| 超轻β固溶体Mg-11Li-3Zn合金的准超塑性与变形机理 |
| 曹富荣1,丁桦1,王昭东2,李英龙1,管仁国1,崔建忠3 |
1. 东北大学材料与冶金学院, 沈阳 110819
2. 东北大学轧制与连轧自动化国家重点实验室, 沈阳 110819
3. 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819 |
|
| QUASI–SUPERPLASTICITY AND DEFORMATION MECHANISM OF ULTRALIGHT β SOLID SOLUTION Mg–11Li–3Zn ALLOY |
| CAO Furong 1, DING Hua 1, WANG Zhaodong 2, LI Yinglong 1, GUAN Renguo 1, CUI Jianzhong 3 |
1. College of Materials and Metallurgy, Northeastern University, Shenyang 110819
2. State Key Lab of Rolling and Tandem Rolling Automation, Northeastern University, Shenyang 110819
3. Key Lab of Materials Electromagnetic Process Research, Ministry of Education, Northeastern University, Shenyang 110819 |
引用本文:
曹富荣 丁桦 王昭东 李英龙 管仁国 崔建忠. 超轻β固溶体Mg-11Li-3Zn合金的准超塑性与变形机理[J]. 金属学报, 2012, 48(2): 250-256.
,
,
,
,
,
.
QUASI–SUPERPLASTICITY AND DEFORMATION MECHANISM OF ULTRALIGHT β SOLID SOLUTION Mg–11Li–3Zn ALLOY[J]. Acta Metall Sin, 2012, 48(2): 250-256.
| [1] Counts W A, Friak M, Raabe D, Neugebauer J. Acta Mater, 2009; 57: 69[2] Cao F R, Lei F, Cui J Z,Wen J L. Acta Metall Sin, 1999; 35: 770(曹富荣, 雷方, 崔建忠, 温景林. 金属学报, 1999; 35: 770)[3] Cao F R, Guan R G, Ding H, Li Y L, Zhou G, Cui J Z. Acta Metall Sin, 2010; 46: 715(曹富荣, 管仁国, 丁 桦, 李英龙, 周舸, 崔建忠. 金属学报, 2010; 46: 715)[4] Nayeb–Hashemi A A, Clark J B, Pelton A D. Bull Alloy Phase Diagram, 1984; 5: 365[5] Raynor G V. The Physical Metallurgy of Magnesium and Its Alloys. London: Pergamon Press, 1959: 265[6] Metenier P, Gonzalez–Doncel G, Ruano O A, Wolfenstine J, Sherby O D. Mater Sci Eng, 1990; A125: 195[7] Fujitani W, Furushiro N, Hori S, Kumeyama K. J Jpn Ins Light Met, 1992; 42: 125[8] Higashi K, Wolfenstine J. Mater Letter, 1991; 10: 329[9] Kojima Y, Inoue M, Tanno O. J Japan Inst Metal, 1990; 54: 354[10] Cao F R, Ding H, Li Y L, Zhou G, Cui J Z. Mater Sci Eng, 2010; A527: 2335[11] Dong S L, Imai T, Lim SW, Kanetake N, Saito N. J Mater Sci, 2007; 42: 5296[12] Liu X H, Zhan H B, Gu S H, Qu Z K, Wu R Z, Zhang M L. Mater Sci Eng, 2010; A528: 6157[13] Furui M, Kitamura H, Anada H, Langdon T G. Acta Mater, 2007; 55: 1083[14] Ashby M F. Acta Metall, 1972; 20: 887[15] Mohamed F A, Langdon T G. Metall Trans, 1974; 5A: 2339[16] Ruano O A, Wadsworth J, Sherby O D. J Mater Sci, 1985; 20: 3735[17] Sajjadi S A, Nategh S. Mater Sci Eng, 2001; A307: 158.[18] Tanaka H, Yamada T, Sato E, Jimbo I. Scr Mater, 2006; 54: 121[19] Chung S W, Higashi K, Kim W J. Mater Sci Eng, 2004; A372: 15[20] Oikawa H, Langdon T G. in: Wilshire B, Evans R W eds., Creep Behavior of Crystalline Solids. UK: Pineridge Press Limited, 1985: 64[21] Woo S S, Kim Y R, Shin D H, Kim W J. Scr Mater, 1997; 37: 1351[22] Yavari P, Langdon T G. Acta Metall, 1982; 30: 2181[23] Langdon T G. Acta Metall Mater, 1994; 42: 2437[24] Weinberg A F, Levinson D W, Rostoker W. Trans ASM, 1956; 48: 855[25] Syn C K, Lesuer D R, Sherby O D. Mater Sci Eng, 1996; A201: 201[26] Ma A B, Nishida Y, Saito N, Shigematsu I, Lim S W. Mater Sci Technol, 2003; 19: 1642[27] Somekawa H, Hirai K, Watanabe H, Takigawa Y, Higashi K. Mater Sci Eng, 2005; A407: 53[28] Li Y, Langdon T G. Acta Mater, 1998; 46: 1143[29] Cao F R. PhD Thesis, Northeastern University, Shenyang, 1999(曹富荣. 东北大学博士学位论文, 沈阳, 1999)[30] Friedel J. Dislocations. Oxford: Pergamon Press, 1964: 331[31] Wang J S, Nix W D. Acta Metall, 1986; 34: 545[32] Fuentes–Samaniego R, Nix W D. Scr Metall, 1981; 15: 15[33] Somekawa H, Mukai T. Scr Metall, 2007; 57: 1008[34] Wolfenstine J, Gonzalez–Docel G, Sherby O D. J Mater Res, 1990; 5: 1359[35] Lee B H, Shin K S, Lee C S. Mater Sci Forum, 2005; 475–479: 2927[36] Zhang B, Mynors D J, Mugarra A, Ostolaza K. Mater Sci Forum, 2004; 447–448: 171[37] Kassner M E, Perez–Prado M T. Prog Mater Sci, 2000; 45: 1[38] Nieh T G, Wadsworth J, Sherby O D. Superplasticity in Metals and Ceramics. Cambridge: Cambridge University Press, 1997: 34[39] Chow K K, Chan K C. Key Eng Mater, 2000; 177–180: 601[40] Langdon T G. J Mater Sci, 2009; 44: 5998[41] Mohri T, Mabuchi M, Nakamura M, Asahina T, Iwasaki H, Aizawa T, Higashi K. Mater Sci Eng, 2000; A290: 139[42] Hirai K, Somekawa H, Takigawa Y, Higashi K. Scr Mater, 2007; 56: 237[43] Cadek J. Creep In Metallic Materials. Holland: Elsevier, 1988: 161[44] Mishra R S, Stolyarov V V, Echer C, Valiev R Z, Mukherjee A K. Mater Sci Eng, 2001; A298: 44[45] Kawasaki M, Kubota K, Higashi K, Langdon T G. Mater Sci Eng, 2006; A429: 334[46] Watanabe H, Mukai T, Kohzu M, Tanabe S, Higashi K. Acta Mater, 1999; 47: 3753 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|