| FB2马氏体耐热钢中Laves相在焊接过程中演化行为的研究* |
李克俭1,蔡志鹏1,2,3( ),李轶非1,潘际銮1 |
1 清华大学机械工程系, 北京 100084 2 清华大学摩擦学国家重点实验室, 北京 100084 3 清华大学先进核能技术协同创新中心, 北京 100084 |
|
| EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING |
Kejian LI1,Zhipeng CAI1,2,3( ),Yifei LI1,Jiluan PAN1 |
1 Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China . 2 State Key Laboratory of Tribology, Tsinghua University, Beijing 100084, China. 3 Collabrative Innovation Center of Advanced Nuclear Energy Technology, Tsinghua University, Beijing 100084, China |
引用本文:
李克俭,蔡志鹏,李轶非,潘际銮. FB2马氏体耐热钢中Laves相在焊接过程中演化行为的研究*[J]. 金属学报, 2016, 52(6): 641-648.
Kejian LI,
Zhipeng CAI,
Yifei LI,
Jiluan PAN.
EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING[J]. Acta Metall Sin, 2016, 52(6): 641-648.
| [1] | Sun R, Cui Z Z, Tao Y.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 1 | | [2] | Di Gianfrancesco A, Tizzanini A, Jedamzik M, Stolzenberger C.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 9 | | [3] | Fukuda M, Saito E, Semba H, Iwasaki J, Izumi S, Takano S, Takahashi T, Sumiyoshi Y.In: Grandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 24 | | [4] | Jara D R.PhD Dissertation, Ruhr University Bochum, 2011 | | [5] | Mayr P.PhD Dissertation, Graz University of Technology, 2007 | | [6] | Di Gianfrancesco A, Budano S, Lombardi P, Paura M, Neri S, Calderini M, Longari N.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 304 | | [7] | Blaes N, Donth B, Bokelmann D.Energy Mater, 2007; 2(4): 207 | | [8] | Azuma T, Miki K, Tanaka Y, Isshiguro T.Tetsu Hagané, 2002; 88: 678 | | [8] | (東司, 三木一宏, 田中泰彦, 石黒徹.鉄と鋼, 2002; 88: 678) | | [9] | Horiuchi T, Igarashi M, Abe F.ISIJ Int, 2002; 42(suppl): S67 | | [10] | Shige T, Magoshi R, Itou S, Ichimura T, Kondou Y.Mitsubishi Heavy Industry Tech Rev, 2001; 38(1): 6 | | [11] | Dzugan J, Novy Z, Konopik P, Podany P.In: Gandy D, Shingledecker J eds., Advances in Materials Technology for Fossil Power Plants Proceedings from the Seventh International Conference, Novelty, Ohio: ASM International, 2014: 924 | | [12] | Xu Y T, Wang M J, Wang Y, Gu T, Chen L, Zhou X, Ma Q, Liu Y M, Huang J.J Alloys Compd, 2015; 621: 93 | | [13] | Dimmler G, Weinert P, Kozeschnik E, Cerjak H.Mater Charact, 2003; 51: 341 | | [14] | Cui H R, Sun F, Chen K, Zhang L T, Wan R C, Shan A D, Wu J S.Mater Sci Eng, 2010; A527: 7505 | | [15] | Korcakova L, Hald J, Somers M.Mater Charact, 2001; 47: 111 | | [16] | Jandová D, Kasl J, Chvostová E.Mater Sci Forum, 2014; 782: 311 | | [17] | Kasl J, Jandová D.Mater Sci Forum, 2014; 782: 179 | | [18] | Brooks J A.Weld J, 1974; 53(suppl): S517 | | [19] | Ying H Y, Shi C G, Hao C Y, Yu E J, Qin X D, Zhang Q.Acta Metall Sin, 1997; 33: 995 | | [19] | (应慧筠, 施成根, 郝传勇, 于尔靖, 秦旭东, 张琪. 金属学报, 1997; 33: 995) | | [20] | Vagi J J, Martin D C.Weld J, 1956; 35(suppl 3): 137s | | [21] | Kasper J S.Acta Metall, 1954; 2: 456 | | [22] | Cieslak M J, Ritter A M, Savage W F.Weld J, 1984; 63: 133 | | [23] | Kautz H R, Gerlach H.Arch Eisenhuttenw, 1968; 39: 151 | | [24] | Omsen A, Eliasson L.ISIJ Int, 1971; 209: 830 | | [25] | Weiss B, Stickler R.Metall Trans, 1972; 3A: 851 |
|
|