等径角挤压和单向轧制高纯Al再结晶晶界面的取向分布* |
陈吉湘1,王卫国1,2( ),林燕2,林琛2,王乾廷1,2,戴品强1,2 |
1 福州大学材料科学与工程学院, 福州 350108 2 福建工程学院材料科学与工程学院, 福州 350118 |
|
GRAIN BOUNDARY PLANE DISTRIBUTIONS IN RECRYSTALLIZED HIGH PURITY Al AFTER A PARALLEL PROCESSING OF EQUAL CHANNEL ANGULAR PRESSING AND DIRECT ROLLING |
Jixiang CHEN1,Weiguo WANG1,2( ),Yan LIN2,Chen LIN2,Qianting WANG1,2,Pinqiang DAI1,2 |
1 School of Materials Science and Engineering, Fuzhou University, Fuzhou 350108, China 2 School of Materials Science and Engineering, Fujian University of Technology, Fuzhou 350118, China |
引用本文:
陈吉湘,王卫国,林燕,林琛,王乾廷,戴品强. 等径角挤压和单向轧制高纯Al再结晶晶界面的取向分布*[J]. 金属学报, 2016, 52(4): 473-483.
Jixiang CHEN,
Weiguo WANG,
Yan LIN,
Chen LIN,
Qianting WANG,
Pinqiang DAI.
GRAIN BOUNDARY PLANE DISTRIBUTIONS IN RECRYSTALLIZED HIGH PURITY Al AFTER A PARALLEL PROCESSING OF EQUAL CHANNEL ANGULAR PRESSING AND DIRECT ROLLING[J]. Acta Metall Sin, 2016, 52(4): 473-483.
[1] | Watanabe T.Res Mech, 1984; 11: 47 | [2] | Kronberg M L,Wilson F H.Trans AIME, 1949; 185: 501 | [3] | Aust K T, Erb U, Palumbo G.Mater Sci Eng, 1994; A176: 329 | [4] | Chadwick G A, Smith D A.Grain Boundary Structure and Properties. London: Academic Press, 1976: 201 | [5] | Randle V.Scr Mater, 2006; 54: 1011 | [6] | Palumbo G, Erb U.MRS Bull, 1999; 24: 27 | [7] | Xia S, Zhou B X, Chen J W, Wang W G.Acta Metall Sin, 2006; 42: 129 | [7] | (夏爽, 周邦新, 陈觉文, 王卫国. 金属学报, 2006; 42: 129) | [8] | Wang W G, Zhou B X, Feng L.Acta Metall Sin, 2006; 42: 715 | [8] | (王卫国, 周邦新, 冯柳. 金属学报, 2006; 42: 715) | [9] | Wang W G, Zhou B X, Rohrer G S, Guo H, Cai Z X.Mater Sci Eng, 2010; A527: 3695 | [10] | Kumar M, Schwartz A J, King W E.Acta Mater, 2002; 50: 2599 | [11] | Thaveeprungsriporn V, Sinsrok P, Hong-Aram D.Scr Mater, 2001; 44: 67 | [12] | Shimada M, Kokawa H, Wang Z J, Sato Y S, Karibe I.Acta Mater, 2002; 50: 2331 | [13] | Fang X Y, Wang W G, Zhou B X.Acta Metall Sin, 2010; 46: 404 | [13] | (方晓英, 王卫国, 周邦新. 金属学报, 2010; 46: 404) | [14] | Fang X Y, Liu Z Y, Tikhonova M, Belyakov A, Kaibyshev R, Rohrer G S, Wang W G.Acta Metall Sin, 2012; 48: 895 | [14] | (方晓英, 刘志勇, Tikhonova M, Belyakov A, Kaibyshev R, Rohrer G S, 王卫国. 金属学报, 2012; 48: 895) | [15] | Fang X Y, Wang W G, Zhou B X.Rare Met Mater Eng, 2007; 36:1500 | [15] | (方晓英, 王卫国, 周邦新. 稀有金属材料与工程, 2007; 36: 1500) | [16] | McNaughtan D, Worsfold M, Robinson M J.Corros Sci, 2003; 45: 2377 | [17] | Li X L, Chen J H, Liu C H, Feng J N, Wang S H.Acta Metall Sin, 2013; 49: 243 | [17] | (李祥亮, 陈江华, 刘春辉, 冯佳妮, 王时豪. 金属学报, 2013; 49: 243) | [18] | Zhang H F, Zheng Z Q, Zhong S, Luo X F, Zhong J.Trans Nonferrous Met Soc China, 2012; 22: 1025 | [18] | (张海锋, 郑子樵, 钟申, 罗先甫, 钟警. 中国有色金属学报, 2012; 22: 1025) | [19] | Saylor D M, Dasher B E, Rollett A D, Rohrer G S.Acta Mater, 2004; 52: 3649 | [20] | Dong L, Wang W G.Acta Phys Sin, 2013; 15: 42 | [20] | (董垒, 王卫国. 物理学报, 2013; 15: 42) | [21] | Wang W G, Lin C, Li G H, Hua N B, Zhou B X, Fang X Y, Dai P Q, Chen W Z.Sci China, 2014; 44E: 1295 | [21] | (王卫国, 林琛, 李广慧, 花能斌, 周邦新, 方晓英, 戴品强, 陈文哲. 中国科学, 2014; 44E: 1295) | [22] | Segal V M.Mater Sci Eng, 1995; A197: 157 | [23] | Beladi H, Rohrer G S.Metall Mater Trans, 2013; 44A: 115 | [24] | Yu Y N, Liu G Q.Stereologic: Principles and Applications of Quantitative Analysis of Tissue. Beijing: Metallurgical Industry Press, 1989: 123 | [24] | (余永宁, 刘国权. 体视学:组织定量分析的原理和应用. 北京: 冶金工业出版社, 1989: 123) | [25] | Rohrer G S, Saylor D M, Dasher B E, Adams B L, Rollett A D, Wynblatt P.Z Metallkd, 2004; 95: 197 | [26] | Engler O, Huh M.Mater Sci Eng,1999; A271: 371 | [27] | MacKenzie J K.Biometrika, 1958; 45: 229 | [28] | Li J, Dillon S J, Rohrer G S.Acta Mater, 2009; 57: 4304 | [29] | Beladi H, Nuhfer N T, Rohrer G S.Acta Mater, 2014; 70: 281 | [30] | Wen Y N, Zhang J M.Solid State Commun, 2007; 144: 163 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|