| 不同温度对含与不含位错α-Fe中He原子行为的影响 |
王瑾, 余黎明, 李冲, 黄远, 李会军, 刘永长( ) |
| 天津大学材料科学与工程学院水利安全与仿真国家重点实验室 天津 300354 |
|
| Effect of Different Temperatures on He Atoms Behavior inα-Fe with and without Dislocations |
Jin WANG, Liming YU, Chong LI, Yuan HUANG, Huijun LI, Yongchang LIU( ) |
| State Key Lab of Hydraulic Engineering Simulation and Safety, School of Materials Science and Engineering,Tianjin University, Tianjin 300354, China |
引用本文:
王瑾, 余黎明, 李冲, 黄远, 李会军, 刘永长. 不同温度对含与不含位错α-Fe中He原子行为的影响[J]. 金属学报, 2019, 55(2): 274-280.
Jin WANG,
Liming YU,
Chong LI,
Yuan HUANG,
Huijun LI,
Yongchang LIU.
Effect of Different Temperatures on He Atoms Behavior inα-Fe with and without Dislocations[J]. Acta Metall Sin, 2019, 55(2): 274-280.
| [1] | Ullmaier H.The influence of helium on the bulk properties of fusion reactor structural materials[J]. Nucl. Fusion, 1984, 24: 1039 | | [2] | Zhou X S, Liu C X, Yu L M, et al.Phase transformation behavior and microstructural control of high-Cr martensitic/ferritic heat-resistant steels for power and nuclear plants: a review[J]. J. Mater. Sci. Technol., 2015, 31: 235 | | [3] | Samaras M.Multiscale modelling: The role of helium in iron[J]. Mater. Today, 2009, 12: 46 | | [4] | Bloom E E.The challenge of developing structural materials for fusion power systems [J]. J. Nucl. Mater., 1998, 258-263: 7 | | [5] | Feng Y C, Xing W W, Wang S L, et al.First-principles study of hydrogen behaviors at oxide/ferrite interface in ODS steels[J]. Acta Metall. Sin., 2018, 54: 325(冯宇超, 邢炜伟, 王寿龙等. ODS钢中氧化物/铁素体界面捕氢行为的第一原理研究[J]. 金属学报, 2018, 54: 325) | | [6] | Yang L, Gao F, Kurtz R J, et al.Atomistic simulations of helium clustering and grain boundary reconstruction in alpha-iron[J]. Acta Mater., 2015, 82: 275 | | [7] | Zhang L, Fu C C, Hayward E, et al.Properties of He clustering in α-Fe grain boundaries[J]. J. Nucl. Mater., 2015, 459: 247 | | [8] | Wang Y X, Xu Q, Yoshiie T, et al.Effects of edge dislocations on interstitial helium and helium cluster behavior in α-Fe[J]. J. Nucl. Mater., 2008, 376: 133 | | [9] | Martínez E, Schwen D, Caro A.Helium segregation to screw and edge dislocations in α-iron and their yield strength[J]. Acta Mater., 2015, 84: 208 | | [10] | Ono K, Miyamoto M, Arakawa K, et al.Effects of precipitated helium, deuterium or alloy elements on glissile motion of dislocation loops in Fe-9Cr-2W ferritic alloy[J]. J. Nucl. Mater., 2014, 455: 162 | | [11] | Yamamoto T, Odette G R, Miao P, et al. Helium effects on microstructural evolution in tempered martensitic steels: In situ helium implanter studies in HFIR [J]. J. Nucl. Mater., 2009, 386-388: 338 | | [12] | Xu Q, Yamasaki H, Sugiura Y, et al.Effects of interactions between dislocations and/or vacancies and He atoms on mechanical property changes in Ni[J]. Mater. Sci. Eng., 2013, A586: 231 | | [13] | Xu Q, Sugiura Y, Pan X Q, et al.Effects of dislocation-trapped helium on mechanical properties of Fe[J]. Mater. Sci. Eng., 2014, A612: 41 | | [14] | Wei Y P, Liu P P, Zhu Y M, et al.Evaluation of irradiation hardening and microstructure evolution under the synergistic interaction of He and subsequent Fe ions irradiation in CLAM steel[J]. J. Alloys Compd., 2016, 676: 481 | | [15] | Chen J, Jung P, Hoffelner W, et al.Dislocation loops and bubbles in oxide dispersion strengthened ferritic steel after helium implantation under stress[J]. Acta Mater., 2008, 56: 250 | | [16] | Galindo-Nava E I, Basha B I Y, Rivera-Díaz-del-Castillo P E J. Hydrogen transport in metals: Integration of permeation, thermal desorption and degassing[J]. J. Mater. Sci. Technol., 2017, 33: 1433 | | [17] | Li Q, Parish C M, Powers K A, et al.Helium solubility and bubble formation in a nanostructured ferritic alloy[J]. J. Nucl. Mater., 2014, 445: 165 | | [18] | Shi J Y, Peng L, Ye M Y, et al.Molecular dynamics study: Effects of He bubble and Cr precipitate on tensile deformation of grain boundaries in α-Fe[J]. IEEE Trans. Plasma Sci., 2017, 45: 289 | | [19] | Tschopp M A, Gao F, Yang L, et al.Binding energetics of substitutional and interstitial helium and di-helium defects with grain boundary structure in α-Fe[J]. J. Appl. Phys., 2014, 115: 033503 | | [20] | Osetsky Y N, Stoller R E.Atomic-scale mechanisms of helium bubble hardening in iron[J]. J. Nucl. Mater., 2015, 465: 448 | | [21] | Yang L, Gao F, Kurtz R J, et al.Effects of local structure on helium bubble growth in bulk and at grain boundaries of bcc iron: A molecular dynamics study[J]. Acta Mater., 2015, 97: 86 | | [22] | Morishita K, Sugano R, Wirth B D, et al.Thermal stability of helium-vacancy clusters in iron[J]. Nucl. Instrum. Methods Phys. Res., 2003, 202B: 76 | | [23] | Fu C C, Willaime F.Ab initio study of helium in α-Fe: Dissolution, migration, and clustering with vacancies[J]. Phys. Rev., 2005, 72B: 064117 | | [24] | Stewart D, Osetskiy Y, Stoller R.Atomistic studies of formation and diffusion of helium clusters and bubbles in BCC iron[J]. J. Nucl. Mater., 2011, 417: 1110 | | [25] | Jia X, Dai Y, Victoria M.The impact of irradiation temperature on the microstructure of F82H martensitic/ferritic steel irradiated in a proton and neutron mixed spectrum[J]. J. Nucl. Mater., 2002, 305: 1 | | [26] | Li X C, Shu X L, Tao P, et al.Molecular dynamics simulation of helium cluster diffusion and bubble formation in bulk tungsten[J]. J. Nucl. Mater., 2014, 455: 544 | | [27] | Ono K, Arakawa K, Hojou K.Formation and migration of helium bubbles in Fe and Fe-9Cr ferritic alloy [J].J. Nucl. Mater., 2002, 307-311: 1507 | | [28] | Yang L, Zu X T, Gao F, et al.Dynamic interactions of helium-vacancy clusters with edge dislocations in α-Fe[J]. Physica, 2010, 405B: 1754 | | [29] | Yang L, Zhu Z Q, Peng S M, et al.Effects of temperature on the interactions of helium-vacancy clusters with gliding edge dislocations in α-Fe[J]. J. Nucl. Mater., 2013, 441: 6 | | [30] | Plimpton S.Fast parallel algorithms for short-range molecular dynamics[J]. J. Comput. Phys., 1995, 117: 1 | | [31] | Stukowski A.Visualization and analysis of atomistic simulation data with OVITO—The Open Visualization Tool[J]. Modell. Simul. Mater. Sci. Eng., 2009, 18: 015012 | | [32] | Stukowski A, Albe K.Dislocation detection algorithm for atomistic simulations[J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 025016 | | [33] | Yang L, Deng H Q, Gao F, et al.Atomistic studies of nucleation of He clusters and bubbles in bcc iron[J]. Nucl. Instrum. Methods Phys. Res., 2013, 303B: 68 | | [34] | Prokhodtseva A, Décamps B, Sch?ublin R.Comparison between bulk and thin foil ion irradiation of ultra high purity Fe[J]. J. Nucl. Mater., 2013, 442(Suppl.1-3): S786 | | [35] | Heinisch H L, Gao F, Kurtz R J, et al.Interaction of helium atoms with edge dislocations in α-Fe[J]. J. Nucl. Mater., 2006, 351: 141 | | [36] | Wirth B D, Odette G R, Maroudas D, et al.Dislocation loop structure, energy and mobility of self-interstitial atom clusters in bcc iron[J]. J. Nucl. Mater., 2000, 276: 33 | | [37] | Marian J, Wirth B D, Perlado J M.Mechanism of formation and growth of <100> interstitial loops in ferritic materials[J]. Phys. Rev. Lett., 2002, 88: 255507 | | [38] | Wang J, Yu L M, Huang Y, et al.Micromechanics mechanism of α-Fe with different types of edge dislocations under radiation damage[J]. Mater. Lett., 2018, 210: 325 | | [39] | Ding M S, Du J P, Wan L, et al.Radiation-induced helium nanobubbles enhance ductility in submicron-sized single-crystalline copper[J]. Nano Lett., 2016, 16: 4118 | | [40] | Hale L M, Zimmerman J A, Wong B M.Large-scale atomistic simulations of helium-3 bubble growth in complex palladium alloys[J]. J. Chem. Phys., 2016, 144: 194705 | | [41] | Carrington W, Hale K F, McLean D. Arrangement of dislocations in iron[J]. Proc. Roy. Soc., 1960, 259A: 203 | | [42] | Ohr S M, Beshers D N.Crystallography of dislocation networks in annealed iron[J]. Philos. Mag., 1963, 8A: 1343 |
|
|