| W对新型Nb稳定化奥氏体耐热铸钢1000 ℃蠕变行为的影响 |
| 张银辉, 冯强 |
| 北京科技大学新金属材料国家重点实验室 北京 100083 |
|
| Effects of W on Creep Behaviors of Novel Nb-Bearing Austenitic Heat-Resistant Cast Steels at 1000 ℃ |
| Yinhui ZHANG, Qiang FENG |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
张银辉, 冯强. W对新型Nb稳定化奥氏体耐热铸钢1000 ℃蠕变行为的影响[J]. 金属学报, 2017, 53(9): 1025-1037.
Yinhui ZHANG,
Qiang FENG.
Effects of W on Creep Behaviors of Novel Nb-Bearing Austenitic Heat-Resistant Cast Steels at 1000 ℃[J]. Acta Metall Sin, 2017, 53(9): 1025-1037.
| [1] | Matsumoto K, Tojo M, Jinnai Y, et al.Development of compact and high performance turbocharger for 1050 ℃ exhaust gas[J]. Mitsubishi Heavy Ind. Tech. Rev., 2008, 45(3): 1 | | [2] | Kunanoppadon J.Thermal efficiency of a combined turbocharger set with gasoline engine[J]. Am. J. Engg. Applied Sci., 2010, 3: 342 | | [3] | Ebisu M, Terakawa Y, Ibaraki S.Mitsubishi turbocharger for lower pollution cars[J]. Mitsubishi Heavy Ind. Tech. Rev., 2004, 41(1): 40 | | [4] | An B, Shiraishi T.Development of variable two-stage turbocharger for passenger car diesel engines[J]. Mitsubishi Heavy Ind. Tech. Rev., 2010, 47(4): 7 | | [5] | Itoh K, Hayashi K, Souda T.Development of HERCUNITE?-S NSHR?-A5N for high performance gasoline engines[J]. Hitachi Metals Tech. Rev., 2006, 22: 51 | | [6] | Shingledecker J P, Maziasz P J, Evans N D, et al.Creep behavior of a new cast austenitic alloy[J]. Int. J. Pres. Ves. Pip., 2007, 84: 21 | | [7] | Takabayashi H, Ueta S, Shimizu T, et al.Development of thermal fatigue resistant ferritic cast steel for turbine housing of diesel engine automobile[J]. SAE Int. J. Mater. Manuf., 2009, 2: 147 | | [8] | Perron A, Toffolon-Masclet C, Ledoux X, et al.Understanding sigma-phase precipitation in a stabilized austenitic stainless steel (316Nb) through complementary CALPHAD-based and experimental investigations[J]. Acta Mater., 2014, 79: 16 | | [9] | Erneman J, Schwind M, Liu P, et al.Precipitation reactions caused by nitrogen uptake during service at high temperatures of a niobium stabilised austenitic stainless steel[J]. Acta Mater., 2004, 52: 4337 | | [10] | Erneman J, Schwind M, Andrén H O, et al.The evolution of primary and secondary niobium carbonitrides in AISI 347 stainless steel during manufacturing and long-term ageing[J]. Acta Mater., 2006, 54: 67 | | [11] | Yamamoto Y, Brady M P, Santella M L, et al.Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels[J]. Metall. Mater. Trans., 2011, 42A: 922 | | [12] | Pickering F B.Physical Metallurgy and the Design of Steels[M]. London: Applied Science Publishers Ltd, 1978: 12 | | [13] | Medvedeva N I, Van Aken D C, Medvedeva J E. Stability of binary and ternary M23C6 carbides from first principles[J]. Comp. Mater. Sci., 2015, 96: 159 | | [14] | Yamamoto Y, Santella M L, Brady M P, et al.Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels[J]. Metall. Mater. Trans., 2009, 40A: 1868 | | [15] | Jung S, Sohn S S, Jo Y H, et al.Effects of Cr and Nb addition on high-temperature tensile properties in austenitic cast steels used for turbo-charger application[J]. Mater. Sci. Eng., 2016, A677: 316 | | [16] | Jung S, Jeon C, Jo Y H, et al.Effects of tungsten and molybdenum on high-temperature tensile properties of five heat-resistant austenitic stainless steels[J]. Mater. Sci. Eng., 2016, A656: 190 | | [17] | Kim Y J, Lee D G, Jeong H K, et al.High temperature mechanical properties of HK40-type heat-resistant cast austenitic stainless steels[J]. J. Mater. Eng. Perform., 2010, 19: 700 | | [18] | Taneike M, Abe F, Sawada K.Creep-strengthening of steel at high temperatures using nano-sized carbonitride dispersions[J]. Nature, 2003, 424: 294 | | [19] | Sherby O D, Burke P M.Mechanical behavior of crystalline solids at elevated temperature[J]. Prog. Mater. Sci., 1968, 13: 323 | | [20] | Rieth M, Falkenstein A, Graf P, et al.Creep of the austenitic steel AISI 316 L(N): Experiments and models [R]. Wissenschaftliche Berichte FZKA 7065, 2004: 1 | | [21] | Zhang Y H, Li M, Godlewski L A, et al.Effects of N/C ratio on solidification behaviors of novel Nb-bearing austenitic heat-resistant cast steels for exhaust components of gasoline engines[J]. Metall. Mater. Trans., 2017, 48A: 1151 | | [22] | Buchanan K, Kral M.Crystallography and morphology of niobium carbide in as-cast HP-niobium reformer tubes[J]. Metall. Mater. Trans., 2012, 43A: 1760 | | [23] | Qiao G W, Wang D H, Cao Z B.An EM study of carbide precipitates in HK40 refractory steel[J]. Acta Metall. Sin., 1986, 22: 67(乔桂文, 王德和, 曹智本. HK40耐热钢碳化物析出的电镜研究[J]. 金属学报, 1986, 22: 67) | | [24] | Ozbayraktar S, Koursaris A.Effect of superheat on the solidification structures of AISI 310S austenitic stainless steel[J]. Metall. Mater. Trans., 1996, 27B: 287 | | [25] | Zhang Y H, Li M, Godlewski L A, et al.Effective design of new austenitic cast steels for ultra-high temperature automotive exhaust components through combined CALPHAD and experimental approaches[J]. Mater. Sci. Eng., 2017, A683: 195 | | [26] | Zhang Y H, Li M, Godlewski L A, et al.Effects of N on creep properties of austeni-tic heat-resistant cast steels developed for exhaust component applications at 1000 ℃[J]. Acta Metall. Sin., 2016, 52: 661(张银辉, Li M, Godlewski L A等. N对汽车发动机用新型奥氏体耐热铸钢1000 ℃蠕变性能的影响[J]. 金属学报, 2016, 52: 661) | | [27] | Lo K H, Shek C H, Lai J K L. Recent developments in stainless steels[J]. Mater. Sci. Eng., 2009, R65: 39 | | [28] | Ribeiro E A A G, Papaléo R, Guimar?es J R C. Microstructure and creep behavior of a niobium alloyed cast heat-resistant 26 pct Cr steel[J]. Metall. Trans., 1986, 17A: 691 | | [29] | Zhang Y H, Li M, Godlewski L A, et al.Creep behavior at 1273 K (1000 ℃) in Nb-bearing austenitic heat-resistant cast steels developed for exhaust component applications[J]. Metall. Mater. Trans., 2016, 47A: 3289 | | [30] | Zhang J S.High Temperature Deformation and Fracture of Materials [M]. Beijing: Science Press, 2007: 3(张俊善. 材料的高温变形与断裂 [M]. 北京: 科学出版社, 2007: 3) | | [31] | Michalska J, Sozańska M.Qualitative and quantitative analysis of σ and χ phases in 2205 duplex stainless steel[J]. Mater. Charact., 2006, 56: 355 |
|
|