| 纵向磁场对不同尺寸定向凝固高温合金DZ417G组织的影响 |
| 玄伟东,任忠鸣,李传军,任维丽,陈超,于湛 |
| 上海大学上海市现代冶金与材料制备重点实验室, 上海 200072 |
|
| EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G WITH DIFFERENT SIZES |
| XUAN Weidong, REN Zhongming, LI Chuanjun, REN Weili, CHEN Chao, YU Zhan |
| Shanghai Key Laboratory of Modern Metallurgy & Materials Processing,Shanghai University, Shanghai 200072 |
引用本文:
玄伟东,任忠鸣,李传军,任维丽,陈超,于湛. 纵向磁场对不同尺寸定向凝固高温合金DZ417G组织的影响[J]. 金属学报, 2012, 48(5): 629-635.
,
,
,
,
,
.
EFFECT OF LONGITUDINAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ417G WITH DIFFERENT SIZES[J]. Acta Metall Sin, 2012, 48(5): 629-635.
| [1] Utech H P, Flemings M C. J Appl Phys, 1966; 37: 2021[2] Chedzey H A, Hurle D T J. Nature, 1966; 210: 933[3] Matthiesen D H, Wargo M J, Motakef S. J Cryst Growth, 1987; 85: 557[4] Robertson G D, Conner D O. J Cryst Growth, 1986; 76: 100[5] Moreau R, Laskar O, Tanaka M. Mater Sci Eng, 1993; A173: 93[6] Lehmann P, Moreau R, Camel D. Acta Mater, 1998; 46: 4067[7] Alboussiere T, Moreau R, Camel D. C R Acad Sci, 1991; 313: 749[8] Zhang H W, Chen R Z. Acta Metall Sin, 1997; 33: 370 (张宏炜, 陈荣章. 金属学报, 1997; 33: 370)[9] Trivedi R, Liu S, Mazumder P, Simsek E. Sci Technol Adv Mater,2001; 2: 309[10] Zheng Q, Hou G C, Sun X F, Jin T, Guan H R, Hu Z Q. J Mater Eng,2002; 3: 24 (郑启, 侯桂臣, 孙晓峰, 金涛, 管恒荣, 胡壮麒. 材料工程, 2002; 3: 24)[11] Qu M, Liu L, Tang F T, Fu H Z. Trans Nonferrous Met Soc China,2009; 19: 1[12] Mukherji D, Rosler J, Kruger M, Heilmaier M, Bolitz M C,Volkl R, Glatzel U, Szentmiklosi L. Scr Mater, 2012; 66: 60[13] Liu L, Huang T W, Qu M, Liu G, Zhang J, Fu H Z. J Mater ProcessTechnol, 2010; 210: 159[14] Huang T W, Liu L, Zhang W G, Zhang J, Fu H Z. Acta Metall Sin,2009; 45: 1225 (黄太文, 刘林, 张卫国, 张军, 傅恒志. 金属学报, 2009, 45: 1225)[15] Ren W L, Zhang T, Ren Z M, Zhao A K, Zhong Y B, Guo J T. Mater Lett, 2009; 63: 382[16] Dong J W, Ren Z M, Ren W L, Li X, Li X. Acta Metall Sin,2010; 46: 71 (董建文, 任忠鸣, 任维丽, 李喜, 李旭. 金属学报, 2010; 46: 71)[17] Li X, Gagnoud A, Ren Z M, Fautrelle Y, Moreau R. Acta Mater, 2009, 57: 2180[18] Zimmermann G, Weiss A, Mbaya Z. Mater Sci Eng, 2005; A413-414: 236[19] Wang X D, Ciobanas A, Baltaretu F, Bianchi A M, Fautrelle Y. Mater Sci Forum, 2006; 508: 163[20] Li X, Ren Z M, Wang J, Han Y F, Sun B D. Mater Lett, 2012; 67: 205[21] Li X, Ren Z M, Cao G H, Gagmoud A, Fautrelle Y. Mater Lett,2011; 65: 3340[22] Li X, Ren Z M, Fautrelle Y. J Crys Growth, 2006; 290: 571[23] Kishida Y, Takeda K, Miyoshino I, Taleuchi E. ISIJ Int,1990; 30: 34[24] Yasuda H, Yoshimoto T, Mizuguchi T, Tamura Y, Nagira T, Yoshiya M. ISIJ Int, 2007; 47: 612[25] Ren Z M, Jin J Z. J Mater Sci, 1992; 27: 4663[26] Zhang T, Ren W L, Dong J W, Li X, Ren Z M, Cao G H, Zhong Y B,Deng K, Lei Z S, Guo J T. J Alloys Compd, 2009; 487: 612[27] Giamei A F, Kear B H. Metall Trans, 1970; 1: 2185[28] Li X, Fautrelle Y, Ren Z M. Acta Mater, 2007; 55: 3803[29] Steinbach S, Ratke L. Mater Sci Eng, 2005; A413-414: 200[30] Hui J, Tiwari R, WU X, Tewari S N, Trivedi R. Metall Mater Trans,2002; 31A: 3499[31] Steinbach S, Ratke L. Metall Mater Trans, 2007; 38A: 1388[32] Dupouy M D, Camel D, Favier J J. Acta Metall Mater, 1992; 40: 1791[33] Ren Z M, Jin J Z, Guo K R. J Mater Sci, 1991; 26: 3599[34] Jackson K A, Hunt J D, Uhlmann D R, Seward T P. Trans TMS-AIME,1966; 236: 149[35] Curreri P A, Lee J E, Stefanescu D M. Metall Mater Trans,1988; 19A: 2671 |
|