| 镍基粉末高温合金中微量元素Hf的作用* |
张义文1,2( ),胡本芙3 |
2 钢铁研究总院高温合金新材料北京市重点实验室, 北京 100081 3 北京科技大学材料科学与工程学院, 北京 100083 |
|
| FUNCTION OF MICROELEMENT Hf IN POWDER METALLURGY NICKEL-BASED SUPERALLOYS |
Yiwen ZHANG1,2( ),Benfu HU3 |
1 High Temperature Material Institute, Central Iron and Steel Research Institute, Beijing 100081 2 Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing 100081 3 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
张义文,胡本芙. 镍基粉末高温合金中微量元素Hf的作用*[J]. 金属学报, 2015, 51(8): 967-975.
Yiwen ZHANG,
Benfu HU.
FUNCTION OF MICROELEMENT Hf IN POWDER METALLURGY NICKEL-BASED SUPERALLOYS[J]. Acta Metall Sin, 2015, 51(8): 967-975.
| [1] | Cochardt A W, Township W, County A. US Pat, 3005705, 1961 | | [2] | Academic Committee of the Superalloys CSM. China Superalloys Handbook. Beijing: China Zhijian Publishing House, 2012: 1 (中国金属学会高温材料分会. 中国高温合金手册(上), 北京: 中国质检出版社, 2012: 1) | | [3] | Davis J R. ASM Specialty Handbook: Nickel, Cobalt and Their Alloys. Materials Park: ASM International, 2000: 203 | | [4] | Evans D J, Eng R D. In: Hausner H H, Antes H W, Smith G D eds., Modern Developments in Powder Metallurgy. Vol.14, Princeton: MPIF and APMI, 1981: 51 | | [5] | Chang M, Koul A K, Cooper C. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Proc 8th Int Symp on Superalloy, Pennsylvania: TMS, 1996: 677 | | [6] | Miner R V. Metall Trans, 1977; 8A: 259 | | [7] | Larson J M, Volin T E, Larson F G. In: Braun J D, Arrowsmith H W, Mccall J L eds., Microstructural Science. Vol.5, New York: American Elsevier Pub., 1977: 209 | | [8] | Warren R, Ingesten N G, Winberg L, R?nnhult T. Powder Metall, 1984; 27: 141 | | [9] | Radavich J, Furrer D, Carneiro T, Lemsky J. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Proc 11th Int Symp on Superalloy, Pennsylvania: TMS, 2008: 63 | | [10] | Schirra J J, Reynolds P L, Huron E S, Bain K R, David P, Mourer D P. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Proc 10th Int Symp on Superalloy, Warrendale: TMS, 2004: 341 | | [11] | Wlodek S T, Kelly M, Alden D. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Sissinger R D, Klarstrom D L eds., Proc 7th Int Symp on Superalloy, Pennsylvania: TMS, 1992: 467 | | [12] | Locq D, Caron P. J Aerospace Lab, 2011; 3: 1 | | [13] | Hardy M C, Zirbel B, Shen G, Shankar R. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Proc 10th Int Symp on Superalloy, Warrendale: TMS, 2004: 83 | | [14] | Starink M J, Reed P A. Mater Sci Eng, 2008; A491: 279 | | [15] | Domingue J A, Boeseh W J, Radavich J F. In: Tien J K, Wlodek S T, Morrow H III eds., Proc 4th Int Symp on Superalloy, Ohio: ASM, 1980: 335 | | [16] | Hu B F, Chen H M, Song D, Li H Y. Acta Metall Sin, 2005; 41: 1042 (胡本芙, 陈焕铭, 宋 铎, 李慧英. 金属学报, 2005; 41: 1042) | | [17] | Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. J Shandong Univ Sci Technol (Nat Sci), 2009; 28: 51 (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 山东科技大学学报(自然科学版), 2009; 28: 51) | | [18] | Lifshitz I M, Slyzov V V. J Phys Chem Solids, 1961; 19: 35 | | [19] | Wagner C. Z Elektrochem, 1961; 65: 581 | | [20] | Menzies R G, Bricknell R H, Craven A J. Philos Mag, 1980; 41A: 493 | | [21] | Qiu C L, Attallah M M, Wu X H, Andrews P. Mater Sci Eng, 2013; A564: 176 | | [22] | Doi M, Miyazaki T, Wakatsuki T. Mater Sci Eng, 1985; 74: 139 | | [23] | Miyazaki T, Imamura H, Mori H, Kozakai T. J Mater Sci, 1981; 16: 1197 | | [24] | Qiu Y Y. J Alloys Compd, 1998; 270: 145 | | [25] | Qiu Y Y. Acta Mater, 1996; 44: 4969 | | [26] | Kaufman M J, Voorhees P W, Johnson W C, Biancaniello F S. Metall Trans, 1989; 20A: 2171 | | [27] | Kotval P S, Venables J D, Calder R W. Metall Trans, 1972; 3: 453 | | [28] | Zhen B L, Zhang S J. Central Iron Steel Res Inst Technol Bull, 1981; 1(1): 65 (甄宝林, 张绍津. 钢铁研究总院学报, 1981; 1(1): 65) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|