| 形变及冷却速率对热轧超高强汽车钢板中纳米析出的影响 |
| 王晓南1,2,邸洪双1,杜林秀1 |
1. 东北大学 轧制技术及连轧自动化国家重点实验室, 沈阳 110819
2. 苏州大学沙钢钢铁学院, 苏州 215201 |
|
| EFFECTS OF DEFORMATION AND COOLING RATE ON NANO-SCALE PRECIPITATION IN HOT-ROLLED ULTRA-HIGH STRENGTH STEEL |
| WANG Xiaonan1,2, DI Hongshuang1, DU Linxiu1 |
1. State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
2. Shagang School of Iron and Steel, Soochow University, Suzhou 215201 |
引用本文:
王晓南,邸洪双,杜林秀. 形变及冷却速率对热轧超高强汽车钢板中纳米析出的影响[J]. 金属学报, 2012, 48(5): 621-628.
,
,
.
EFFECTS OF DEFORMATION AND COOLING RATE ON NANO-SCALE PRECIPITATION IN HOT-ROLLED ULTRA-HIGH STRENGTH STEEL[J]. Acta Metall Sin, 2012, 48(5): 621-628.
| [1] Jiao Z B, Liu J C. Mater China, 2011; 30: 6 (焦增宝, 刘锦川. 中国材料进展, 2011; 30: 6)[2] Kashima T, Muka Y. “R$\&$D” Kobe Steel Eng Rep, 2002; 52: 19[3] Tetsuo S, Yoshimasa F, Shinjiro K. JFE Technol Rep, 2004; 4: 25[4] Kazuhiro S, Yoshimasa F, Shinjiro K. JFE Technol Rep, 2007; 10: 19[5] Misra R D K, Nathani H, Hartmann J E, Siciliano F. Mater Sci Eng, 2005; A394: 339[6] Lu J X, Wang G D. Iron Steel, 2005; 40: 69 (陆匠心, 王国栋. 钢铁, 2005; 40: 69)[7] Sha Q Y, Li G Y, Yan P Y, Ao L G, Hao S. Mater China, 2011; 30: 23 (沙庆云, 李桂艳, 严平沅, 熬列格, 郝森. 中国材料进展, 2011; 30: 23)[8] Zhou J, Kang Y L, Mao X P, Li L J, Lin Z Y. Iron Steel, 2006; 41(Suppl.): 343 (周建, 康永林, 毛新平, 李烈军, 林振源. 钢铁, 2006; 41(增刊): 343)[9] Huang Q Y, Yan H W, Pan Y L, Yang J R. Min Metall, 2008; 53: 45(黄庆渊, 颜鸿威, 潘永林, 杨哲人. 矿冶, 2008; 53: 45)[10] Chen C Y, Yen H W, Kao F H , Li W C, Huang C Y, Yang J R, Wang S H. Mater Sci Eng, 2009; A499: 162[11] Wang T P, Kao F H, Wang S H, Yang Z R, Huang C Y, Chen H R. Mater Lett, 2011; 65: 396[12] Wang X N, Du L X, Zhang H L, Di H S. J Iron Steel Res, 2011; 23: 45 (王晓南, 杜林秀, 张海仑, 邸洪双. 钢铁研究学报, 2011; 23: 45)[13] Wang X N, Du L X, Xie H, Di H S, Gu D H. Steel Res Int, 2011; 82: 1417[14] Okamoto R, Borgenstam A, Agren J. Acta Mater, 2010; 58: 4783[15] Jia Z, Misra R D K, O'Malley R, Jansto S J. Mater Sci Eng, 2011; A528: 7077[16] Xu G, Gan X L, Ma G J, Luo F, Zou H. Mater Des, 2010; 31: 2891[17] Niakan H, Najiafizadeh A. Mater Sci Eng, 2010; A527: 5410[18] Olasolo M, Uranga P, Rodriguez-Ibabe J M, Lopez B. Mater Sci Eng, 2011; A528: 2559[19] Okamoto R, Borgenstam A, Agren J. Acta Mater, 2010; 58: 4783[20] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 145 (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 145)[21] He X L, Shang C J, Yang S W, Wang X M, Guo H. High Performance Low Carbon Bainite Steel. Beijing: Metallurgical Industry Press, 2008: 202 (贺信莱, 尚成嘉, 杨善武, 王学敏, 郭晖. 高性能低碳贝氏体钢. 北京: 冶金工业出版社, 2008: 202)[22] Manohar P A, Dunne D P, Chandar T, Killmore C R. ISIJ Int, 1996; 36: 194[23] Kang Y L, Fu J, Liu D L, Yu H.Control of Microstructure and Properties in Thin Slab Casting and Rolling Steel.Beijing: Metallurgical Industry Press, 2006: 144 (康永林, 傅杰, 柳得橹, 于浩. 薄板坯连铸连轧钢的组织性能控制. 北京: 冶金工业出版社, 2006: 144)[24] Dutta B, Sellars C M. Mater Sci Technol, 1987; 3: 197[25] Porter D A, Easterlin K E. Phase Transformations in Metals and Alloys.New York: Van Nostrand Reinhold Company Ltd., 1981: 303[26] Takashi S, Shuji K, Sadao H, Akio S, Takao O, Kuniaki O. JFE Technol Rep, 2004; 2: 1 |
|