| 铝合金薄板高转速搅拌摩擦焊接头组织与力学性能 |
刘奋军1,2, 傅莉1,3,4( ), 陈海燕1,3,4 |
1 西北工业大学材料学院 西安 710072 2 榆林学院能源工程学院 榆林 719000 3 西北工业大学凝固技术国家重点实验室 西安 710072 4 西北工业大学陕西省摩擦焊接工程技术重点实验室 西安 710072 |
|
| Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding |
Fenjun LIU1,2, Li FU1,3,4( ), Haiyan CHEN1,3,4 |
1 School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China 2 College of Energy Engineering, Yulin University, Yulin 719000, China 3 State Key Laboratory of Solidification, Northwestern Polytechnical University, Xi'an 710072, China 4 Shaanxi Key Laboratory of Friction Welding Technologies, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
刘奋军, 傅莉, 陈海燕. 铝合金薄板高转速搅拌摩擦焊接头组织与力学性能[J]. 金属学报, 2017, 53(12): 1651-1658.
Fenjun LIU,
Li FU,
Haiyan CHEN.
Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding[J]. Acta Metall Sin, 2017, 53(12): 1651-1658.
| [1] | Rhodes C G, Mahoney M W, Bingel W H, et al.Effects of friction stir welding on microstructure of 7075 aluminum[J]. Scr. Mater., 1997, 36: 69 | | [2] | Da Silvada A A M, Arruti E, Janeiro G, et al. Material flow and mechanical behaviour of dissimilar AA2024-T3 and AA7075-T6 aluminium alloys friction stir welds[J]. Mater. Des., 2011, 32: 2021 | | [3] | Mishra R S, Ma Z Y.Friction stir welding and processing[J]. Mater. Sci. Eng., 2005, R50: 1 | | [4] | Threadgill P L, Leonard A J, Shercliff H R, et al.Friction stir welding of aluminium alloys[J]. Int. Mater. Rev., 2009, 54: 49 | | [5] | Nandan R, DebRoy T, Bhadeshia H K D H. Recent advances in friction stir welding—Process, weldment structure and properties[J]. Prog. Mater. Sci., 2008, 53: 980 | | [6] | Wang T, Zou Y, Matsuda K.Micro-structure and micro-textural studies of friction stir welded AA6061-T6 subjected to different rotation speeds[J]. Mater. Des., 2016, 90: 13 | | [7] | Liu F C, Ma Z Y.Influence of tool dimension and welding parameters on microstructure and mechanical properties of friction stir welded 6061-T651 aluminum alloy[J]. Metall. Mater. Trans., 2008, 39A: 2378 | | [8] | Guo J F, Chen H C, Sun C N, et al.Friction stir welding of dissimilar materials between AA6061 and AA7075 Al alloys effects of process parameters[J]. Mater. Des., 2014, 56: 185 | | [9] | Liu H J, Hou J C, Guo H.Effect of welding speed on microstructure and mechanical properties of self-reacting friction stir welded 6061-T6 aluminum alloy[J]. Mater. Des., 2013, 50: 872 | | [10] | He C, Liu Y J, Dong J F, et al.Through thickness property variations in friction stir welded AA6061 joint fatigued in very high cycle fatigue regime[J]. Int. J. Fatigue, 2016, 82: 379 | | [11] | Rodrigues D M, Loureiro A, Leitao C, et al.Influence of friction stir welding parameters on the microstructural and mechanical properties of AA 6016-T4 thin welds[J]. Mater. Des., 2009, 30: 1913 | | [12] | Galvao I, Leitao C, Loureiro A, et al.Friction stir welding of very thin plates[J]. Soldag. Insp. Sao. Paulo., 2012, 17: 2 | | [13] | Leal R M, Leit?o C, Loureiro A, et al.Material flow in heterogeneous friction stir welding of thin aluminium sheets: Effect of shoulder geometry[J]. Mater. Sci. Eng., 2008, A498: 384 | | [14] | Scialpi A, De Filippis L A C, Cavaliere P. Influence of shoulder geometry on microstructure and mechanical properties of friction stir welded 6082 aluminium alloy[J]. Mater. Des., 2007, 28: 1124 | | [15] | De Giorgi M, Scialpi A, Panella F W, et al.Effect of shoulder geometry on residual stress and fatigue properties of AA6082 FSW joints[J]. J. Mech. Sci. Technol., 2009, 23: 26 | | [16] | Scialpi A, De Giorgi M, De Filippis L A C, et al. Mechanical analysis of ultra-thin friction stir welding joined sheets with dissimilar and similar materials[J]. Mater. Des., 2008, 29: 928 | | [17] | Murr L E, Liu G, McClure J C. A TEM study of precipitation and related microstructures in friction-stir-welded 6061 aluminium[J]. J. Mater. Sci., 1998, 33: 1243 | | [18] | Zhao H H, Feng X S, Xiong Y Y, et al.Microstructure and properties of micro friction stir welded joint of Al-alloy ultra thin plate with zero tilt angle[J]. Trans. China Weld. Inst., 2014, 35(7): 47(赵慧慧, 封小松, 熊艳艳等. 铝合金超薄板无倾角微搅拌摩擦焊接头组织性能[J]. 焊接学报, 2014, 35(7): 47) | | [19] | Schmidt H, Hattel J, Wert J.An analytical model for the heat generation in friction stir welding[J]. Model. Simul. Mater. Sci. Eng., 2004, 12: 143 | | [20] | Schmidt H B, Hattel J H.Thermal modelling of friction stir welding[J]. Scr. Mater., 2008, 58: 332 | | [21] | Chen H Y, Fu Li, Liang P.Microstructure, texture and mechanical properties of friction stir welded butt joints of 2A97 Al-Li alloy ultra-thin sheets[J]. J. Alloys Compd., 2017, 692: 155 | | [22] | Malopheyev S, Vysotskiy I, Kulitskity V, et al.Optimization of processing-microstructure-properties relationship in friction-stir welded 6061-T6 aluminum alloy[J]. Mater. Sci. Eng., 2016, A662: 136 | | [23] | Liu F J, Fu L, Zhang W Y, et al.Interface structure and mechanical pro-perties of friction stir welding joint of 2099-T83/2060-T8 dissimilar Al-Li alloys[J]. Acta Metall. Sin., 2015, 51: 281(刘奋军, 傅莉, 张纹源等. 2099-T83/2060-T8异质Al-Li合金搅拌摩擦焊搭接界面结构与力学性能[J]. 金属学报, 2015, 51: 281) | | [24] | Sato Y S, Kokawa H, Enomoto M, et al.Microstructural evolution of 6063 aluminum during friction-stir welding[J]. Metall. Mater. Trans., 1999, 30A: 2429 | | [25] | Sato Y S, Urata M, Kokawa H, et al.Hall-Petch relationship in friction stir welds of equal channel angular-pressed aluminium alloys[J]. Mater. Sci. Eng., 2003, A354: 298 | | [26] | Sattari S, Bisadi H, Sajed M.Mechanical properties and temperature distributions of thin friction stir welded sheets of AA5083[J]. Int. J. Mech. Appl., 2012, 2: 1 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|