| 高碳钢连铸坯大区域C元素分布不均匀度 |
郭中傲1,2, 彭治强1,2, 柳前1,2, 侯自兵1,2( ) |
1.重庆大学 材料科学与工程学院 重庆 400044 2.重庆大学 钒钛冶金及新材料重庆市重点实验室 重庆 400044 |
|
| Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet |
GUO Zhongao1,2, PENG Zhiqiang1,2, LIU Qian1,2, HOU Zibing1,2( ) |
1.College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China 2.Chongqing Key Laboratory of Vanadium-Titanium Metallurgy and New Materials, Chongqing University, Chongqing 400044, China |
引用本文:
郭中傲, 彭治强, 柳前, 侯自兵. 高碳钢连铸坯大区域C元素分布不均匀度[J]. 金属学报, 2021, 57(12): 1595-1606.
Zhongao GUO,
Zhiqiang PENG,
Qian LIU,
Zibing HOU.
Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. Acta Metall Sin, 2021, 57(12): 1595-1606.
| 1 |
Wang G D. Technology innovation and development direction of iron and steel industry [J]. Iron Steel, 2015, 50(9): 1
|
| 1 |
王国栋. 钢铁行业技术创新和发展方向 [J]. 钢铁, 2015, 50(9): 1
|
| 2 |
Song X F, He A R, Qiu Z S. Influence of initial temperature difference on high strength strip buckling in laminar cooling [J]. Iron Steel, 2016, 51(5): 52
|
| 2 |
宋小芳, 何安瑞, 邱增帅. 基于初始温差的高强钢板层冷过程前屈曲分析 [J]. 钢铁, 2016, 51(5): 52
|
| 3 |
Li J, Wu M H, Ludwig A, et al. Simulation of macrosegregation in a 2.45-ton steel ingot using a three-phase mixed columnar-equiaxed model [J]. Int. J. Heat Mass Transf., 2014, 72: 668
|
| 4 |
Ge H H, Ren F L, Li J, et al. Four-phase dendritic model for the prediction of macrosegregation, shrinkage cavity, and porosity in a 55-ton ingot [J]. Metall. Mater. Trans., 2017, 48A: 1139
|
| 5 |
Pickering E J. Macrosegregation in steel ingots: The applicability of modelling and characterisation techniques [J]. ISIJ Int., 2013, 53: 935
|
| 6 |
Choudhary S K, Ganguly S. Morphology and segregation in continuously cast high carbon steel billets [J]. ISIJ Int., 2007, 47: 1759
|
| 7 |
Mayer F, Wu M, Ludwig A. On the formation of centreline segregation in continuous slab casting of steel due to bulging and/or feeding [J]. Steel Res. Int., 2010, 81: 660
|
| 8 |
Miyamura K, Kitamura S Y, Sakaguchi S, et al. Development of segregation etch print method and its application to investigation of CC slab segregation [J]. Trans. Iron Steel Inst. Japan, 1984, 24: 718
|
| 9 |
Sang B G, Kang X H, Li D Z. A novel technique for reducing macrosegregation in heavy steel ingots [J]. J. Mater. Process. Technol., 2010, 210: 703
|
| 10 |
Lesoult G. Macrosegregation in steel strands and ingots: Characterisation, formation and consequences [J]. Mater. Sci. Eng., 2005, A413-414: 19
|
| 11 |
Yoshida N, Umezawa O, Nagai K. Influence of phosphorus on solidification structure in continuously cast 0.1 mass% carbon steel [J]. ISIJ Int., 2003, 43: 348
|
| 12 |
Wang H Z. Original position statistic distribution analysis (original position analysis)—A new analytical method in research and quality evaluation of materials [J]. Sci. China, 2003, 46B: 119
|
| 13 |
Chen Y, Yang S B, Zhu M Y. Key technologies of internal quality control for continuously cast high-speed rail steel bloom [J]. Iron Steel, 2006, 41(12): 36
|
| 13 |
陈 永, 杨素波, 朱苗勇. 高速轨用钢连铸坯内部质量控制的关键技术 [J]. 钢铁, 2006, 41(12): 36
|
| 14 |
Chang Y, Hou Z B, Wang W, et al. Characteristics and mechanism of carbon element and manganese element distribution along casting direction in high-carbon billet [J]. Iron Steel, 2016, 51(11): 43
|
| 14 |
常 毅, 侯自兵, 王 伟等. 高碳钢方坯碳锰元素纵向分布及机理 [J]. 钢铁, 2016, 51(11): 43
|
| 15 |
Harada H, Miyazawa K I, Matsumiya T, et al. Numerical prediction of solidification structure taking account of molten steel flow [J]. Tetsu Hagané, 2003, 89: 265
|
| 15 |
原田寛, 宮沢憲一, 松宮徹等. 流動の影響を考慮した凝固組織推定モデル [J]. 鐵と鋼. 2003, 89: 265
|
| 16 |
Zhang N, Yang P, Mao W M. Influence of columnar grains on the cold rolling texture evolution in Fe-3%Si electrical steel [J]. Acta Metall. Sin., 2012, 48: 782
|
| 16 |
张 宁, 杨 平, 毛卫民. 柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响 [J]. 金属学报, 2012, 48: 782
|
| 17 |
Hou Z B, Guo Z A, Guo D W, et al. A new method for carbon content distribution based on grayscale image of casting blank macrostructure in carbon steel [J]. J. Iron Steel Res., 2019, 31: 620
|
| 17 |
侯自兵, 郭中傲, 郭东伟等. 利用碳钢铸坯组织灰度图获取C含量分布的方法 [J]. 钢铁研究学报, 2019, 31: 620
|
| 18 |
Lai Y L, Chen W F, Hu Z W, et al. Corrosion of magnesium alloy and its corrosion morphology fractal [J]. Mater. Prot., 2018, 51(6): 28
|
| 18 |
赖勇来, 陈文峰, 胡志文等. 镁合金腐蚀及其腐蚀形貌分形 [J]. 材料保护, 2018, 51(6): 28
|
| 19 |
Wang G T, Deng Y H, Wu L M. Metallographic quantitative analysis using digital image process [J]. Heat Treat. Met., 2006, 31(2):66
|
| 19 |
王桂棠, 邓耀华, 吴黎明. 基于数字图像处理技术的金相组织定量分析 [J]. 金属热处理, 2006, 31(2): 66
|
| 20 |
Liao K W, Lee Y T. Detection of rust defects on steel bridge coatings via digital image recognition [J]. Automat. Constr., 2016, 71: 294
|
| 21 |
Huang Z L. The high-temperature billet crack detection research based on digital image processing [D] Chengdu: University of Electronic Science and Technology of China, 2013
|
| 21 |
黄志良. 基于数字图像处理的高温钢坯裂纹检测研究 [D]. 成都: 电子科技大学, 2013
|
| 22 |
Gong H J. Estimating paddy yield based on fractal and image texture analysis [D]. Nanjing Agricultural University, 2008
|
| 22 |
龚红菊. 基于分形理论及图像纹理分析的水稻产量预测方法研究 [D]. 南京: 南京农业大学, 2008
|
| 23 |
Mandelbrot B B. The Fractal Geometry of Nature [M]. San Francisco: Freeman, 1982: 206
|
| 24 |
Wang Y Q, Huang L P, Li J. The application of fractal theory in the surface analyzing of worn materials [J]. Mater. Rep., 1998, 12(2): 8
|
| 24 |
王乙潜, 黄立萍, 郦 剑. 分形理论在材料磨损表面分析中的应用 [J]. 材料导报, 1998, 12(2): 8
|
| 25 |
Mandelbrot B B, Passoja D E, Paullay A J. Fractal character of fracture surfaces of metals [J]. Nature, 1984, 308: 721
|
| 26 |
Wang S Y, Song S Z. Corrosion morphology diagnosing syste of metallic materials in seawater based on fractal [J]. Acta Metall. Sin., 2004, 40: 94
|
| 26 |
王守琰, 宋诗哲. 基于分形的金属材料海水腐蚀形貌图像分析诊断系统 [J]. 金属学报, 2004, 40: 94
|
| 27 |
Sarkar N, Chaudhuri B B. An efficient differential box-counting approach to compute fractal dimension of image [J]. IEEE Trans. Syst. Man Cybern., 1994, 24: 115
|
| 28 |
Haralick R M. Statistical and structural approaches to texture [J]. Proc. IEEE, 1957, 67: 786
|
| 29 |
Renzetti F R, Zortea L. Use of a gray level co-occurrence matrix to characterize duplex stainless steel phases microstructure [J]. Frattura ed Integrità Strutturale, 2013, 5: 43
|
| 30 |
Tong X Y, Li H X, Yao L J, et al. Feature extraction and analysis of surface microscopic image of pure copper subjecting low cycle fatigue [J]. Mech. Sci. Technol. Aerosp. Eng., 2015, 34: 1446
|
| 30 |
童小燕, 李洪旭, 姚磊江等. 纯铜低周疲劳表面显微形貌的特征提取与分析 [J]. 机械科学与技术, 2015, 34: 1446
|
| 31 |
Hou Z B, Cao J H, Chang Y, et al. Morphology characteristics of carbon segregation in die steel billet by ESR based on fractal dimension [J]. Acta Metall. Sin., 2017, 53: 769
|
| 31 |
侯自兵, 曹江海, 常 毅等. 基于分形维数的模具钢电渣重熔铸坯碳偏析形貌特征研究 [J]. 金属学报, 2017, 53: 769
|
| 32 |
Wang H Z, Zhao P, Chen J W, et al. In situ statistical distribution analysis of low alloy steel continuous casting slab [J]. Sci. China, 2005, 35E: 260
|
| 32 |
王海舟, 赵 沛, 陈吉文等. 低合金钢连铸坯的原位统计分布分析研究 [J]. 中国科学, 2005, 35E: 260
|
| 33 |
Bowe T F, Brody H D, Flemings M C. Measurements of solute redistribution in dendritic solidification [J]. Trans. Metall. Soc. AIME, 1996, 236: 624
|
| 34 |
Hou Z B, Guo D W, Cao J H, et al. A method based on the centroid of segregation points: A Voronoi polygon application to solidification of alloys [J]. J. Alloys Compd., 2018, 762: 508
|
| 35 |
Burton J A, Prim R C, Slichter W P. The distribution of solute in crystals grown from the melt. Part I. Theoretical [J]. J. Chem. Phys., 1953, 21: 1987
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|