| 医用纯Mg表面多种复合处理膜层的组织结构和体内外性能 |
李慕勤( ), 姚海涛, 魏方红, 刘明达, 王赞, 彭书浩 |
| 佳木斯大学黑龙江省高校生物医学材料重点实验室 佳木斯 154007 |
|
| The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface |
Muqin LI( ), Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG |
| Key Laboratory of Biomaterials of Heilongjiang Province, Jiamusi University, Jiamusi 154007, China |
引用本文:
李慕勤, 姚海涛, 魏方红, 刘明达, 王赞, 彭书浩. 医用纯Mg表面多种复合处理膜层的组织结构和体内外性能[J]. 金属学报, 2017, 53(10): 1337-1346.
Muqin LI,
Haitao YAO,
Fanghong WEI,
Mingda LIU,
Zan WANG,
Shuhao PENG.
The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. Acta Metall Sin, 2017, 53(10): 1337-1346.
| [1] | Vormann J.Magnesium: Nutrition and metabolism[J]. Mol. Aspects Med., 2003, 24: 27 | | [2] | Witte F.The history of biodegradable magnesium implants: A review[J]. Acta Biomater., 2010, 6: 1680 | | [3] | Narayan R J.The next generation of biomaterial development[J]. Philos. Trans. Roy. Soc., 2010, 368A: 1831 | | [4] | Hench L L, Polak J M.Third-generation biomedical materials[J]. Science, 2002, 295: 1014 | | [5] | Chen Y J, Xu Z G, Smith C, et al.Recent advances on the development of magnesium alloys for biodegradable implants[J]. Acta Biomater., 2014, 10: 4561 | | [6] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 | | [7] | Han X G, Zhu X P, Lei M K.Electrochemical properties of microarc oxidation films on a magnesium alloy modified by high-intensity pulsed ion beam[J]. Surf. Coat. Technol., 2011, 206: 874 | | [8] | Pan Y K, Chen C Z, Wang D G, et al.Influence of additives on microstructure and property of microarc oxidized Mg-Si-O coatings[J]. Ceram. Int., 2012, 38: 5527 | | [9] | Qu L J, Li M Q, Zhang E L, et al.Corrosion resistance of magnesium alloy coated by ultrasonic-micro arc oxidation in simulated body fluid[J]. Trans. Mater. Heat Treat., 2013, 34(3): 130(曲立杰, 李慕勤, 张二林等. 超声微弧氧化处理镁合金模拟体液中的耐蚀性[J]. 材料热处理学报, 2013, 34(3): 130) | | [10] | Xu Y D, Chen Y B, Shi M, et al.Surface treatment application of silane on metals[J]. Met. Funct. Mater., 2011, 18(5): 66(许育东, 陈云帮, 石敏等. 金属表面硅烷化处理应用的研究[J]. 金属功能材料, 2011, 18(5): 66) | | [11] | Palanivel V, Zhu D Q, van Ooij W J. Nanoparticle-filled silane films as chromate replacements for aluminum alloys[J]. Prog. Org. Coat., 2003, 47: 384 | | [12] | Hu J M, Liu L, Zhang J T, et al.Studies of surface treatment of aluminum alloys by BTSE silane agent[J]. Acta Metall. Sin., 2004, 40: 1189(胡吉明, 刘倞, 张金涛等. 铝合金表面BTSE硅烷化处理研究[J]. 金属学报, 2004, 40: 1189) | | [13] | Zucchi F, Grassi V, Frignani A, et al.Influence of a silane treatment on the corrosion resistance of a WE43 magnesium alloy[J]. Surf. Coat. Technol., 2006, 200: 4136 | | [14] | Zhang W, Sun Z F, Ding T, et al.Effect of silane treatment on corrosion resistance of AZ31 magnesium alloys[J]. J. Chongqing Inst. Technol.(Nat. Sci.), 2009, 23(9): 128(张微, 孙智富, 丁婷等. 硅烷处理对AZ31镁合金耐蚀性的影响[J]. 重庆工学院学报(自然科学版), 2009, 23(9): 128) | | [15] | Zhou C Z, Confalonieri F, Medina N, et al.Fine organization of Bombyx mori fibroin heavy chain gene[J]. Nucleic Acids Res., 2000, 28: 2413 | | [16] | Tanaka K, Kajiyama N, Ishikura K, et al.Determination of the site of disulfide linkage between heavy and light chains of silk fibroin produced by Bombyx mori[J]. Biochim. Biophys. Acta, 1999, 1432: 92 | | [17] | Mirahmadi F, Tafazzoli-Shadpour M, Shokrgozar M A, et al.Enhanced mechanical properties of thermo sensitive chitosan hydrogel by silk fibers for cartilage tissue engineering[J]. Mater. Sci. Eng., 2013, C33: 4786 | | [18] | Zhu H L, Wu B W, Feng X X, et al.Preparation and characterization of bioactive mesoporous calcium silicate-silk fibroin composite films[J]. J. Biomed. Mater. Res., 2011, 98B: 330 | | [19] | Wang X Y, Kim H J, Xu P, et al.Biomaterial coatings by stepwise deposition of silk fibroin[J]. Langmuir, 2005, 21: 11335 | | [20] | Li M Q, Liu J, Ma C.Preparation method of magnesium surface ultrasonic micro-arc oxidation-HF-silane coupling agent multistage compound bioactive coating [P]. Chin Pat, 201310537474.5, 2014(李慕勤, 刘江, 马臣. 镁表面超声微弧氧化-HF-硅烷偶联剂多级复合生物活性涂层制备方法 [P]. 中国专利, 201310537474.5, 2014) | | [21] | Li M Q, Ma C, Zhang A Q.Preparation method of ultrasonic microarc oxidation silver-carrying antibiotic bioactive coating on magnesium and titanium surface [P]. Chin Pat, 200910072105.7, 2010(李慕勤, 马臣, 张爱琴. 镁、钛表面超声微弧氧化载银抗菌生物活性涂层制备方法 [P]. 中国专利, 2009100721057.7, 2010) | | [22] | Gao J C, Li L C, Wang Y, et al.Corrosion resistance of alkali heat treated magnesium in bionics simulated body fluid[J]. Trans. Mater. Heat Treat., 2005, 30(4): 38(高家诚, 李龙川, 王勇等. 碱热处理镁及其在仿生模拟体液中耐蚀性能[J]. 金属热处理, 2005, 30(4): 38) | | [23] | Correa P S, Malfatti C F, Azambuja D S.Corrosion behavior study of AZ91 magnesium alloy coated with methyltriethoxy silane doped with cerium ions[J]. Prog. Org. Coat., 2011, 72: 739 | | [24] | Wu H J, Lu J T.Characterization and formation of silane film on hot-dipped galvanized steel sheet[J]. Mater. Prot., 2009, 42(5): 7(吴海江, 卢锦堂. 热镀锌钢表面硅烷膜的制备、表征及成膜机理[J]. 材料保护, 2009, 42(5): 7) | | [25] | Fang X X, Cao Y B, Liang W, et al.Conventional treatment technology and silanization technology for the surface of magnesium alloy[J]. J. Chongqing Inst. Technol.(Nat. Sci.), 2010, 12(2): 123(方欣欣, 曹岳斌, 梁伟等. 镁合金表面常规处理与硅烷化处理技术[J]. 重庆科技学院学报(自然科学版), 2010, 12(2): 123) | | [26] | Shi P J, Goh J C H. Self-assembled silk fibroin particles: Tunable size and appearance [J]. Powder Technol., 2012, 215-216: 85 | | [27] | Cheng C, Shao Z Z, Vollrath F.Silk fibroin-regulated crystallization of calcium carbonate[J]. Adv. Funct. Mater., 2008, 18: 2172 | | [28] | Hu D D, Yang M Y, Zhu L J.Influence of silk fibroin-based biomaterials on cell behaviors[J]. Bull. Seric., 2016, 47(1): 6(胡豆豆, 杨明英, 朱良均. 丝素蛋白生物材料对细胞行为的影响[J]. 蚕桑通报, 2016, 47(1): 6) | | [29] | Marolt D, Augst A, Freed L E, et al.Bone and cartilage tissue constructs grown using human bone marrow stromal cells, silk scaffolds and rotating bioreactors[J]. Biomaterials, 2006, 27: 6138 | | [30] | Yang Y M, Ding F, Wu J, et al.Development and evaluation of silk fibroin-based nerve grafts used for peripheral nerve regeneration[J]. Biomaterials, 2007, 28: 5526 | | [31] | Hein J, Hartmann K.Reference ranges for laboratory parameters in rabbits[J]. Tier?rztl. Praxis Kleint., 2003, (5): 321 | | [32] | Yang L, Chen Y, Zhu L J, et al.In vivo degradation test of a novel silk fibroin scaffold[J]. Bull. Seric., 2011, 37: 713(杨磊, 陈宇, 朱良均等. 一种新型丝素支架材料的体内降解试验[J]. 蚕桑通报, 2011, 37: 713) |
|
|