| 考虑固溶及时效处理的镁合金铸件微观组织模拟及力学性能预测 |
| 韩国民1), 韩志强1), 霍亮1), 段军鹏2), 朱训明2), 柳百成1, 3) |
1) 清华大学机械工程系, 先进成形制造教育部重点实验室, 北京 100084
2) 威海万丰镁业科技发展有限公司, 威海 264209
3) 清华大学汽车工程系, 汽车安全与节能国家重点实验室, 北京 100084 |
|
| MICROSTRUCTURE SIMULATION AND MECHANICAL PROPERTY PREDICTION OF MAGNESIUM ALLOY CASTING CONSIDERING SOLID SOLUTION AND AGING PROCESS |
| HAN Guomin1), HAN Zhiqiang1), HUO Liang1), DUAN Junpeng2), ZHU Xunming2), LIU Baicheng1, 3) |
1) Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2) Wanfeng Magnesium Co. Ltd., Weihai 264209
3) State Key Laboratory of Automotive Safety and Energy, Department of Automotive Engineering, Tsinghua University, Beijing 100084 |
引用本文:
韩国民 韩志强 霍亮 段军鹏 朱训明 柳百成. 考虑固溶及时效处理的镁合金铸件微观组织模拟及力学性能预测[J]. 金属学报, 2012, 48(3): 363-370.
,
,
,
,
,
.
MICROSTRUCTURE SIMULATION AND MECHANICAL PROPERTY PREDICTION OF MAGNESIUM ALLOY CASTING CONSIDERING SOLID SOLUTION AND AGING PROCESS[J]. Acta Metall Sin, 2012, 48(3): 363-370.
| [1] Fribourg G, Brechet Y, Deschamps A, Simar A. Acta Mater, 2011; 59: 3621[2] Smoljan B, Iljki´c, D, Tomaˇsi´c N. J Achiev Mater Manuf Eng, 2010; 40: 155[3] Panuˇskov´a M, Tillov´a E, Chalupov´a M. Strength Mater, 2008; 40: 98[4] Liu Z Y, Xu Q Y, Liu B C. Acta Metall Sin, 2007; 43: 367(刘志勇, 许庆彦, 柳百成. 金属学报, 2007; 43: 367)[5] Huo L, Han Z Q, Liu B C. Acta Metall Sin, 2009; 45: 1414(霍亮, 韩志强, 柳百成. 金属学报, 2009; 45: 1414)[6] Huo L, Han Z Q, Liu B C. In: Agnew S, Neelameggham N R, Nyberg E A eds., Magnesium Technology 2010. Warrendale, PA: The Minerals, Metals and Materials Society, 2010: 601[7] Yin H B, Felicelli S D. Modell Simul Mater Sci Eng, 2009; 17: 1[8] Huo L. PhD Thesis, Tsinghua University, Beijing, 2011(霍亮. 清华大学博士学位论文, 北京, 2011)[9] Maltais A, Dub´e D, FisetM, Laroche G, Turgeon S. Mater Charact, 2004; 52: 103[10] Deschamps A, Brechet Y. Acta Mater, 1998; 47: 293[11] Celotto S. Acta Mater, 2000; 48: 1775[12] Gharghouri M A, Weatherly G C, Embury J D, Root J. Philos Mag, 1999; 79A: 1671[13] Volmer M, Weber A. Phys Chem, 1926; 119: 277[14] Becker R, Doring W. Ann Phys, 1935; 24: 719[15] Zeldovich J B. Acta Physicochim, 1943; 18: 1[16] Hillert M, Hoglund L, Agren J. Acta Mater, 2003; 51: 2089[17] Lifshitz I, Slyozova V. J Phys Chem Solids, 1961; 19: 35[18] Wagner C Z. Elektrochem, 1961; 65: 581[19] Voorhees P W. Annu Rev Mater Sci, 1992; 22: 197[20] Hutchinson C R, Nie J F, Gorsse S. Metall Mater Trans, 2005; 36A: 2093[21] C´aceres C H, Davidson C J, Griffiths J R, Newton C L. Mater Sci Eng, 2002; A325: 344[22] Akhtar A, Teghtsoonian E. Acta Metall, 1969; 17: 1339[23] Akhtar A, Teghtsoonian E. Philos Mag, 1972; 25: 897[24] Lukac P. Phys Status Solidi, 1992; 131A: 377[25] Nussbaum G, Sainfort P, Regazzoni G, Gjestland H. Scr Metall, 1989; 23: 1079[26] Shaw C, Jones H. Mater Sci Eng, 1997; A226: 856[27] C´aceres C, Rovera D. J Light Met, 2001; 1: 151[28] Hall E O. Proc Phys Soc Lond, 1951; 64B: 747[29] Petch N J. J Iron Steel Inst, 1953; 174: 25[30] Hauser F E, Landon P R, Dorn J E. Trans Am Inst Mining Metall Eng, 1956; 206: 589[31] Brown L M, Ham P K. Strengthening Methods in Crystals. London: Elsevier, 1971: 10[32] Miller W S, Humphreys F J. Scr Metall, 1991; 25: 33[33] Armstrong R, Douthwaite R M, Codd I, Petch N J. Philos Mag, 1962; 7: 45[34] Leroy G, Embury J D, Edward G, Ashby MF. Acta Metall, 1981; 29: 1509[35] Brown L M, Stobbs W M. Philos Mag, 1971; 23: 1185[36] Brown L M, Stobbs W M. Philos Mag, 1971; 23: 1201[37] Brown L M, Clarke D R. Acta Metall, 1975; 23: 821[38] Lemaitre J, Chaboche J L. Mechanics of Solid Materialsrm. Cambridge: Cambridge University Press, 1990: 167 |
|