| B和P对GH984合金组织和力学性能的影响 |
| 肖旋1,赵海强1,2,王常帅2,郭永安2,郭建亭2,周兰章2 |
1) 沈阳理工大学材料科学与工程学院, 沈阳 110168
2) 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECTS OF B AND P ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF GH984 ALLOY |
| XIAO Xuan1), ZHAO Haiqiang1,2), WANG Changshuai2), GUO Yongan2), GUO Jianting2),ZHOU Lanzhang2) |
1) School of Materials Science and Engineering, Shenyang Ligong University, Shenyang 110168
2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
肖旋,赵海强,王常帅,郭永安,郭建亭,周兰章. B和P对GH984合金组织和力学性能的影响[J]. 金属学报, 2013, 29(4): 421-427.
XIAO Xuan,
ZHAO Haiqiang,
WANG Changshuai,
GUO Yongan,
GUO Jianting,
ZHOU Lanzhang.
EFFECTS OF B AND P ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF GH984 ALLOY[J]. Acta Metall Sin, 2013, 29(4): 421-427.
| [1] Guo J T. Acta Metall Sin, 2010; 46: 513 (郭建亭. 金属学报, 2010; 46: 513) [2] Jφrgen B, Sven K, Blum R. Energy, 2006; 31: 1439 [3] Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Chem Phys, 2005; 90: 275 [4] Jablonski P D, Hawk J A, Cowen C J, Maziasz P J. J Metal, 2012; 64: 271 [5] Guo J T, Du X K. Acta Metall Sin, 2005; 41: 1221 (郭建亭, 杜秀魁. 金属学报, 2005; 41: 1221) [6] Wang S H, Du X K, Xu H Z, Yu C S, Guo J T, Hu Q W. Acta Metall Sin, 1995; 31(suppl.): 137 (王淑荷, 杜秀魁, 许慧珍, 于长生, 郭建亭, 胡秋文. 金属学报, 1995; 31(增刊): 137) [7] Zhang J, Luo Y S, Zhao Y S, Yang S, Jia Y L, Cui L L, Xu J W, Tang D Z. J Aeronaut Mater, 2011; 31(suppl.): 90 (张剑, 骆宇时, 赵云松, 杨帅, 贾玉亮, 崔丽丽, 许剑伟, 唐定中. 航空材料学报, 2011; 31(增刊): 90) [8] Sun W R, Guo S R, Lu D Z, Hu Z Q. Metall Mater Trans, 1997; A28: 649 [9] Hu Z Q, Song H W, Guo S R, Sun W R. J Mater Sci Technol, 2001; 17: 39901 [10] Xiao L, Chen D L, Chaturvedi M C. Metall Mater Trans, 2005; A36: 2671 [11] Li N, Guo S R, Lu D Z, Sun W R, Meng X N, Hu Z Q. Acta Metall Sin, 2003; 39: 1255 (李娜, 郭守仁, 卢德忠, 孙文儒, 孟晓娜, 胡壮麒. 金属学报, 2003; 39: 1255) [12] Seah M P. Acta Metall Mater, 1980; 28: 955 [13] Was G S, Sung J K, Angeliu T M. Metall Mater Trans, 1992; A23: 3343 [14] Sun W R, Guo S R, Lu D Z, Hu Z Q. Metall Mater Trans, 1997; A28: 649 [15] McKamey C G, Carmichael C A, Cao W D, Kennedy R L. Scr Mater, 1998; 38: 485 [16] Sheng L Y, Zhang W, Guo J T, Wang Z S, Ovcharenko V E, Zhou L Z, Ye H Q. Intermetallics, 2009; 17: 572 [17] Sheng L Y, Xi T F, Lai C, Guo J T, Zheng Y F. Trans Nonferrous Met Soc China, 2012; 22: 489 [18] Sheng L Y, Xie Y, Xi T F, Guo J T, Zheng Y F, Ye H Q. Mater Sci Eng, 2011; A528: 8324 [19] Sheng L Y, Yang F, Xi T F, Guo J T, Ye H Q. Mater Sci Eng, 2012; A555: 131 [20] Zheng L, Xu T D, Deng Q, Si H, Dong J X. Acta Metall Sin, 2007; 43: 893 (郑磊, 徐庭栋, 邓群, 司红, 董建新. 金属学报, 2007; 43: 893) [21] Tytko D, Choi P, Klower J, Kostka A, Inden G, Raabe D. Acta Mater, 2012; 60: 1731 [22] Wang L G, Wang C Y. Mater Sci Eng, 1997; A234: 521 [23] Hu Z Q, Sun W R, Guo S R, Lu D Z. Chin J Nonferrous Met, 2001; 11: 947 (胡壮麒, 孙文儒, 郭守仁, 卢德忠. 中国有色金属学报, 2001; 11: 947) [24] Shu D L. Mechanical Properties of Engineering Materials. Beijing: China Machine Press, 2010: 164 (束德林. 工程材料力学性能. 北京: 机械工业出版社, 2010: 164) [25] Sheng L Y, Guo J T, Zhang W, Xie Y, Zhou L Z, Ye H Q. Acta Metall Sin, 2009; 45: 1025 (盛立远, 郭建亭, 章炜, 谢亿, 周兰章, 叶恒强. 金属学报, 2009; 45: 1025) [26] Sheng L Y, Yang F, Xi T F, Zheng Y F, Guo J T. Intermetallics, 2012; 27: 14 [27] Sheng L Y, Yang F, Xi T F, Guo J T. Ye H Q. Composites, 2012; 45B: 785 [28] Guo J T. Material Science of Superalloy. Beijing: Science Press, 2008: 239 (郭建亭. 高温合金材料学(下册). 北京: 科学出版社, 2008: 239) [29] Peng B C, Zhang H X, Hong J, Gao J Q, Zhang H Q, Li J F, Wang Q J. Mater Sci Eng, 2010; A527: 4424 |
|