| Fe-22Mn TRIP/TWIP钢拉伸过程组织、性能及晶体学行为分析 |
| 鲁法云,杨平,孟利,王会珍 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| MICROSTRUCTURE, MECHANICAL PROPERTIES AND CRYSTALLOGRAPHY ANALYSIS OF Fe-22Mn TRIP/TWIP STEEL AFTER TENSILE DEFORMATION |
| LU Fayun, YANG Ping, MENG Li, WANG Huizhen
|
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
鲁法云,杨平,孟利,王会珍. Fe-22Mn TRIP/TWIP钢拉伸过程组织、性能及晶体学行为分析[J]. 金属学报, 2013, 49(1): 1-9.
LU Fayun,
YANG Ping,
MENG Li,
WANG Huizhen.
MICROSTRUCTURE, MECHANICAL PROPERTIES AND CRYSTALLOGRAPHY ANALYSIS OF Fe-22Mn TRIP/TWIP STEEL AFTER TENSILE DEFORMATION[J]. Acta Metall Sin, 2013, 49(1): 1-9.
| [1] Grassel O, Kruger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391 [2] Schumann V H. Neue Hutte, 1972; 17: 605 [3] Saeed-Akbari A, Imlau J, Prahl U, Bleck W. Metall Mater Trans, 2009; 40A: 3076 [4] Allain S, Chateau J-P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387-389: 158 [5] Dumay A, Chateau J-P, Allain S, Migot S, Bouaziz O. Mater Sci Eng, 2008; A483-484: 184 [6] Frommeyer G, Brux U, Neumann P. ISIJ Int, 2003; 3: 438 [7] Bracke L, Kestensa L, Penning J. Scr Mater, 2007; 57: 385 [8] Mina X H, Sawaguchi T, Ogawa K, Maruyama T, Yin F X, Tsuzaki K. Mater Sci Eng, 2011; A528: 5251 [9] Chun Y S, Kim J S, Park K-T, Lee Y-K, Lee C S. Mater Sci Eng, 2012; A533: 87 [10] Kirindi T, Dikici M. J Alloys Compd, 2006; 407: 157 [11] Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1998; A242: 87 [12] Wu X, Tao N, Hong Y, Lu J, Lu K. Scr Mater, 2005; 52: 547 [13] Yang H-S, Bhadeshia H K D H. Scr Mater, 2009; 60: 493 [14] Lu F Y, Yang P, Meng L, Cui F E, Ding H. J Mater Sci Technol, 2011; 27: 257 [15] Lu Y P, Hutchinson B, Molodov D A, Gottstein G. Acta Mater, 2010; 58: 3079 [16] Koyama M, Sawaguchi T, Lee T, Lee C S, Tsuzaki K. Mater Sci Eng, 2011; A528: 7310 [17] Datta K, Delhez R, Bronsveld P M, Beyer J, Geijselaers H J M, Post J. Acta Mater, 2009; 57: 3321 [18] Hedstrom P, Lienert U, Almer J, Oden M. Mater Lett, 2008; 62: 338 [19] Wu C-C, Wang S-H, Chen C-Y, Yang J-R, Chiu P-K, Fang J. Scr Mater, 2007; 56: 717 [20] Yang P, Lu F Y, Meng L, Cui F E. Acta Metall Sin, 2010; 46: 657 (杨平, 鲁法云, 孟利, 崔凤娥. 金属学报, 2010; 46: 657) [21] Yang P, Lu F Y, Meng L, Cui F E. Acta Metall Sin, 2010; 46: 666 (杨平, 鲁法云, 孟利, 崔凤娥. 金属学报, 2010; 46: 666) [22] Liu T Y, Yang P, Meng L, Lu F Y. J Alloys Compd, 2011; 509: 8337 [23] Yang P, Liu T Y, Lu F Y, Meng L. Steel Res Int, 2012; 83: 368 [24] Barbier D, Gey N, Allain S, Bozzolo N, Humbert M. Mater Sci Eng, 2009; A500: 196 [25] Jin J E, Lee Y K. Mater Sci Eng, 2009; A527: 157 [26] Beladi H, Timokhina I B, Estrin Y, Kim J, De Cooman B C, Kim S K. Acta Mater, 2011; 59: 7787 |
|