| 电磁连铸对Incoloy800H合金铸坯内TiN分布和内裂纹的影响 |
王菲,王恩刚( ),贾鹏,王韬,邓安元 |
| 东北大学材料电磁过程研究教育部重点实验室 沈阳 110819 |
|
| Effect of Electromagnetic Continuous Casting on TiN Distribution and Internal Crack of Incoloy800H Alloy Billet |
Fei WANG,Engang WANG( ),Peng JIA,Tao WANG,Anyuan DENG |
| Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China |
引用本文:
王菲,王恩刚,贾鹏,王韬,邓安元. 电磁连铸对Incoloy800H合金铸坯内TiN分布和内裂纹的影响[J]. 金属学报, 2017, 53(1): 97-106.
Fei WANG,
Engang WANG,
Peng JIA,
Tao WANG,
Anyuan DENG.
Effect of Electromagnetic Continuous Casting on TiN Distribution and Internal Crack of Incoloy800H Alloy Billet[J]. Acta Metall Sin, 2017, 53(1): 97-106.
| [1] | Chen W S, Kai W, Tsay L W, et al.The oxidation behavior of three different zones of welded Incoloy 800H alloy[J]. Nucl. Eng. Des., 2014, 272: 92 | | [2] | Tan L, Allen T R, Yang Y.Corrosion behavior of alloy 800H (Fe-21Cr-32Ni) in supercritical water[J]. Corros. Sci., 2011, 53: 703 | | [3] | Kim D J, Seo D Y, Tsang J, et al.The crack growth behavior of Incoloy 800H under fatigue and dwell-fatigue conditions at elevated temperature[J]. J. Mech. Sci. Technol., 2012, 26: 2023 | | [4] | Kanbe Y, Ishii T, Todoroki H, et al.Prevention of longitudinal cracks in a continuously cast slab of Fe-Cr-Ni superalloy containing Al and Ti[J]. Int. J. Cast Met. Res., 2009, 22: 143 | | [5] | Ma J, Zheng H G, Huang J, et al.An analysis on forming mechanism of longitudinal crack of N08810 corrosion resistant alloy 200 mm thickness casting slab[J]. Spec. Steel, 2012, 33(3): 61 | | [5] | (马骏, 郑宏光, 黄坚等. N08810耐蚀合金200mm厚连铸板坯纵向裂纹形成机理的分析[J]. 特殊钢, 2012, 33(3): 61) | | [6] | Todoroki H, Ishii T, Mizuno K, et al. Effect of crystallization behavior of mold flux on slab surface quality of a Ti-bearing Fe-Cr-Ni super alloy cast by means of continuous casting process [J]. Mater. Sci. Eng., 2005, A413-414: 121 | | [7] | Zeng Y P, Fan H M, Wang X S, et al. Study on micro-mechanism of crack initiation and propagation induced by inclusion in ultra-high strength steel [J]. Key Eng. Mater., 2007, 353-358: 1185 | | [8] | Du J, Strangwood M, Davis C L.Effect of TiN particles and grain size on the charpy impact transition temperature in steels[J]. J. Mater. Sci. Technol., 2012, 28: 878 | | [9] | Li X H, Huang F, Wang J Q, et al.Influences of TiN inclusion on corrosion and stress corrosion behaviors of alloy 690 tube in high temperature and high pressure water[J]. Acta Metall. Sin., 2011, 47: 847 | | [9] | (郦晓慧, 黄发, 王俭秋等. TiN夹杂物对690合金管在高温高压水中的腐蚀和应力腐蚀行为的影响[J]. 金属学报, 2011, 47: 847) | | [10] | Tan J B, Wu X Q, Han E H, et al.Role of TiN inclusion on corrosion fatigue behavior of alloy 690 steam generator tubes in borated and lithiated high temperature water[J]. Corros. Sci., 2014, 88: 349 | | [11] | Yan Z M, Jin W Z, Li T J.Effect of rotating magnetic field (RMF) on segregation of solute elements in CuNi10Fe1Mn alloy hollow billet[J]. J. Mater. Eng. Perform., 2012, 21: 1970 | | [12] | Liu Z, Liu X M, Zhu T, et al.Effects of electromagnetic stirring with low current frequency on Re distribution in semisolid aluminum alloy[J]. Acta Metall. Sin., 2015, 51: 272 | | [12] | (刘政, 刘小梅, 朱涛等. 低频电磁搅拌对半固态铝合金中稀土分布的影响[J]. 金属学报, 2015, 51: 272) | | [13] | Zhang Q, Chen D, Sun G X, et al.Restraining effects on central defects of 1560 nickel-based alloy ingot by electromagnetic horizontal continuous casting[J]. Foundry, 2013, 62: 384 | | [13] | (张勤, 陈定, 孙光曦等. 电磁水平连铸对1560镍基合金铸坯中心缺陷的抑制作用[J]. 铸造, 2013, 62: 384) | | [14] | Liu Q.Simulation of steel flow heat transfer and stress for Incoloy800 superalloy slab vertical continuous casting process [D]. Shenyang: Northeastern University, 2014 | | [14] | (刘琦. 高温合金立式连铸流动传热和应力的模拟研究 [D]. 沈阳: 东北大学, 2014) | | [15] | Miki Y, Kitaoka H, Sakuraya T, et al.Mechanism for separating inclusions from molten steel stirred with a rotating electro-magnetic field[J]. ISIJ Int., 1992, 32: 142 | | [16] | Fu J, Zhu J, Di L, et al.Study on the precipitation behavior of TiN in the microalloyed steels[J]. Acta Metall. Sin., 2000, 36: 801(傅杰, 朱剑, 迪林等. 微合金钢中TiN的析出规律研究 [J]. 金属学报, 2000, 36: 801) | | [17] | Shi Z X, Dong J X, Zhang M C, et al.Solidification characteristics and hot tearing susceptibility of Ni-based superalloys for turbocharger turbine wheel[J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2737 | | [18] | Campanella T, Charbon C, Rappaz M.Grain refinement induced by electromagnetic stirring: a dendrite fragmentation criterion[J]. Metall. Mater. Trans., 2004, 35A: 3201 | | [19] | Liu L, Zheng H G, Ma T J, et al.Precipitation behavior of titanium nitride in alloy Ni30Cr20[J]. Spec. Steel, 2012, 33(6): 49 | | [19] | (刘亮, 郑宏光, 马天军等. Ni30Cr20合金中氮化钛的析出行为[J]. 特殊钢, 2012, 33(6): 49) | | [20] | Park J H.Effect of inclusions on the solidification structures of ferritic stainless steel: computational and experimental study of inclusion evolution[J]. Calphad, 2011, 35: 455 | | [21] | He Y J, Li Q L, Liu W.Separating effect of a novel combined magnetic field on inclusions in molten aluminum alloy[J]. Metall. Mater. Trans., 2012, 43B: 1149 | | [22] | Wang F, Zhang L T, Deng A Y, et al.Continuous casting of Incoloy800H superalloy billet under an alternating electromagnetic field[J]. Metals, 2016, 6: 2 | | [23] | Cockcroft S L, Degawa T, Mitchell A, et al.Inclusion Precipitation in Superalloys [A]. Superalloys 1992[C]. Champoin, Pennsylvania: TMS, 1992: 557 | | [24] | Jia P, Wang E G, Lu H, et al.Effect of electromagnetic field on microstructure and mechanical property for Inconel 625 superalloy[J]. Acta Metall. Sin., 2013, 49: 1573 | | [24] | (贾鹏, 王恩刚, 鲁辉等. 电磁场对Inconel 625合金凝固组织及力学性能的影响[J]. 金属学报, 2013, 49: 1573) | | [25] | Eskin D G, Suyitno, Katgerman L.Mechanical properties in the semi-solid state and hot tearing of aluminium alloys[J]. Prog. Mater. Sci., 2004, 49: 629 | | [26] | Wang X S, Liang F, Zeng Y P, et al.SEM in situ observations to the effects of inclusions on initiation and propagation of the low cyclic fatigue crack in super strength steel[J]. Acta Metall. Sin., 2005, 41: 1272 | | [26] | (王习术, 梁峰, 曾燕屏等. 夹杂物对超高强度钢低周疲劳裂纹萌生及扩展影响的原位观测[J]. 金属学报, 2005, 41: 1272) | | [27] | Wang C, Zeng Y P, Xie X S.Influence of characteristic inclusion parameters on crack initiation and propagation in ultra-high strength steels for aerospace application under tensile and low cyclic fatigue loading[J]. J. Univ. Sci. Technol. Beijing, 2009, 31: 557 | | [27] | (王冲, 曾燕屏, 谢锡善. 拉伸与低周疲劳载荷作用下夹杂物特征参数对航空用超高强度钢中裂纹萌生与扩展的影响[J]. 北京科技大学学报, 2009, 31: 557) |
|
|