熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究* |
邵珩1,李岩2,南海2,许庆彦1( ) |
2 北京航空材料研究院, 北京 100095 |
|
RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY |
Heng SHAO1,Yan LI2,Hai NAN2,Qingyan XU1( ) |
1 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084 2 Beijing Institute of Aeronautical Materials, Beijing 100095 |
引用本文:
邵珩,李岩,南海,许庆彦. 熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究*[J]. 金属学报, 2015, 51(8): 976-984.
Heng SHAO,
Yan LI,
Hai NAN,
Qingyan XU.
RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY[J]. Acta Metall Sin, 2015, 51(8): 976-984.
[1] | Liu J, Yang Y, Lu D. Foundry, 2008; 57: 1155 (刘 剑, 杨 屹, 卢 东. 铸造, 2008; 57: 1155) | [2] | Atwood R C, Lee P D, Curtis R V, Maijer D M. Dent Mater, 2007; 23(1): 60 | [3] | Liang Z J, Xu Q Y, Li J T, Li S Q, Zhang J, Liu B C, Zhong Z Y. Rare Met Mater Eng, 2003; 32: 164 (梁作俭, 许庆彦, 李俊涛, 李世琼, 张 继, 柳百成, 仲增墉. 稀有金属材料与工程, 2003; 32: 164) | [4] | Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1149 (郭志鹏, 熊守美, 曹尚铉, 崔正吉. 金属学报, 2007; 43: 1149) | [5] | Guo Z P, Xiong S M, Cho S H, Choi J K. Acta Metall Sin, 2007; 43: 1155 (郭志鹏, 熊守美, 曹尚铉, 崔正吉. 金属学报, 2007; 43: 1155) | [6] | Cao Y Y, Guo Z P, Xiong S M. China Foundry, 2014; 11: 314 | [7] | Guo Z P, Xiong S M, Liu B C, Mei L, Allison J. Int J Heat Mass Transfer, 2008; 51: 6032 | [8] | Long A, Thornhill D, Armstrong C, Watson D. Appl Therm Eng, 2011; 31: 3996 | [9] | O'Mahoney D, Browne D J. Exp Therm Fluid Sci, 2000; 22: 111 | [10] | Yuan S, Bu K, Dong Y W. Foundry Technol, 2012; 33: 177 (袁 帅, 卜 昆, 董一巍. 铸造技术, 2012; 33: 177) | [11] | Konrad C H, Brunner M, Kyrgyzbaev K, V?lkl R, Glatzel U. J Mater Process Technol, 2011; 211: 181 | [12] | Zhang W H, Xie G N, Zhang D. Exp Therm Fluid Sci, 2010; 34: 1068 | [13] | Dong Y W, Bu K, Dou Y Q, Zhang D H. J Mater Process Technol, 2011; 211: 2123 | [14] | Rafique M M A, Iqbal J. Int J Heat Mass Transfer, 2009; 52: 2132 | [15] | Jin H P, Li J R, Yu J, Liu S Z. Rare Met Mater Eng, 2010; 39: 767 | [16] | Sun Z Z, Hu H, Niu X P. J Mater Process Technol, 2011; 211: 1432 | [17] | Ilkhchy A F, Jabbari M, Davami P. Int Commun Heat Mass Transfer, 2012; 39: 705 | [18] | Aweda J O, Adeyemi M B. J Mater Process Technol, 2009; 209: 1477 | [19] | Xu H, Hou H, Zhao Y H, Chen Z. Chin J Nonferrous Met, 2003; 13: 881 (徐 宏, 侯 华, 赵宇宏, 陈 铮. 中国有色金属学报, 2003; 13: 881) | [20] | Palumbo G, Piglionico V, Piccininni A, Guglielmi P, Sorgente D, Tricarico L. Appl Therm Eng, 2015; 78: 682 | [21] | Chen L P, Wang Y X, Peng L M, Fu P H, Jiang H Y. Exp Therm Fluid Sci, 2014; 54: 196 | [22] | Wang Z F, Yao M, Wang X D, Zhang X B, Yang L S, Lu H Z, Wang X. J Mater Process Technol, 2014; 214: 44 | [23] | Watanabe K, Miyakawa O, Takada Y, Okuno O, Okabe T. Biomaterials, 2003; 24: 1737 | [24] | Liang Z J, Xu Q Y, Li J T, Li S Q, Zhang J, Liu B C, Zhong Z Y. Rare Met Mater Eng, 2002; 31: 353 (梁作俭, 许庆彦, 李俊涛, 李世琼, 张 继, 柳百成, 仲增墉. 稀有金属材料与工程, 2002; 31: 353) | [25] | Beck J V, Blackwell B, St Clair C R. Inverse Heat Conduction: Ill-Posed Problems. New York: Wiley, 1985: 145 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|