高强耐蚀管钢点状偏析及带状缺陷的特征与演变 |
李博1,张忠铧2,刘华松1,罗明2,兰鹏1,唐海燕1,张家泉1( ) |
1. 北京科技大学冶金与生态工程学院 北京 100083 2. 宝钢中央研究院钢管技术中心 上海 201900 |
|
Characteristics and Evolution of the Spot Segregations and Banded Defects in High Strength Corrosion Resistant Tube Steel |
Bo LI1,Zhonghua ZHANG2,Huasong LIU1,Ming LUO2,Peng LAN1,Haiyan TANG1,Jiaquan ZHANG1( ) |
1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China 2. Tube & Pipe Department, Baosteel Research Institute, Baoshan Iron & Steel Co. , Ltd. , Shanghai 201900, China |
引用本文:
李博,张忠铧,刘华松,罗明,兰鹏,唐海燕,张家泉. 高强耐蚀管钢点状偏析及带状缺陷的特征与演变[J]. 金属学报, 2019, 55(6): 762-772.
Bo LI,
Zhonghua ZHANG,
Huasong LIU,
Ming LUO,
Peng LAN,
Haiyan TANG,
Jiaquan ZHANG.
Characteristics and Evolution of the Spot Segregations and Banded Defects in High Strength Corrosion Resistant Tube Steel[J]. Acta Metall Sin, 2019, 55(6): 762-772.
[1] | Dong X M, Chen Y X, Zhang Z H. Corrosion behavior of H2S resistant steel in H2S solution [J]. Corros. Prot., 2016, 37: 832 | [1] | (董晓明, 陈业新, 张忠铧. 耐硫化氢腐蚀钢在硫化氢介质中的腐蚀行为 [J]. 腐蚀与防护, 2016, 37: 832) | [2] | Tsay L W, Chi M Y, Chen H R, et al. Investigation of hydrogen sulfide stress corrosion cracking of PH 13-8 Mo stainless steel [J]. Mater. Sci. Eng., 2006, A416: 155 | [3] | Zhao M C, Shan Y Y, Li Y H, et al. Effect of microstructure on sulfide stress corrosion cracking of pipeline steels [J]. Acta Metall. Sin., 2001, 37: 1087 | [3] | (赵明纯, 单以银, 李玉海等. 显微组织对管线钢硫化物应力腐蚀开裂的影响 [J]. 金属学报, 2001, 37: 1087) | [4] | Yin Y Q, Tang C X, Zhao J B, et al. Effect of microstructure characteristics on hydrogen sulfide corrosion resistance of X70MS pipe steel [J]. Heat Treat. Met., 2013, 38(5): 32 | [4] | (尹雨群, 唐春霞, 赵晋斌等. 组织特征对X70MS管线钢抗H2S腐蚀行为的影响 [J]. 金属热处理, 2013, 38(5): 32) | [5] | Omura T, Kobayashi K. Hydrogen Embrittlement of OCTG and Linepipes [J]. Corros. Eng., 2011, 60(4): 156 | [6] | Zhang Z H, Liu M, Liu Y H, et al. A systematical analysis with respect to multiple hydrogen traps influencing sulfide stress cracking behavior of API-5CT-C110 casing steel [J]. Mater. Sci. Eng., 2018, A721: 81 | [7] | Vollmer L W. The behavior of steels in hydrogen sulfide environments [J]. Corrosion, 1958, 14(7): 38 | [8] | Urband B E, Morey S. High strength sour service C110 casing [A]. SPE/IADC Drilling Conference [C]. Amsterdam: Society of Petroleum Engineers (SPE), 1999: 14 | [9] | Haida O, Kitaoka H, Habu Y, et al. Macro- and semi-macroscopic features of the centerline segregation in CC slabs and their effect on product quality [J]. Trans. Iron Steel Inst. Jpn., 1984, 24: 891 | [10] | Ji Y, Lan P, Geng H, et al. Behavior of spot segregation in continuously cast blooms and the resulting segregated band in oil pipe steels [J]. Steel Res. Int., 2018, 89: 331 | [11] | Zhang Y L, Liu H Y, Ruan X J, et al. Microsegregation behaviors of alloy elements and their effects on the formation of banded structure in pinion steels [J]. J. Univ. Sci. Technol. Beijing, 2009, 31(suppl.): 199 | [11] | (张延玲, 刘海英, 阮小江等. 中低碳齿轮钢中合金元素的偏析行为及其对带状组织的影响 [J]. 北京科技大学学报, 2009, 31(suppl.): 199) | [12] | Tian Y Q, Song J Y, Wei Y L, et al. Influence of controlled rolling and cooling on banded structure of J55 oil casing [J]. J. Plast. Eng., 2011, 18(6): 110 | [12] | (田亚强, 宋进英, 魏英立等. 控轧控冷工艺对J55石油套管用钢带状组织影响 [J]. 塑性工程学报, 2011, 18(6): 110) | [13] | Oh K S, Chang Y W. Macro and microscopic segregation behavior of center segregations in high carbon steel CC blooms during the final stage of solidification [J]. Process. Technol., 1995, 13: 381 | [14] | Tsuchida Y, Nakada M, Sugawara I, et al. Behavior of semi-macroscopic segregation in continuously cast slabs and technique for reducing the segregation [J]. Trans. Iron Steel Inst. Jpn., 1984, 24: 899 | [15] | Xu Z G, Wang X H, Huang F X, et al. Solidification structure and semi-macro segregation of pipeline steel continuous casting slabs [J]. J. Univ. Sci. Technol. Beijing, 2014, 36: 751 | [15] | (许志刚, 王新华, 黄福祥等. 管线钢连铸板坯的半宏观偏析和凝固组织 [J]. 北京科技大学学报, 2014, 36: 751) | [16] | Pre?linger H, Mayr M, Tragl E, et al. Assessment of the primary structure of slabs and the influence on hot-and cold-rolled strip structure [J]. Steel Res. Int., 2006, 77: 107 | [17] | Ji Y, He Q, Geng H, et al. Effect of dendritic structure on the spot segregation of continuously cast round bloom [A]. AISTech 2017-Proceedings of the Iron and Steel Technology Conference [C]. Nashiville: Association for Iron and Steel Technology (AISTECH), 2017: 2599 | [18] | Wang Q Y. Introduction to Metallurgical Technology [M]. Beijing: Metallurgical Industry Press, 2006: 104 | [18] | (王庆义. 冶金技术概论 [M]. 北京: 冶金工业出版社, 2006: 104) | [19] | Chaube S, Tennyson G, Singh A. Modelling of columnar-to-equiaxed transition and inclusion distribution in continuously cast steel billets [J]. Trans. Indian Inst. Met., 2015, 68: 1207 | [20] | Ma X P, Li D Z. The 3-dimensional morphology of dendrite during equiaxed solidification of an Al-5 wt.% Cu alloy [J]. J. Mater. Sci. Technol., 2019, 35: 239 | [21] | Ji Y. Segregation of billet castings and its heredity effect on the hot-rolled products [D]. Beijing: University of Science & Technology Beijing, 2018 | [21] | (纪 元. 连铸坯偏析及其铸轧遗传性研究 [D]. 北京: 北京科技大学, 2018) | [22] | Verhoeven J D. A review of microsegregation induced banding phenomena in steels [J]. J. Mater. Eng. Perform., 2000, 9: 286 | [23] | Krauss G. Solidification, segregation, and banding in carbon and alloy steels [J]. Metall. Mater. Trans., 2003, 34B: 781 | [24] | Kirkaldy J S, Von Destinon-Forstmann J, Brigham R J. Simulation of banding in steels [J]. Can. Metall. Quart., 1962, 1: 59 | [25] | Thompson S W, Howell P R. Factors influencing ferrite/pearlite banding and origin of large pearlite nodules in a hypoeutectoid plate steel [J]. Mater. Sci. Technol., 1992, 8: 777 | [26] | Kirkaldy J S, Purdy G R. Diffusion in multicomponent metallic systems: V. Interstitial diffusion in dilute ternary austenites [J]. Can. J. Phys., 1962, 40: 208 | [27] | Eckert J A, Howell P R, Thompson S W. Banding and the nature of large, irregular pearlite nodules in a hot-rolled low-alloy plate steel: A second report [J]. J. Mater. Sci., 1993, 28: 4412 | [28] | Gro?terlinden R, Kawalla R, Lotter U, et al. Formation of pearlitic banded structures in ferritic-pearlitic steels [J]. Steel. Res. Int., 1992, 63: 331 | [29] | Rivera-Díaz-Del-Castillo P E J, van Der Zwaag S, Sietsma J. A model for ferrite/pearlite band formation and prevention in steels [J]. Metall. Mater. Trans., 2004, 35A: 425 | [30] | Du C W. Study on surface microstructure and crack control of microalloyed continuous casting billet [D]. Beijing: University of Science and Technology Beijing, 2016 | [30] | (杜辰伟. 微合金连铸坯表层组织与裂纹技术控制研究 [D]. 北京: 北京科技大学, 2016) | [31] | Yong Q L. Second Phase in Steel Material [M]. Beijing: Metallurgical Industry Press, 2006: 102 | [31] | (雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 102) |
|
|