, 2011: 178921
|
| 119 |
Zhang X, Wan Y, Ren B, et al. Preparation of superhydrophobic surface on titanium alloy via micro-milling, anodic oxidation and fluorination [J]. Micromachines, 2020, 11: 316
doi: 10.3390/mi11030316
|
| 120 |
Patiño-Herrera R, González-Alatorre G, Estrada-Baltazar A, et al. Hydrophobic coatings for prevention of dental enamel erosion [J]. Surf. Coat. Technol., 2015, 275: 148
doi: 10.1016/j.surfcoat.2015.05.026
|
| 121 |
Mi G J, Shi D, Wang M, et al. Reducing bacterial infections and biofilm formation using nanoparticles and nanostructured antibacterial surfaces [J]. Adv. Healthc. Mater., 2018, 7: 1800103
doi: 10.1002/adhm.201800103
|
| 122 |
Kingshott P, Wei J, Bagge-Ravn D, et al. Covalent attachment of poly(ethylene glycol) to surfaces, critical for reducing bacterial adhesion [J]. Langmuir, 2003, 19: 6912
doi: 10.1021/la034032m
|
| 123 |
Harris L G, Tosatti S, Wieland M, et al. Staphylococcus aureus adhesion to titanium oxide surfaces coated with non-functionalized and peptide-functionalized poly(l-lysine)-grafted-poly(ethylene glycol) copolymers [J]. Biomaterials, 2004, 25: 4135
pmid: 15046904
|
| 124 |
Yang F, Williams C G, Wang D A, et al. The effect of incorporating RGD adhesive peptide in polyethylene glycol diacrylate hydrogel on osteogenesis of bone marrow stromal cells [J]. Biomaterials, 2005, 26: 5991
pmid: 15878198
|
| 125 |
Ding X, Yang C, Lim T P, et al. Antibacterial and antifouling catheter coatings using surface grafted PEG-b-cationic polycarbonate diblock copolymers [J]. Biomaterials, 2012, 33: 6593
doi: 10.1016/j.biomaterials.2012.06.001
pmid: 22748920
|
| 126 |
Yang C, Ding X, Ono R J, et al. Brush-like polycarbonates containing dopamine, cations, and PEG providing a broad-spectrum, antibacterial, and antifouling surface via one-step coating [J]. Adv. Mater., 2014, 26: 7346
doi: 10.1002/adma.201402059
|
| 127 |
Li L L, Qi G B, Yu F Q, et al. An adaptive biointerface from self-assembled functional peptides for tissue engineering [J]. Adv. Mater., 2015, 27: 3181
doi: 10.1002/adma.201500658
|
| 128 |
Ivanova E P, Hasan J, Webb H K, et al. Bactericidal activity of black silicon [J]. Nat. Commun., 2013, 4: 2838
doi: 10.1038/ncomms3838
pmid: 24281410
|
| 129 |
Mainwaring D E, Nguyen S H, Webb H, et al. The nature of inherent bactericidal activity: Insights from the nanotopology of three species of dragonfly [J]. Nanoscale, 2016, 8: 6527
doi: 10.1039/c5nr08542j
pmid: 26935293
|
| 130 |
Li J, Tan L, Liu X M, et al. Balancing bacteria-osteoblast competition through selective physical puncture and biofunctionalization of ZnO/polydopamine/arginine-glycine-aspartic acid-cysteine nanorods [J]. ACS Nano, 2017, 11: 11250
doi: 10.1021/acsnano.7b05620
|
| 131 |
Zhong Z X, Xu Z, Sheng T, et al. Unusual air filters with ultrahigh efficiency and antibacterial functionality enabled by ZnO nanorods [J]. ACS Appl. Mater. Interfaces, 2015, 7: 21538
doi: 10.1021/acsami.5b06810
|
| 132 |
Nguyen M N, Lebarbe T, Zouani O F, et al. Impact of RGD nanopatterns grafted onto titanium on osteoblastic cell adhesion [J]. Biomacromolecules, 2012, 13: 896
doi: 10.1021/bm201812u
pmid: 22288777
|
| 133 |
Bellis S L. Advantages of RGD peptides for directing cell association with biomaterials [J]. Biomaterials, 2011, 32: 4205
doi: 10.1016/j.biomaterials.2011.02.029
pmid: 21515168
|
| 134 |
Swartjes J J T M, Das T, Sharifi S, et al. A functional DNase I coating to prevent adhesion of bacteria and the formation of biofilm [J]. Adv. Funct. Mater., 2013, 23: 2843
doi: 10.1002/adfm.201202927
|
| 135 |
Flemming H C, Wingender J. The biofilm matrix [J]. Nat. Rev. Microbiol., 2010, 8: 623
doi: 10.1038/nrmicro2415
|
| 136 |
Arciola C R, Campoccia D, Montanaro L. Implant infections: Adhesion, biofilm formation and immune evasion [J]. Nat. Rev. Microbiol., 2018, 16: 397
doi: 10.1038/s41579-018-0019-y
pmid: 29720707
|
| 137 |
Chen Z W, Ji H W, Liu C Q, et al. A multinuclear metal complex based dnase-mimetic artificial enzyme: Matrix cleavage for combating bacterial biofilms [J]. Angew. Chem. Int. Ed., 2016, 55: 10732
doi: 10.1002/anie.201605296
|
| 138 |
Liu Z W, Wang F M, Ren J S, et al. A series of MOF/Ce-based nanozymes with dual enzyme-like activity disrupting biofilms and hindering recolonization of bacteria [J]. Biomaterials, 2019, 208: 21
doi: 10.1016/j.biomaterials.2019.04.007
|
| 139 |
Miller M B, Bassler B L. Quorum sensing in bacteria [J]. Annu. Rev. Microbiol., 2001, 55: 165
pmid: 11544353
|
| 140 |
Waters C M, Bassler B L. Quorum sensing: Cell-to-cell communication in bacteria [J]. Annu. Rev. Cell. Dev. Biol., 2005, 21: 319
doi: 10.1146/annurev.cellbio.21.012704.131001
|
| 141 |
Flickinger S T, Copeland M F, Downes E M, et al. Quorum sensing between Pseudomonas aeruginosa biofilms accelerates cell growth [J]. J. Am. Chem. Soc., 2011, 133: 5966
doi: 10.1021/ja111131f
pmid: 21434644
|
| 142 |
Sun Y H, Qin H S, Yan Z Q, et al. Combating biofilm associated infection in vivo: Integration of quorum sensing inhibition and photodynamic treatment based on multidrug delivered hollow carbon nitride sphere [J]. Adv. Funct. Mater., 2019, 29: 1808222
doi: 10.1002/adfm.201808222
|
| 143 |
Vermote A, Brackman G, Risseeuw M D P, et al. Hamamelitannin analogues that modulate quorum sensing as potentiators of antibiotics against Staphylococcus aureus [J]. Angew. Chem. Int. Ed., 2016, 55: 6551
doi: 10.1002/anie.201601973
pmid: 27095479
|
| 144 |
Ivanova K, Fernandes M M, Mendoza E, et al. Enzyme multilayer coatings inhibit Pseudomonas aeruginosa biofilm formation on urinary catheters [J]. Appl. Microbiol. Biotechnol., 2015, 99: 4373
doi: 10.1007/s00253-015-6378-7
|
| 145 |
Yuan Z, He Y, Lin C C, et al. Antibacterial surface design of biomedical titanium materials for orthopedic applications [J]. J. Mater. Sci. Technol., 2021, 78: 51
doi: 10.1016/j.jmst.2020.10.066
|
| 146 |
Handke L D, Rogers K L, Olson M E, et al. Staphylococcus epidermidis saeR is an effector of anaerobic growth and a mediator of acute inflammation [J]. Infect. Immun., 2008, 76: 141
doi: 10.1128/IAI.00556-07
pmid: 17954724
|
| 147 |
Yang S B, Han X G, Yang Y, et al. Bacteria-targeting nanoparticles with microenvironment-responsive antibiotic release to eliminate intracellular Staphylococcus aureus and associated infection [J]. ACS Appl. Mater. Interfaces, 2018, 10: 14299
doi: 10.1021/acsami.7b15678
|
| 148 |
Chatterjee S S, Joo H S, Duong A C, et al. Essential Staphylococcus aureus toxin export system [J]. Nat. Med., 2013, 19: 364
doi: 10.1038/nm.3047
pmid: 23396209
|
| 149 |
Sutrisno L, Hu Y, Shen X K, et al. Fabrication of hyaluronidase-responsive biocompatible multilayers on BMP2 loaded titanium nanotube for the bacterial infection prevention [J]. Mater. Sci. Eng., 2018, C89: 95
|
| 150 |
Zhuk I, Jariwala F, Attygalle A B, et al. Self-defensive layer-by-layer films with bacteria-triggered antibiotic release [J]. ACS Nano, 2014, 8: 7733
doi: 10.1021/nn500674g
|
| 151 |
Yuan Z, Huang S Z, Lan S X, et al. Surface engineering of titanium implants with enzyme-triggered antibacterial properties and enhanced osseointegration in vivo [J]. J. Mater. Chem., 2018, 6B: 8090
|
| 152 |
Jia Z J, Xiu P, Li M, et al. Bioinspired anchoring AgNPs onto micro-nanoporous TiO2 orthopedic coatings: Trap-killing of bacteria, surface-regulated osteoblast functions and host responses [J]. Biomaterials, 2016, 75: 203
doi: 10.1016/j.biomaterials.2015.10.035
|
| 153 |
Lin X, Yang S F, Lai K, et al. Orthopedic implant biomaterials with both osteogenic and anti-infection capacities and associated in vivo evaluation methods [J]. Nanomed: Nanotechnol. Biol. Med., 2017, 13: 123
doi: 10.1016/j.nano.2016.08.003
|
| 154 |
Afewerki S, Bassous N, Harb S, et al. Advances in dual functional antimicrobial and osteoinductive biomaterials for orthopaedic applications [J]. Nanomed: Nanotechnol., Biol. Med., 2020, 24: 102143
doi: 10.1016/j.nano.2019.102143
|
| 155 |
Wang Z M, Wang K F, Lu X, et al. Nanostructured architectures by assembling polysaccharide-coated BSA nanoparticles for biomedical application [J]. Adv. Healthc. Mater., 2015, 4: 927
doi: 10.1002/adhm.201400684
|
| 156 |
Min J, Choi K Y, Dreaden E C, et al. Designer dual therapy nanolayered implant coatings eradicate biofilms and accelerate bone tissue repair [J]. ACS Nano, 2016, 10: 4441
doi: 10.1021/acsnano.6b00087
|
| 157 |
Verlee A, Mincke S, Stevens C V. Recent developments in antibacterial and antifungal chitosan and its derivatives [J]. Carbohydr. Polym., 2017, 164: 268
doi: 10.1016/j.carbpol.2017.02.001
|
| 158 |
Chua P H, Neoh K G, Kang E T, et al. Surface functionalization of titanium with hyaluronic acid/chitosan polyelectrolyte multilayers and RGD for promoting osteoblast functions and inhibiting bacterial adhesion [J]. Biomaterials, 2008, 29: 1412
doi: 10.1016/j.biomaterials.2007.12.019
|
| 159 |
Ordikhani F, Tamjid E, Simchi A. Characterization and antibacterial performance of electrodeposited chitosan-vancomycin composite coatings for prevention of implant-associated infections [J]. Mater. Sci. Eng., 2014, C41: 240
|
| 160 |
Lin J, Qiu S Y, Lewis K, et al. Mechanism of bactericidal and fungicidal activities of textiles covalently modified with alkylated polyethylenimine [J]. Biotechnol. Bioeng., 2003, 83: 168
doi: 10.1002/bit.10651
|
| 161 |
Atar-Froyman L, Sharon A, Weiss E I, et al. Anti-biofilm properties of wound dressing incorporating nonrelease polycationic antimicrobials [J]. Biomaterials, 2015, 46: 141
doi: 10.1016/j.biomaterials.2014.12.047
pmid: 25678123
|
| 162 |
Asri L A T W, Crismaru M, Roest S, et al. A shape-adaptive, antibacterial-coating of immobilized quaternary-ammonium compounds tethered on hyperbranched polyurea and its mechanism of action [J]. Adv. Funct. Mater., 2014, 24: 346
doi: 10.1002/adfm.201301686
|
| 163 |
Wei T, Zhan W J, Yu Q, et al. Smart biointerface with photoswitched functions between bactericidal activity and bacteria-releasing ability [J]. ACS Appl. Mater. Interfaces, 2017, 9: 25767
doi: 10.1021/acsami.7b06483
|
| 164 |
Zasloff M. Antimicrobial peptides of multicellular organisms [J]. Nature, 2002, 415: 389
doi: 10.1038/415389a
|
| 165 |
Reddy K V R, Yedery R D, Aranha C. Antimicrobial peptides: Premises and promises [J]. Int. J. Antimicrob. Agents, 2004, 24: 536
doi: 10.1016/j.ijantimicag.2004.09.005
|
| 166 |
Brogden K A. Antimicrobial peptides: Pore formers or metabolic inhibitors in bacteria? [J]. Nat. Rev. Microbiol., 2005, 3: 238
doi: 10.1038/nrmicro1098
pmid: 15703760
|
| 167 |
Campoccia D, Montanaro L, Arciola C R. A review of the biomaterials technologies for infection-resistant surfaces [J]. Biomaterials, 2013, 34: 8533
doi: 10.1016/j.biomaterials.2013.07.089
pmid: 23953781
|
| 168 |
Mellier C, Fayon F, Boukhechba F, et al. Design and properties of novel gallium-doped injectable apatitic cements [J]. Acta Biomater., 2015, 24: 322
doi: 10.1016/j.actbio.2015.05.027
|
| 169 |
Mei S L, Wang H Y, Wang W, et al. Antibacterial effects and biocompatibility of titanium surfaces with graded silver incorporation in titania nanotubes [J]. Biomaterials, 2014, 35: 4255
doi: 10.1016/j.biomaterials.2014.02.005
|
| 170 |
Zhang L, Gao Q, Han Y. Zn and Ag co-doped anti-microbial TiO2 coatings on Ti by micro-arc oxidation [J]. J. Mater. Sci. Technol., 2016, 32: 919
doi: 10.1016/j.jmst.2016.01.008
|
| 171 |
Sedelnikova M B, Komarova E G, Sharkeev Y P, et al. Modification of titanium surface via Ag-, Sr- and Si-containing micro-arc calcium phosphate coating [J]. Bioact. Mater., 2019, 4: 224
doi: 10.1016/j.bioactmat.2019.07.001
pmid: 31406950
|
| 172 |
Roknian M, Fattah-alhosseini A, Gashti S O, et al. Study of the effect of ZnO nanoparticles addition to PEO coatings on pure titanium substrate: Microstructural analysis, antibacterial effect and corrosion behavior of coatings in ringer's physiological solution [J]. J. Alloys Compd., 2018, 740: 330
doi: 10.1016/j.jallcom.2017.12.366
|
| 173 |
Liu W W, Su P L, Chen S, et al. Synthesis of TiO2 nanotubes with ZnO nanoparticles to achieve antibacterial properties and stem cell compatibility [J]. Nanoscale, 2014, 6: 9050
doi: 10.1039/C4NR01531B
|
| 174 |
Maimaiti B, Zhang N Y, Yan L, et al. Stable ZnO-doped hydroxyapatite nanocoating for anti-infection and osteogenic on titanium [J]. Colloids Surf., 2020, 186B: 110731
|
| 175 |
Ma Z, Ren L, Shahzad M B, et al. Hot deformation behavior of Cu-bearing antibacterial titanium alloy [J]. J. Mater. Sci. Technol., 2018, 34: 1867
doi: 10.1016/j.jmst.2017.12.015
|
| 176 |
Liu H, Liu R, Ullah I, et al. Rough surface of copper-bearing titanium alloy with multifunctions of osteogenic ability and antibacterial activity [J]. J. Mater. Sci. Technol., 2020, 48: 130
doi: 10.1016/j.jmst.2019.12.019
|
| 177 |
Liu R, Tang Y L, Liu H, et al. Effects of combined chemical design (Cu addition) and topographical modification (SLA) of Ti-Cu/SLA for promoting osteogenic, angiogenic and antibacterial activities [J]. J. Mater. Sci. Technol., 2020, 47: 202
doi: 10.1016/j.jmst.2019.10.045
|
| 178 |
Agarwal A, Weis T L, Schurr M J, et al. Surfaces modified with nanometer-thick silver-impregnated polymeric films that kill bacteria but support growth of mammalian cells [J]. Biomaterials, 2010, 31: 680
doi: 10.1016/j.biomaterials.2009.09.092
pmid: 19864019
|
| 179 |
Cheng H, Xiong W, Fang Z, et al. Strontium (Sr) and silver (Ag) loaded nanotubular structures with combined osteoinductive and antimicrobial activities [J]. Acta Biomater., 2016, 31: 388
doi: S1742-7061(15)30222-1
pmid: 26612413
|
| 180 |
Tîlmaciu C M, Mathieu M, Lavigne J P, et al. In vitro and in vivo characterization of antibacterial activity and biocompatibility: A study on silver-containing phosphonate monolayers on titanium [J]. Acta Biomater., 2015, 15: 266
doi: 10.1016/j.actbio.2014.12.020
|
| 181 |
van Hengel I A J, Putra N E, Tierolf M W A M, et al. Biofunctionalization of selective laser melted porous titanium using silver and zinc nanoparticles to prevent infections by antibiotic-resistant bacteria [J]. Acta Biomater., 2020, 107: 325
doi: S1742-7061(20)30132-X
pmid: 32145392
|
| 182 |
Shen X K, Hu Y, Xu G Q, et al. Regulation of the biological functions of osteoblasts and bone formation by Zn-incorporated coating on microrough titanium [J]. ACS Appl. Mater. Interfaces, 2014, 6: 16426
doi: 10.1021/am5049338
|
| 183 |
Jin G D, Cao H L, Qiao Y Q, et al. Osteogenic activity and antibacterial effect of zinc ion implanted titanium [J]. Colloids Surf., 2014, 117B: 158
|
| 184 |
Huo K F, Zhang X M, Wang H R, et al. Osteogenic activity and antibacterial effects on titanium surfaces modified with Zn-incorporated nanotube arrays [J]. Biomaterials, 2013, 34: 3467
doi: 10.1016/j.biomaterials.2013.01.071
|
| 185 |
Liu P, Zhao Y C, Yuan Z, et al. Construction of Zn-incorporated multilayer films to promote osteoblasts growth and reduce bacterial adhesion [J]. Mater. Sci. Eng., 2017, C75: 998
|
| 186 |
Wu M C, Deokar A R, Liao J H, et al. Graphene-based photothermal agent for rapid and effective killing of bacteria [J]. ACS Nano, 2013, 7: 1281
doi: 10.1021/nn304782d
|
| 187 |
Wang C, Wang Y L, Zhang L L, et al. Pretreated macrophage-membrane-coated gold nanocages for precise drug delivery for treatment of bacterial infections [J]. Adv. Mater., 2018, 30: 1804023
doi: 10.1002/adma.201804023
|
| 188 |
Qiao Y, Ping Y, Zhang H B, et al. Laser-activatable CuS nanodots to treat multidrug-resistant bacteria and release copper ion to accelerate healing of infected chronic nonhealing wounds [J]. ACS Appl. Mater. Interfaces, 2019, 11: 3809
doi: 10.1021/acsami.8b21766
|
| 189 |
Yin W Y, Yu J, Lv F T, et al. Functionalized nano-MoS2 with peroxidase catalytic and near-infrared photothermal activities for safe and synergetic wound antibacterial applications [J]. ACS Nano, 2016, 10: 11000
doi: 10.1021/acsnano.6b05810
|
| 190 |
Cheng W, Zeng X W, Chen H Z, et al. Versatile polydopamine platforms: Synthesis and promising applications for surface modification and advanced nanomedicine [J]. ACS Nano, 2019, 13: 8537
doi: 10.1021/acsnano.9b04436
pmid: 31369230
|
| 191 |
Lei W X, Ren K F, Chen T T, et al. Polydopamine nanocoating for effective photothermal killing of bacteria and fungus upon near-infrared irradiation [J]. Adv. Mater. Interfaces, 2016, 3: 1600767
doi: 10.1002/admi.201600767
|
| 192 |
Yuan Z, Tao B L, He Y, et al. Biocompatible MoS2/PDA-RGD coating on titanium implant with antibacterial property via intrinsic ROS-independent oxidative stress and NIR irradiation [J]. Biomaterials, 2019, 217: 119290
doi: 10.1016/j.biomaterials.2019.119290
|
| 193 |
Xie X Z, Mao C Y, Liu X M, et al. Synergistic bacteria killing through photodynamic and physical actions of graphene oxide/Ag/collagen coating [J]. ACS Appl. Mater. Interfaces, 2017, 9: 26417
doi: 10.1021/acsami.7b06702
|
| 194 |
Wang D, Niu L J, Qiao Z Y, et al. Synthesis of self-assembled porphyrin nanoparticle photosensitizers [J]. ACS Nano, 2018, 12: 3796
doi: 10.1021/acsnano.8b01010
|
| 195 |
Zhu Y W, Xu C, Zhang N, et al. Polycationic synergistic antibacterial agents with multiple functional components for efficient anti-infective therapy [J]. Adv. Funct. Mater., 2018, 28: 1706709
doi: 10.1002/adfm.201706709
|
| 196 |
Deng Q Q, Sun P P, Zhang L, et al. Porphyrin MOF dots-based, function-adaptive nanoplatform for enhanced penetration and photodynamic eradication of bacterial biofilms [J]. Adv. Funct. Mater., 2019, 29: 1903018
doi: 10.1002/adfm.201903018
|
| 197 |
Su K, Tan L, Liu X M, et al. Rapid photo-sonotherapy for clinical treatment of bacterial infected bone implants by creating oxygen deficiency using sulfur doping [J]. ACS Nano, 2020, 14: 2077
doi: 10.1021/acsnano.9b08686
|
| 198 |
Feng Z Z, Liu X M, Tan L, et al. Electrophoretic deposited stable chitosan@MoS2 coating with rapid in situ bacteria-killing ability under dual-light irradiation [J]. Small, 2018, 14: 1704347
doi: 10.1002/smll.201704347
|
| 199 |
Yuan Z, Tao B L, He Y, et al. Remote eradication of biofilm on titanium implant via near-infrared light triggered photothermal/photodynamic therapy strategy [J]. Biomaterials, 2019, 223: 119479
doi: 10.1016/j.biomaterials.2019.119479
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|