AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究 |
邓丽萍1,崔凯旋2,汪炳叔2(),向红亮1,李强2 |
1. 福州大学机械工程及自动化学院 福州 350108 2. 福州大学材料科学与工程学院 福州 350108 |
|
Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature |
Liping DENG1,Kaixuan CUI2,Bingshu WANG2(),Hongliang XIANG1,Qiang LI2 |
1. School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108, China 2. College of Materials Science and Engineering, Fuzhou University,Fuzhou 350108, China |
引用本文:
邓丽萍,崔凯旋,汪炳叔,向红亮,李强. AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究[J]. 金属学报, 2019, 55(8): 976-986.
Liping DENG,
Kaixuan CUI,
Bingshu WANG,
Hongliang XIANG,
Qiang LI.
Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. Acta Metall Sin, 2019, 55(8): 976-986.
[1] | Liu Q. Research progress on plastic deformation mechanism of Mg alloys [J]. Acta Metall. Sin., 2010, 46: 1458 | [1] | (刘 庆. 镁合金塑性变形机理研究进展 [J]. 金属学报, 2010, 46: 1458) | [2] | Chakkedath A, Boehlert C J. In situ scanning electron microscopy observations of contraction twinning and double twinning in extruded Mg-1Mn (wt. %) [J]. JOM, 2015, 67: 1748 | [3] | Knezevic M, Levinson A, Harris R, et al. Deformation twinning in AZ31: Influence on strain hardening and texture evolution [J]. Acta Mater., 2010, 58: 6230 | [4] | Barnett M R. Twinning and the ductility of magnesium alloys: Part I: "Tension" twins [J]. Mater. Sci. Eng., 2007, A464: 1 | [5] | Li S Q, Tang W N, Chen R S, et al. Effect of pre-induced twinning on microstructure and tensile ductility in GW92K magnesium alloy during multi-direction forging at decreasing temperature [J]. J. Magnes. Alloys, 2014, 2: 287 | [6] | Xu S, Liu T M, Chen H C, et al. Reducing the tension-compression yield asymmetry in a hot-rolled Mg-3Al-1Zn alloy via multidirectional pre-compression [J]. Mater. Sci. Eng., 2013, A565: 96 | [7] | Kuang X L, Liu T M, He J J. Evolution of texture and yielding behavior induced by {101ˉ2} twinning of magnesium alloy [J]. Chin. J. Nonferrous Met., 2014, 24: 1111 | [7] | (况新亮, 刘天模, 何杰军. 基于镁合金{1012}孪生的织构调整及屈服行为演变 [J]. 中国有色金属学报, 2014, 24: 1111) | [8] | Xin Y C, Jiang J, Chapuis A, et al. Plastic deformation behavior of AZ31 magnesium alloy under multiple passes cross compression [J]. Mater. Sci. Eng., 2012, A532: 50 | [9] | Song G S, Jiang J Q, Xu Y, et al. Influence of AZ31 magnesium alloy sheet compressed along various paths on mechanical properties [J]. Chin. J. Nonferrous Met., 2016, 26: 2469 | [9] | (宋广胜, 姜敬前, 徐 勇等. AZ31镁合金板材变路径压缩对力学性能影响 [J]. 中国有色金属学报, 2016, 26: 2469) | [10] | Hou D W, Liu T M, Luo L J, et al. Twinning behaviors of a rolled AZ31 magnesium alloy under multidirectional loading [J]. Mater. Charact., 2017, 124: 122 | [11] | Yang X Y, Miura H, Sakai T. Structural development at severely high strain in AZ31 magnesium alloy processed by cold forging and subsequent annealing [J]. Mater. Des., 2013, 44: 573 | [12] | Xia X S, Chen Q, Zhao Z D, et al. Microstructure, texture and mechanical properties of coarse-grained Mg-Gd-Y-Nd-Zr alloy processed by multidirectional forging [J]. J. Alloys Compd., 2015, 623: 62 | [13] | Jiang M G, Yan H, Chen R S. Twinning, recrystallization and texture development during multi-directional impact forging in an AZ61 Mg alloy [J]. J. Alloys Compd., 2015, 650: 399 | [14] | Ulacia I, Dudamell N V, Gálvez F, et al. Mechanical behavior and microstructural evolution of a Mg AZ31 sheet at dynamic strain rates [J]. Acta Mater., 2010, 58: 2988 | [15] | Chun Y B, Davies C H J. Twinning-induced negative strain rate sensitivity in wrought Mg alloy AZ31 [J]. Mater. Sci. Eng., 2011, A528: 5713 | [16] | Yang X Y, Sun Z Y, Zhang L. Preparation of submicro and nanosized magnesium alloys by multiply compressed deformation [J]. Acta Metall. Sin., 2010, 46: 607 | [16] | (杨续跃, 孙争艳, 张 雷. 室温多向多道次压缩变形制备亚微米和纳米级镁合金 [J]. 金属学报, 2010, 46: 607) | [17] | Wang B S, Shi J J, Ye P, et al. In-situ investigation on nucleation and propagation of {101ˉ2} twins during uniaxial multi-pass compression in an extruded AZ31 Mg alloy [J]. Mater. Sci. Eng., 2018, A731: 71 | [18] | Li J Q, Liu J, Cui Z S. Microstructures and mechanical properties of AZ61 magnesium alloy after isothermal multidirectional forging with increasing strain rate [J]. Mater. Sci. Eng., 2015, A643: 32 | [19] | Wang L F, Huang G S, Quan Q, et al. The effect of twinning and detwinning on the mechanical property of AZ31 extruded magnesium alloy during strain-path changes [J]. Mater. Des., 2014, 63: 177 | [20] | Guo C F, Xin R L, Ding C H, et al. Understanding of variant selection and twin patterns in compressed Mg alloy sheets via combined analysis of Schmid factor and strain compatibility factor [J]. Mater. Sci. Eng., 2014, A609: 92 | [21] | Wang B S, Deng L P, Guo N, et al. EBSD analysis of {101ˉ2} twinning activity in Mg-3Al-1Zn alloy during compression [J]. Mater. Charact., 2014, 98: 180 | [22] | Xin R L, Liang Y C, Ding C H, et al. Geometrical compatibility factor analysis of paired extension twins in extruded Mg-3Al-1Zn alloys [J]. Mater. Des., 2015, 86: 656 | [23] | Xin Y C, Zhou X J, Wu Y, et al. Deformation behavior and mechanical properties of composite twin structures under different loading paths [J]. Mater. Sci. Eng., 2015, A640: 118 | [24] | Wang C, Ding H, Wang B S, et al. Effects of deformation texture and twins on the corrosion resistance of rolled AZ31 Mg alloy under 5% uniaxial compression [J]. Acta. Metall. Sin. (Engl. Lett.), 2017, 30: 921 | [25] | Park S H, Hong S G, Lee J H, et al. Texture evolution of rolled Mg-3Al-1Zn alloy undergoing a {101ˉ2} twinning dominant strain path change [J]. J. Alloys Compd., 2015, 646: 573 |
|
|