| THE INTERFACIAL REACTION AND INTERMETALLIC COMPOUND GROWTH BEHAVIOR OF BGA STRUC-TURE Sn-3.0Ag-0.5Cu/Cu SOLDER JOINT AT LOW REFLOW TEMPERATURES |
| ZHOU Minbo, MA Xiao, ZHANG Xinping |
| School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 |
引用本文:
周敏波,马骁,张新平. BGA结构Sn-3.0Ag-0.5Cu/Cu焊点低温回流时界面反应和IMC生长行为[J]. 金属学报, 2013, 49(3): 341-350.
ZHOU Minbo,
MA Xiao,
ZHANG Xinping.
THE INTERFACIAL REACTION AND INTERMETALLIC COMPOUND GROWTH BEHAVIOR OF BGA STRUC-TURE Sn-3.0Ag-0.5Cu/Cu SOLDER JOINT AT LOW REFLOW TEMPERATURES[J]. Acta Metall Sin, 2013, 49(3): 341-350.
| [1] Zeng K, Tu K N.Mater Sci Eng, 2002; R38: 55 [2] Chan Y C, Yang D.Prog Mater Sci, 2010; 55: 428 [3] Ulrich R K, Brown W D.Advanced Electronic Packaging. 2nd Ed., New York: IEEE Press, 2004: 1 [4] Bernstein L.J Electrochem Soc, 1966; 113: 1282 [5] Bosco N S, Zok F W.Acta Mater, 2004; 52: 2965 [6] Bosco N S, Zok F W.Acta Mater, 2005; 53: 2019 [7] Xu H B, Li M Y, Fu Y G, Wang L, Kim J.Solder Surf Mount Technol, 2009; 21: 45 [8] Xu H B, Li M Y, Kim J, Kim D.J Mater Process Technol, 2009; 209: 2781 [9] Tu K N.Mater Chem Phys, 1996; 46: 217 [10] Tu K N, Zeng K.Mater Sci Eng, 2001; R34: 1 [11] Laurila T, Vuorinen V, Paulasto-Krockel M.Mater Sci Eng, 2010; R68: 1 [12] Kajihara M.Acta Mater, 2004; 52: 1193 [13] Li J F, Agyakwa P A.Acta Mater, 2010; 58: 3429 [14] Li X P, Zhou M B, Xia J M, Ma X, Zhang X P.Acta Metall Sin, 2011; 47: 611 (李勋平, 周敏波, 夏建民, 马骁, 张新平. 金属学报, 2011; 47: 611) [15] Shen J, Chan Y C, Liu S Y.Acta Mater, 2009; 57: 5196 [16] Onishi M, Fujibuchi H.Trans Jpn Inst Met, 1975; 16: 539 [17] Schaefer M, Fournelle R A, Liang J.J Electron Mater, 1998; 27: 1167 [18] Vianco P T, Hlava P, Kilgo A.J Electron Mater, 1994; 23: 583 [19] Mei Z, Sunwoo A, Morris J.Metall Mater Trans, 1992; 23A: 857 [20] Vianco P T, Erickson K L, Hopkins P L.J Electron Mater, 1994; 23: 721 [21] Erickson K L, Hopkins P L, Vianco P T.J Electron Mater, 1994; 23: 729 [22] Deng X, Piotrowski G, Williams J J, Chawla N.J Electron Mater, 2003; 32: 1403 [23] Li J F, Agyakwa P A, Johnson C M.Acta Mater, 2010; 58: 3429 [24] Zeng K, Stierman R, Chiu T C, Edwards D, Ano K, Tu K N.J Appl Phys, 2005; 97: 024508 [25] Tu K N, Thompson R D.Acta Metall, 1982; 30: 947 [26] Ghosh G.Acta Mater, 2000; 48: 3719 [27] Ma D, Wang W D, Lahiri S K.J Appl Phys, 2002; 91: 3312 [28] Moon K W, Boettinger W J, Kattner U R, Biancaniello F S, Handwerker C A.J Electron Mater, 2000; 29: 1122 [29] Loomans M, Fine M.Metall Mater Trans, 2000; 31A: 1155 [30] Boettinger W J, Johnson C E, Bendersky L A, Moon K W, Williams M E, Stafford G R.Acta Mater, 2005; 53: 5033 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|