| 电渣重熔全过程的数学模型开发及过程模拟研究 |
李青( ),王资兴,谢树元 |
| 宝山钢铁股份有限公司研究院 上海 201900 |
|
| Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation |
Qing LI( ),Zixing WANG,Shuyuan XIE |
| Research Institute, Baoshan Iron & Steel Co., Ltd., Shanghai 201900, China |
引用本文:
李青,王资兴,谢树元. 电渣重熔全过程的数学模型开发及过程模拟研究[J]. 金属学报, 2017, 53(4): 494-504.
Qing LI,
Zixing WANG,
Shuyuan XIE.
Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. Acta Metall Sin, 2017, 53(4): 494-504.
| [1] | Hernandez-Morales B, Mitchell A.Review of mathematical models of fluid flow, heat transfer, and mass transfer in electroslag remel-ting process[J]. Ironmak. Steelmak., 1999, 26: 423 | | [2] | Kelkar K M, Patankar S V, Mitchell A.Computational modeling of the electroslag remelting (ESR) process used for the production of ingots of high-performance alloys [A]. Proceedings of the 2005 International Symposium on Liquid Metal Processing and Casting[C]. Materials Park, OH, USA: Wiley-TMS, 2005: 137 | | [3] | Rückert A, Pfeifer H.Numerical modelling of the electroslag remelting process[J]. METAL 2007-Hradec nad Moravici, 2007, 5: 22 | | [4] | Mackenbrock A, Maronnier V, K?ser O, et al.Numerical simulation of the protective gas electroslag remelting process and its industrial validation[J]. BHM Berg- und Hüttenm?nnische Monatshefte, 2007, 152: 345 | | [5] | Weber V, Jardy A, Dussoubs B, et al.A comprehensive model of the electroslag remelting process: Description and validation[J]. Metall. Mater. Trans., 2009, 40B: 271 | | [6] | Wei J H, Ren Y L.Mathematical simulation of magnetic field in ESR system[J]. Acta Metall. Sin., 1995, 31: 51 | | [6] | (魏季和, 任永莉. 电渣重熔体系内磁场的数学模拟[J]. 金属学报, 1995, 31: 51) | | [7] | Geng M P, Sun D X.Process Control and Simulation in Electroslag Casting [M]. Beijing: Metallurgical Industry Press, 2008: 21 | | [7] | (耿茂鹏, 孙达昕. 电渣熔铸过程控制与模拟仿真 [M]. 北京: 冶金工业出版社, 2008: 21) | | [8] | Li B K, Wang B, Tsukihashi F.Modeling of electromagnetic field and liquid metal pool shape in an electroslag remelting process with two series-connected electrodes[J]. Metall. Mater. Trans., 2014, 45B: 1122 | | [9] | Wang Q, He Z, Li B K, et al.A general coupled mathematical model of electromagnetic phenomena, two-phase flow, and heat transfer in electroslag remelting process including conducting in the mold[J]. Metall. Mater. Trans., 2014, 45B: 2425 | | [10] | Kharicha A, Mackenbrock A, Ludwig A, et al.Selected numerical investigations on ESR process [A]. Proceedings of the 2007 International Symposium on Liquid Metal Processing and Casting[C]. Nancy, France: Wiley-TMS, 2007: 107 | | [11] | Fezi K, Yanke J, Krane M J M. Macrosegregation during electroslag remelting of alloy 625[J]. Metall. Mater. Trans., 2015, 46B: 766 | | [12] | Wei J H, Ren Y L.Mathematical modelling of slag flow field in ESR system[J]. Acta Metall. Sin., 1994, 30: 481 | | [12] | (魏季和, 任永莉. 电渣重熔体系内熔渣流场的数学模拟[J]. 金属学报, 1994, 30: 481) | | [13] | Liu F B, Chen X, Jiang Z H, et al.Mathematical modeling of electroslag remelting process[J]. J. Northeast. Univ.(Nat. Sci.), 2014, 35: 539 | | [13] | (刘福斌, 陈旭, 姜周华等. 电渣重熔过程的数值模拟[J]. 东北大学学报(自然科学版), 2014, 35: 539) | | [14] | Chang L Z, Li Z B.Dynamic simulation on temperature field of slab ingot during electroslag remelting[J]. Spec. Steel, 2007, 28(5): 34 | | [14] | (常立忠, 李正邦. 电渣重熔板锭过程中温度场的动态模拟[J]. 特殊钢, 2007, 28(5): 34) | | [15] | Bai H J, Li Y, Li B K.Effect of electromagnetic stirring on temperature field of ESR ingot[J]. Spec. Steel, 2008, 29(1): 7 | | [15] | (白海军, 厉英, 李宝宽. 电磁搅拌对电渣重熔钢锭温度场的影响[J]. 特殊钢, 2008, 29(1): 7) | | [16] | Wei J H, Mitchell A.Changes in composition during A. C. ESR—I. Theoretical development[J]. Acta Metall. Sin., 1984, 20: B261 | | [16] | (魏季和, Mitchell A.交流电渣重熔过程中的成分变化——I.理论传质模型[J]. 金属学报, 1984, 20: B261) | | [17] | Nastac L, Sundarraj S, Yu K O, et al.The stochastic modeling of solidification structures in alloy 718 remelt ingots[J]. JOM, 1998, 50(3): 30 | | [18] | Li B K, Wang Q, Wang F, et al.A coupled cellular automaton-finite-element mathematical model for the multiscale phenomena of electroslag remelting H13 die steel ingot[J]. JOM, 2014, 66: 1153 | | [19] | Bertram L A, Williamson R L, Melgaard D K, et al.Dynamic control of remelting processes [P]. US Pat., 6115404, 2000 | | [20] | Xie D X, Yao Y Y, Bai B D, et al.The Finite Element Analysis of Three-dimensional Eddy Current Field [M]. Beijing: China Machine Press, 2001: 12 | | [20] | (谢德馨, 姚缨英, 白保东等. 三维涡流场的有限元分析 [M]. 北京: 机械工业出版社, 2001: 12) | | [21] | Tao W Q.Numerical Heat Transfer [M]. 2nd Ed., Xi'an: Xi'an Jiaotong University Press, 2001: 242, 273, 347, 351, 353 | | [21] | (陶文铨. 数值传热学 [M]. 第2版. 西安: 西安交通大学出版社, 2001: 242, 273, 347, 351, 353) | | [22] | Bai Y F.Coupled modeling and numerical calculation for transport phenomena in electromagnetic directional solidification of titanium alloy in cold crucible [D]. Harbin: Harbin Institute of Technology, 2006 | | [22] | (白云峰. 钛合金冷坩埚电磁定向凝固传输过程耦合模型与数值计算 [D]. 哈尔滨: 哈尔滨工业大学, 2006) | | [23] | Sun D L, Qu Z G, He Y L, et al.Inner doubly-iteration efficient algorithm for linked-equations based on three-dimensional non-staggered grid[J]. Chin. Sci. Bull., 2008, 53: 3014 | | [23] | (孙东亮, 屈治国, 何雅玲等. 基于三维同位网格的高效稳定的分离式算法IDEAL[J]. 科学通报, 2008, 53: 3014) | | [24] | Wang F J.Computational Fluid Dynamics Analysis——Principle and Application of CFD Software [M]. Beijing: Tsinghua University Press, 2004: 11, 50 | | [24] | (王福军. 计算流体动力学分析——CFD软件原理与应用 [M]. 北京: 清华大学出版社, 2004: 11, 50) | | [25] | Auburtin P, Wang T, Cockcroft S L, et al.Freckle formation and freckle criterion in superalloy castings[J]. Metall. Mater. Trans., 2000, 31B: 801 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|