| 热变形和淬火配分处理的复合作用对低碳合金钢马氏体相变机制的影响* |
王存宇1,常颖2( ),杨洁3,赵坤民2,董瀚1 |
2 大连理工大学汽车工程学院工业装备结构分析国家重点实验室, 大连 116024 3 长城汽车股份有限公司技术中心, 保定 071000 |
|
| THE COMBINED EFFECT OF HOT DEFORMATION PLUS QUENCHING AND PARTITIONING TREATMENT ON MARTENSITE TRANSFORMATION OF LOW CARBON ALLOYED STEEL |
Cunyu WANG1,Ying CHANG2( ),Jie YANG3,Kunmin ZHAO2,Han DONG1 |
1 East China Branch of Central Iron & Steel Research Institute, Beijing 100081 2 State Key Laboratory of Industrial Equipment Structural Analysis, School of Automotive Engineering, Dalian University of Technology, Dalian 116024 3 Technology Center, Great Wall Motor Company Limited, Baoding 071000 |
引用本文:
王存宇,常颖,杨洁,赵坤民,董瀚. 热变形和淬火配分处理的复合作用对低碳合金钢马氏体相变机制的影响*[J]. 金属学报, 2015, 51(8): 913-919.
Cunyu WANG,
Ying CHANG,
Jie YANG,
Kunmin ZHAO,
Han DONG.
THE COMBINED EFFECT OF HOT DEFORMATION PLUS QUENCHING AND PARTITIONING TREATMENT ON MARTENSITE TRANSFORMATION OF LOW CARBON ALLOYED STEEL[J]. Acta Metall Sin, 2015, 51(8): 913-919.
| [1] | Briant C L, Banerji S K. Metall Trans, 1979; 10A: 1729 | | [2] | Lee W S, Su T T. J Mater Process Technol, 1999; 87: 198 | | [3] | Salemi A, Abdollah-Zadeh A. Mater Charact, 2008; 59: 484 | | [4] | Matlock D K, BrautigamV E, Speer J G. Mater Sci Forum, 2003; 426-432: 1089 | | [5] | Speer J, Matlock D K, De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611 | | [6] | Santofimia M J, Speer J G, Clarke A J, Zhao L, Sietsma J. Acta Mater, 2009; 57: 4548 | | [7] | Wang C Y, Shi J, Cao W Q, Hui W J, Wang M Q, Dong H. Acta Metall Sin, 2011; 47: 720 (王存宇, 时 捷, 曹文全, 惠卫军, 王毛球, 董 瀚, 金属学报, 2011; 47: 720) | | [8] | Clarke A J, Speer J G, Matlock D K, Rizzo F C, Edmonds D V, Santofimia M J. Scr Mater, 2009; 61: 149 | | [9] | Rizzo F, Martins A R, Speer J G. Mater Sci Forum, 2007; 539-543: 4476 | | [10] | Wang C Y, Shi J, Cao W Q, Dong H. Mater Sci Eng, 2011; A527: 3442 | | [11] | Cheng L, Wu K M, Wan X L, Wei R. Mater Charact, 2014; 87: 86 | | [12] | Marder A R, Krauss G. Trans ASM, 1969; 69: 957 | | [13] | Hao Q G, Wang Y, Jia X S, Zuo X W, Chen N L, Rong Y H. Acta Metall Sin (Engl Lett), 2014; 27: 444 | | [14] | Hsu T Y, Jin X J, Rong Y H. J Alloys Compd, 2013; 577: S568 | | [15] | Xiong X C, Chen B, Huang M X, Wang J F, Wang L. Scr Mater, 2013; 68: 321 | | [16] | Speer J G, Matlock D K. World Iron Steel, 2009; 1: 31 | | [17] | Chandra T, Ionescu M, Mantovani D. Mater Sci Forum, 2012; 706-709: 2824 | | [18] | Zhou S, Zhang K, Chen N L, Gu J F, Rong Y H. ISIJ Int, 2011; 51: 1688 | | [19] | Thomas G A, Speer J G, Matlock D K. Metall Mater Trans, 2011; 42A: 3652 | | [20] | Koistinen D P, Marburger R E. Acta Metall, 1959; 7: 59 | | [21] | Guimaraes J R C, Shyne J C. Metall Trans, 1973; 2: 2063 | | [22] | Wang C Y. PhD Dissertation, Central Iron & Steel Research Institute, Beijing, 2010 (王存宇. 钢铁研究总院博士学位论文, 北京, 2010) | | [23] | Olson G B, Cohen M. J Less-Common Met, 1972; 28: 107 | | [24] | Hsu T Y. Martensitic Transformation and Martensite. 2nd Ed., Beijing: Science Press, 1999: 690 (徐祖耀. 马氏体相变与马氏体. 第二版, 北京: 科学出版社, 1999: 690) | | [25] | Liu C C, Yao K F, Gao G F, Liu Z. Acta Metall Sin, 1999; 35: 1125 (刘春成, 姚可夫, 高国峰, 刘 庄. 金属学报, 1999; 35: 1125) | | [26] | Zhang Y J, Wang C Y, Liu W Z, Cao W Q. Trans Met Heat Treat, 2013; 34(5): 97 (张玉杰, 王存宇, 刘文忠, 曹文全. 材料热处理学报, 2013; 34(5): 97) |
|
|